SILICON-OXIDE-COATED SOFT MAGNETIC POWDER, AND METHOD FOR MANUFACTURING SAME

    公开(公告)号:US20220392676A1

    公开(公告)日:2022-12-08

    申请号:US17773865

    申请日:2020-11-19

    Abstract: A silicon oxide-coated soft magnetic powder, in which the ratio of a volume-based cumulative 50% particle diameter D50 (HE) according to a dry laser diffraction particle size distribution analysis to the same particle diameter D50 (MT) according to a wet laser diffraction particle size distribution analysis is 0.7 or more, and a coverage ratio R defined by R=Si×100/(Si+M) (Si and M are molar fractions of Si and elements constituting the soft magnetic powder) is 70% or more is obtained by subjecting a slurry containing a soft magnetic powder containing 20 mass % or more of iron and a hydrolysate of a silicon alkoxide to a dispersion treatment when the surface of the soft magnetic powder is coated with the hydrolysate in a mixed solvent of water and an organic substance. The powder has good insulation/dispersibility properties and a high filling factor during molding.

    METHOD FOR PRODUCING SILVER NANOWIRES
    5.
    发明申请

    公开(公告)号:US20190240735A1

    公开(公告)日:2019-08-08

    申请号:US16342545

    申请日:2017-10-25

    Abstract: [Problem] In the production of silver nanowires, the necessarily amount of the silver-containing liquid is decreased, and the yield of long silver nanowires is improved.[Solution] A method for producing silver nanowires, including adding a silver-containing liquid to an alcohol solvent having dissolved therein a chloride, a bromide, an aluminum salt, an alkali metal hydroxide, and an organic protective agent, so as to perform reduction deposition of silver in a wire form in the alcohol solvent, the silver-containing liquid to be added having dissolved therein a silver compound in a silver concentration of from 3.5 to 32.0 mol/L. The silver-containing liquid used is preferably a water-containing solvent having a mass proportion of water of from 4.0 to 100.0%.

    METHOD OF MANUFACTURING SILICON-OXIDE-COATED SOFT MAGNETIC POWDER

    公开(公告)号:US20240416418A1

    公开(公告)日:2024-12-19

    申请号:US18819107

    申请日:2024-08-29

    Abstract: [Problem] To provide a silicon oxide-coated soft magnetic powder having a silicon oxide coating with few defects so as to have an excellent insulation property, and having good dispersibility in an aqueous solution, and capable of obtaining a high filling factor when molding a green compact.
    [Means for Solution] A highly insulating silicon oxide-coated soft magnetic powder, in which the ratio of a volume-based cumulative 50% particle diameter D50 (HE) according to a dry laser diffraction particle size distribution analysis to the same particle diameter D50 (MT) according to a wet laser diffraction particle size distribution analysis is 0.7 or more, and a coverage ratio R defined by R=Si×100/(Si+M) (wherein Si and M are molar fractions of Si and elements constituting the soft magnetic powder) is 70% or more is obtained by subjecting a slurry containing a soft magnetic powder containing 20 mass % or more of iron and a hydrolysate of a silicon alkoxide to a dispersion treatment when the surface of the soft magnetic powder is coated with the hydrolysate in a mixed solvent of water and an organic substance.