Abstract:
A paint composition of the present invention contains an aluminum pigment and a mica pigment. The content of the aluminum pigment is equal to or higher than the content of the mica pigment. The aluminum pigment has a specific surface area, determined by the BET method, of not more than 55000 cm2/g, an average thickness of not less than 0.3 μm, and an aspect ratio of not more than 50.
Abstract:
A resin particle composition includes resin particles, polishing agent particles having an average circle-equivalent diameter of 0.1 μm to 3.0 μm, and silica particles having a compression aggregation degree of 60% to 95% and a particle compression ratio of 0.20 to 0.40.
Abstract:
Provided is a spherical alumina powder which, when incorporated into resins in a high concentration, enables a resin composition to have low viscosity and which has reduced viscosity increase in the resin composition over time after surface treatment of the spherical alumina powder. The spherical alumina powder has an alkyl group(s) derived from a silane compound(s) on its surface, and is characterized in that an intensity ratio {I (CH3)/I (CH2)} of a peak (2960±5 cm−1) associated with asymmetric vibration of CH3 to a peak (2925±5 cm−1) associated with asymmetric vibration of CH2 in the alkyl group(s) of the silane compound(s) in the same spectral data obtained by infrared spectroscopic analysis measurement is 0.2 or more and less than 2.0.
Abstract:
Provided are a molded product having an effective thickness of 1 mm or more, the molded product being formed from an aliphatic polyester resin composition containing from 1 to 30 parts by mass of a carboxylic acid anhydride and preferably further containing from 1 to 50 parts by mass of at least one type of a short fiber reinforcing material, a thermoplastic elastomer, or an acrylic rubber core-shell polymer per 100 parts by mass of an aliphatic polyester resin containing not less than 50 mass % of a polyglycolic acid resin, the effective thickness being 1 mm or more; a downhole tool for hydrocarbon resource recovery formed from the molded product having an effective thickness of 1 mm or more; an aliphatic polyester resin composition for the downhole tool member for hydrocarbon resource recovery; and a well drilling method.
Abstract:
A heat-shrinkable protective element having at least one protective layer is obtained from a polymeric composition having a polymer material, where the polymeric composition additionally has an electrically conducting filler having a BET specific surface of at least 100 m2/g according to Standard ASTM D 6556.
Abstract:
Provided is a polyamide molding composition comprising a) at least one semi-aromatic, semi-crystalline polyamide, at least flat glass fiber as reinforcing filler, c) at least one aliphatic polyamide comprising recurring units complying with the formula —NH—R2—NH—CO—R3—CO—, wherein R2 and R3, equal to or different from each other at each occurrence, are divalent aliphatic hydrocarbon groups, and d) at least one additive.
Abstract:
Disclosed is a method of manufacturing ceramic coated graphite having electric resistance in a range from 108 to 1016 Ω/sq via a sol-gel method, the ceramic coated graphite comprising graphite; and ceramic chemically bonded to a lateral defect area of the graphite, wherein the graphite is oval graphite having an aspect ratio selected from the group consisting of 10:1 to 200:1, and the ceramic is at least one type selected from the group consisting of magnesium oxide, aluminum oxide, zinc oxide, zirconium oxide, and silica.
Abstract:
The coating composition of the present invention is characterized in that hydrophobic microparticles, and flat-shaped microparticles forming a card-house aggregate structure, are dispersed in a binder resin dissolved in a solvent. Preferably, the aspect ratio of table faces and end faces of the flat-shaped microparticles is 10 or higher. Preferably, the average particle size of the flat-shaped microparticles in an aggregated state ranges from 125 nm to 200 μm. The coating composition of the present invention can form a coating film having few cracks and can impart high water repellency and high oil repellency without the need for a complex operation.
Abstract:
Powder compositions and articles and methods of forming articles from powder compositions are provided. In one embodiment the powder compositions include at least one polyester polymer powder and an amount of reinforcing particles having an aspect ratio of preferably at least about 5:1. In another embodiment the ponder compositions include at least one medium-high melting temperature, aromatic and crystalline polyester polymer powder. In a preferred embodiment, the powder composition is capable of being formed, via a laser sintering process, into a three-dimensional article that exhibits one or more desirable mechanical properties in an elevated temperature environment.
Abstract:
A carbon material having a continuous porous structure oriented to the stretching axis is provided, which carbon material can be used as a structural material excellent in interfacial adhesion. The porous carbon material has a continuous porous structure in at least a portion thereof, in which the continuous porous structure has an orientation degree measured by a small-angle X-ray scattering method or an X-ray CT method of 1.10 or more.