Abstract:
There is provided a dispersion composition containing (A) a metal oxide particle having a primary particle diameter of 1 nm to 100 nm, (B) a polymer compound represented by the specific formula having a weight average molecular weight of 5,000 to 8,000 and an acid value of 70 to 90 mgKOH/g, and (C) a solvent, and a curable composition containing the dispersion composition and (D) a polymerizable compound.
Abstract:
The near-infrared absorption composition includes a processed coloring agent obtained by coating a near-infrared absorption coloring agent with a resin having one or more selected from a coloring agent structure, a heterocyclic structure, and an acyclic hetero atom-containing group. The near-infrared absorption coloring agent is preferably one or more selected from a phthalocyanine coloring agent, a perylene coloring agent, a pyrrolopyrrole coloring agent, a cyanine coloring agent, a dithiol metal complex coloring agent, a naphthoquinone coloring agent, a diimmonium coloring agent, an azo coloring agent, and a squarylium coloring agent and more preferably a pyrrolopyrrole coloring agent.
Abstract:
There is provided a dispersion composition having a high dispersion stability, and containing metal oxide particles having a primary particle diameter of 1 nm to 100 nm (A), a polymer compound having an acid value of 120 mgKOH/g or more, which is represented by the following Formula (1) (B), and a solvent (C). (A1-R2nR1P1)m Formula (1)
Abstract:
There is provided a dispersion composition capable of forming a film being excellent in surface conditions, the dispersion composition containing metal oxide particles (A) having a primary particle diameter of 1 nm to 100 nm, a polymer compound (B) having an acid value of less than 120 mgKOH/g, which is represented by the following Formula (1), and a solvent (C).
Abstract:
A film in which a light transmittance when light is transmitted from one surface of the film to the other surface has a maximum value of 10% or lower in a wavelength range of 400 to 830 nm and has a minimum value of 70% or higher in a wavelength range of 1000 to 1300 nm.
Abstract:
A coloring composition includes colorants and a resin, in which a ratio A/B of a minimum value A of an absorbance in a wavelength range of 400 to 830 nm to a maximum value B of an absorbance in a wavelength range of 1000 to 1300 nm is 4.5 or higher.
Abstract:
There is provided a dispersion composition having a high dispersion stability, and containing metal oxide particles having a primary particle diameter of 1 nm to 100 nm (A), a polymer compound having an acid value of 120 mgKOH/g or more, which is represented by the following formula (1) (B), and a solvent (C). (A1-R2nR1P1)m Formula (1)