公开(公告)号:US5547482A
公开(公告)日:1996-08-20
申请号:US270423
申请日:1994-07-05
Applicant: Julie B. Chalk , Jonathan C. Rowe , Paul M. Schermerhorn , Robert D. Shoup
Inventor: Julie B. Chalk , Jonathan C. Rowe , Paul M. Schermerhorn , Robert D. Shoup
CPC classification number: C03C3/06 , C03B19/06 , C03B19/066 , C03B19/12 , C03B20/00 , C03B32/00 , C03B2201/08 , C03B2201/20 , C03B2201/28 , C03B2201/30 , C03B2201/31 , C03B2201/32 , C03B2201/34 , C03B2201/40 , C03B2201/42 , C03B2201/50 , C03B2201/54 , C03C2201/06 , C03C2201/42 , C03C2203/26 , C03C2203/27 , C03C2203/50 , Y02P40/57
Abstract: This invention is directed to the production of essentially defect-free high purity fused silica glass articles, the method comprising the following steps: (a) forming a green body from silica particulates or a porous body of amorphous silica; (b) sintering said body in a chamber by raising the temperature of the chamber to above 1720.degree. C., while purging the chamber with helium or applying a vacuum to the chamber; and (c) consolidating the sintered body in a chamber by raising the temperature within the chamber to at least 1750.degree. C., introducing an inert gas into the chamber at a pressure less than about 6.9 MPa (1000 psig), and cooling the chamber while maintaining the pressurized atmosphere to a temperature at least below the annealing point of the glass. In the most preferred practice, a green body of silica particulates will be prepared via a sol-gel process.
Abstract translation: 本发明涉及生产基本上无缺陷的高纯度熔融石英玻璃制品,该方法包括以下步骤:(a)由二氧化硅微粒或无定形二氧化硅的多孔体形成生坯; (b)通过将腔室的温度升高到1720℃以上,同时用氦气吹扫腔室或向室内施加真空来在室内烧结所述主体; 和(c)通过将室内的温度升高至至少1750℃将烧结体固化在室中,在小于约6.9MPa(1000psig)的压力下将惰性气体引入室中,并冷却室 同时将加压气氛保持在至少低于玻璃退火点的温度。 在最优选的实践中,将通过溶胶 - 凝胶法制备生物体的二氧化硅颗粒。