Abstract:
A PHA copolymer which is slowly crystallized is improved in crystallization speed to improve the melt workability of the PHA copolymer in working such as injection molding, film molding, blow molding, fiber spinning, extrusion foaming or bead foaming, thereby improving the resultant articles in productivity. A method for the improvement is a method for producing a PHA mixture, including the step of culturing a microorganism having both of a gene encoding a PHA synthase that synthesizes a copolymer PHA (A) and that is derived from the genus Aeromonas, and a gene encoding a PHA synthase that synthesizes a PHA (B) different in melting point from the copolymer PHA (A) by 10° C. or more to produce, in a cell of the microorganism, two or more PHAs different in melting point from one another by 10° C. or more simultaneously.
Abstract:
A PHA copolymer which is slowly crystallized is improved in crystallization speed to improve the melt workability of the PHA copolymer in working such as injection molding, film molding, blow molding, fiber spinning, extrusion foaming or bead foaming, thereby improving the resultant articles in productivity. A method for the improvement is a method for producing a PHA mixture, including the step of culturing a microorganism having both of a gene encoding a PHA synthase that synthesizes a copolymer PHA (A) and that is derived from the genus Aeromonas, and a gene encoding a PHA synthase that synthesizes a PHA (B) different in melting point from the copolymer PHA (A) by 10° C. or more to produce, in a cell of the microorganism, two or more PHAs different in melting point from one another by 10° C. or more simultaneously.
Abstract:
A polyester resin composition includes: a polylactic acid; a poly(3-hydroxyalkanoate); pentaerythritol; and a silicate. In the polyester resin composition, an amount of the polylactic acid is from 55 to 75 parts by weight, and an amount of the poly(3-hydroxyalkanoate) (B) is from 25 to 45 parts by weight, with respect to 100 parts by weight of a total amount of the polylactic acid and the poly(3-hydroxyalkanoate); an amount of the pentaerythritol is from 0.05 to 20 parts by weight with respect to 100 parts by weight of the total amount of the polylactic acid and the poly(3-hydroxyalkanoate); and an amount of the silicate is from 10 to 40 parts by weight with respect to 100 parts by weight of the total amount of the polylactic acid and the poly(3-hydroxyalkanoate).
Abstract:
An object of the present invention is to improve spinnability, productivity, and tensile strength of a polyester fiber containing poly(3-hydroxybutyrate-co-3-hydroxyhexanoate).By spinning the polyester resin containing the poly(3-hydroxybutyrate-co-3-hydroxyhexanoate) at a high spinning velocity, the spinnability, productivity, and tensile strength of the polyester fiber can be improved.
Abstract:
Disclosed herein is an aliphatic polyester resin composition that simultaneously improves slow crystallization, low impact strength, and low tensile elongation that are the drawbacks of a polyhydroxyalkanoate.The aliphatic polyester resin composition comprises: a polyhydroxyalkanoate (A); a graft copolymer (B); and pentaerythritol (C), wherein the graft copolymer (B) is obtained by graft polymerization of a vinyl-based monomer onto at least one rubber selected from the group consisting of a composite rubber (b1) comprising a polyorganosiloxane component and a polyalkyl(meth)acrylate component, an acrylic rubber (b2), and a diene-based rubber (b3) comprising a diene-based monomer.
Abstract:
An object is to improve both slow crystallization and brittleness that are drawbacks of polyhydroxyalkanoates, so that processability in mold processing, such as injection molding, is improved, processing speed is increased, and ductility is imparted to a resulting molded article. Provided is an aliphatic polyester resin composition including a polyhydroxyalkanoate (A), an ethylene-vinyl acetate copolymer resin (B), and pentaerythritol (C), wherein the ethylene-vinyl acetate copolymer resin (B) has a vinyl acetate content of 65 to 95 wt %, and the polyhydroxyalkanoate (A) and the ethylene-vinyl acetate copolymer resin (B) are compatible.
Abstract:
Provided are poly(3-hydroxyalkanoate) foam particles, which can give a foam molded article having good surface aspects and a low shrinkage ratio of a molding, and the foam molded article. The poly(3-hydroxyalkanoate) foam particles have at least two melting peaks on a DSC curve obtained by differential scanning calorimetry and in which a melting calorie (X) on a high temperature side is 0.1 to 20 J/g, a gel fraction (Y) is 20 to 75% by weight, and the melting calorie (X) and the gel fraction (Y) satisfy Formula: X+Y≥30.
Abstract:
Provided is a resin composition excellent in processability and productivity, which improves low crystallization rate and improves processability in forming such as injection molding or sheet forming. Provided is a polyester resin composition including a polyester resin (A), a crystallization promoter (B), and pentaerythritol (C).
Abstract:
An object is to increase crystallization speed, which is a drawback of polyhydroxyalkanoate, to improve processability in processing such as injection molding or blow molding and increase the speed of processing and is, in addition, to refine the crystal of polyhydroxyalkanoate to suppress a change of mechanical properties with passage of time of a resulting molded article. Disclosed herein is a polyester resin composition containing polyhydroxyalkanoate and pentaerythritol.
Abstract:
A poly-3-hydroxyalkanoate resin composition having excellent ductility and transparency, and a molded article thereof. The poly-3-hydroxyalkanoate resin composition includes: a poly-3-hydroxyalkanoate resin (A); and an ethylene-vinyl acetate copolymer resin (B) having a vinyl acetate content of 65 to 95 wt %, wherein the resin (A) and the resin (B) are miscible and a ratio of resin (A)/resin (B) is 90/10 to 55/45 (wt/wt). The molded article is produced using such a poly-3-hydroxyalkanoate resin composition.