Abstract:
An optical film includes a plurality of alternating first and second layers. The first layers have a first in-plane birefringence, the second layers have a second in-plane birefringence, and the second in-plane birefringence is less than the first in-plane birefringence and greater than 0.03. The first layers may include polyethylene terephthalate homopolymer and the second layers may include glycol-modified co (polyethylene terephthalate). The optical film has a shrinkage along a first direction of greater than 4% and a shrinkage along an orthogonal second direction of greater than 3% when heated at 150° C. for 15 minutes. A glass laminate is prepared by disposing the optical film between glass layers and laminating the optical film to the glass layers.
Abstract:
A microstructured diffuser is described comprising a light transmissive film comprising a first microstructured surface comprising a plurality of peaks and valleys. A coating is disposed on the first microstructured surface. The coating partially fills the valleys forming a second microstructured surface.
Abstract:
A multilayer optical film has a packet of microlayers that selectively reflect light by constructive or destructive interference to provide a first reflective characteristic. At least some of the microlayers are birefringent. A stabilizing layer attaches to and covers the microlayer packet proximate an outer exposed surface of the film. Heating element(s) can physically contact the film to deliver heat to the packet through the stabilizing layer by thermal conduction, at altered region(s) of the film, such that the first reflective characteristic changes to an altered reflective characteristic in the altered region(s) to pattern the film. The stabilizing layer provides sufficient heat conduction to allow heat from the heating elements to change (e.g. reduce) the birefringence of the birefringent microlayers disposed near the outer exposed surface in the altered region(s), while providing sufficient mechanical support to avoid substantial layer distortion of the microlayers near the outer exposed surface in the altered region(s).
Abstract:
A microstructured diffuser is described comprising a light transmissive film comprising a first microstructured surface comprising a plurality of peaks and valleys. A coating is disposed on the first microstructured surface. The coating partially fills the valleys forming a second microstructured surface.
Abstract:
Light directing film is disclosed. The light directing film includes a first structured major surface and an opposing second major surface. The first structured major surface includes a plurality of unitary discrete structures. Each unitary discrete structure includes a light directing portion that is primarily for directing light and includes a plurality of first side facets. Each first side facet makes an angle with the plane of the light directing film in a range from about 35 degrees to about 55 degrees. Each light directing portion also includes a first base that is defined by the plurality of first side facets and has a first minimum dimension. Each light directing portion also has a first maximum height. Each unitary discrete structure also includes a bonding portion that is primarily for bonding the light directing film to a surface. The bonding portion is disposed on and between the plurality of first side facets and includes a plurality of second side facets. Each second side facet makes an angle with the plane of the light directing film greater than about 70 degrees. The bonding portion also includes a second base that is defined by the plurality of second side facets and has a second minimum dimension less than about 10% of the first minimum dimension. The bonding portion also has a second maximum height. The ratio of the second maximum height to the second minimum dimension is at least about 1.5.
Abstract:
Multilayer reflective polarizers are described. In particular, multilayer reflective polarizers that include both crystalline high index layers and low index layers are disclosed. These reflective polarizers may be particularly suitable for automotive, architectural, and industrial applications.
Abstract:
Vehicle projection assemblies are described. In particular, vehicle projection assemblies within a housing including a projection module, and selective reflective polarizing element are described. Particular selective reflective polarizing elements may enable advantageous configurations for such vehicle projection assemblies.
Abstract:
Presently described are optical stacks comprising a first optical film comprising a plurality of structures comprising an optically active portion designed primarily to provide optical gain and optionally an optically in-active bonding portion disposed on a first surface bonded to a second optical film with a light-transmissive adhesive layer such that a portion of the structures penetrate the adhesive layer and a separation is provided between the adhesive layer and the first surface. In one embodiment, the optical stacks exhibit a combination of high peel strength and high retained brightness, particularly after aging. The adhesive layer preferably comprises an interpenetrating network of the reaction product of a polyacrylate component and a polymerizable monomer and the adhesive layer has an elastic modulus ranging from 100 to 2000 MPa at 25° C.
Abstract:
The present disclosure describes light delivery and distribution components of a ducted lighting system having a cross-section that includes at least one curved portion and a remote light source. The delivery and distribution system (i.e., light duct and light duct extractor) can function effectively with any light source that is capable of delivering light which is substantially collimated about the longitudinal axis of the light duct, and which is also preferably substantially uniform over the inlet of the light duct.
Abstract:
An optical film includes a plurality of alternating first and second layers. The first layers have a first in-plane birefringence, the second layers have a second in-plane birefringence, and the second in-plane birefringence is less than the first in-plane birefringence and greater than 0.03. The first layers may include polyethylene terephthalate homopolymer and the second layers may include glycol-modified co(polyethylene terephthalate). The optical film has a shrinkage along a first direction of greater than 4% and a shrinkage along an orthogonal second direction of greater than 3% when heated at 150° C. for 15 minutes. A glass laminate is prepared by disposing the optical film between glass layers and laminating the optical film to the glass layers.