Abstract:
The present invention concerns friction reducers for use in lubricating oil compositions which comprise certain groups of aromatic compounds, esters, narrow mixtures of base stocks, and/or amorphous polymers such as amorphous olefin copolymers. These compositions can provide substantial reductions in the coefficient of friction and fuel economy improving benefits when admixed to lubricating oils without deleterious effects such as instability, undesirable high viscosities and deposits. In one aspect of the invention, pentaerythritol esters and optionally triol esters are added to lubricating oil compositions to provide reduced friction and improved fuel economy. In a second aspect of the invention, similar results are obtained by adding hydrocarbyl aromatics to a lubricating oil composition containing one or more of Groups II and III base stock. In a third aspect, the invention concerns a lubricating oil composition comprising an amorphous olefin copolymer and one or more of Groups II and III base stocks. In one embodiment, the third aspect also includes one or more of hydrocarbyl aromatics and polyol esters as part of the composition. In a forth aspect, moderate concentrations of hydrocarbyl aromatics are used in a lubricating oil composition comprising paraffinic base oil stocks and preferably a borated polyisobutenyl succinimide ashless dispersant.
Abstract:
The invention aims to provide a rolling bearing that secures a sufficient bearing life economically even when used under such conditions that water from the outside or water formed by moisture condensation may seep into the lubricant or the bearing is affected by the vibrations, and particularly a rolling bearing suited to the electric parts and accessaries of au automobile engine, such as an alternator. To accomplish the object, the hydrogen ion exponent pH of the grease sealed into the inside of the bearing is adjusted in a range of from 7 to 13. For the same purpose, the hydrogen ion exponent pH of the grease is adjusted in a range of from 5 to 13 where a prescribed amount of an organic metal salt or ADTC is added to the grease, where a prescribed amount of an inorganic compound having an average particle size of 2 nullm or smaller is added to the grease, or where a diurea compound containing an aromatic amine or a mixture of the diurea compound is added to the grease as a thickener.
Abstract:
Disclosed are lubricant compositions comprising a dispersed hydrated alkali metal borate and a polyalkylene succinic anhydride, a mixture of polyalkylene succinic anhydrides or derivatives thereof. Also disclosed are methods for improving the water tolerance of a lubricant composition comprising an alkali metal borate. Such methods employ compositions comprising a dispersed hydrated alkali metal borate and a polyalkylene succinic anhydride, a mixture of polyalkylene succinic anhydrides or derivatives thereof.
Abstract:
This invention provides a release agent for low speed casting, which does not pollute working environment, has a superior running property and lubricating property and further shows a superior cleanability of a die. An aqueous release agent for a low speed injection die casting comprises as main components an inorganic lubricant, spherical resin particles having an average particle size of 0.1-10 nullm, an organic carboxylic acid metal salt and water.
Abstract:
A process for preparing a stable cooling lubricant emulsion for use in the cutting of metals involves the steps of (a) forming a mixture having an oil component, water and an emulsifier with the oil component being emulsified in the water, then (b) dispersing into 100 parts by weight of the mixture by means of high shear from about 1 to about 14 parts by weight of a natural, water-immiscible cutting oil. The stable oil-in-water cooling lubricant emulsion formed has at least 50 percent of the cutting oil present in the form of particles having a diameter of 0.5 to 8 &mgr;m. The cooling lubricant emulsion formed may be used in an extended range of applications.
Abstract:
An aqueous cutting liquid comprises a cationic water-soluble resin having an amine value of 20 to 200 mgKOH/g, and at least one rheology control agent selected from the group consisting of an inorganic bentonite, an organic bentonite and an aqueous silica sol, wherein the content of a nonvolatile matter of the rheology control agent is 0.1 to 30 percent by weight of the amount of the nonvolatile matter of the cationic water-soluble resin. An aqueous cutting agent comprises the aqueous cutting liquid, and an abrasive grain, wherein the content of the abrasive grain is 100 to 1000 percent by weight of the amount of the nonvolatile matter of the aqueous cutting liquid. A hard and brittle material is cut by a cutting device using the aqueous cutting agent. The present invention provides an aqueous cutting agent which is excellent in dispersion stability of the abrasive grain and viscosity stability during cutting/slicing operations, aqueous cutting liquid usable for the aqueous cutting agent, and a cutting/slicing method excellent in cutting performance, cleanability and the like of the work material on cutting/slicing hard and brittle material by using the cutting agent.
Abstract:
An improved polybutene-free lubricant composition for marine diesel engines, comprising a major amount of oil of lubricating viscosity and, provided by admixing therewith, minor amounts of a) at least one of a borated dispersant or oil-soluble or oil-dispersible boron compound; and b) one or more overbased metal compounds the or each compound having a TBN of at least 300, with the proviso that if an overbased metal salicylate is present then the TBN of said salicylate is at least 200; wherein the TBN of the composition is at least 10 and the viscosity index of the composition is at least 90.
Abstract:
The disclosure relates to improved gel/grease compositions as well as grease compositions capable of imparting improved corrosion resistance. The grease includes a silica/silicate mixture that can imparts a relatively high pH and corrosion resistant properties to the grease.
Abstract:
A lubricant is provided for use in hot working such as cross-roll rolling of a seamless steel pipe. It effectively reduces the friction coefficient between the working tools and the material under the hot work, thus extending the lives of the tools. The lubricant contains: (A) from about 10 to about 60 wt % of alkali silicate; (B) from about 1 to about 20 wt % of silane coupling agent; (C) from about 0.1 to about 5.0 wt % of at least one kind of alkali compound selected from a group consisting of an alkali hydroxide, an alkali carbonate, an alkali borate and an alkali salt of mineral acid; and (D) from about 30 to about 70 wt % of water. Alternatively, the lubricant contains: (A) from about 10 to about 60 wt % of alkali silicate; (B) from about 1 to about 20 wt % of silane coupling agent; (C) from about 0.1 to about 5.0 wt % of at least one kind of alkali compound selected from a group consisting of an alkali hydroxide, an alkali carbonate, an alkali borate and an alkali salt of mineral acid; (D) from about 5 to about 50 wt % of water; (E) from about 10 to about 60 wt % of iron oxide; and (F) from about 0.1 to about 5.0 wt % of at least one additive selected from a group consisting of a dispersant and a thickening agent.
Abstract:
A lubricant film coated steel sheet having excellent phosphatability, in accordance with the present invention, is a lubricant film coated steel sheet produced by forming a coating containing silicic acid or silicate on a steel sheet or a plated steel sheet, wherein the surface roughness of the steel sheet or the plated steel sheet is 0.5 to 1.5 .mu.m as the centerline-average roughness RA and the PPI (cut-off value of 1.25 .mu.m) thereof is 75 to 300; and the content of silicic acid or silicate in the coating is 1 to 200 mg/m.sup.2 as corrected into dried SiO.sub.2 weight or the coating ratio of the coating is 1 to 60%.