公开(公告)号:US20160045957A1
公开(公告)日:2016-02-18
申请号:US14926747
申请日:2015-10-29
Applicant: Howmedica Osteonics Corp.
Inventor: John Lapszynski , Robert W. Klein , Michael A. DeLuise
CPC classification number: B22F3/11 , A61F2/30771 , A61F2/3094 , A61F2/34 , A61F2/36 , A61F2/3859 , A61F2/389 , A61F2/4455 , A61F2002/30013 , A61F2002/30957 , A61F2002/30968 , A61F2250/0024 , A61F2310/00017 , A61F2310/00023 , A61F2310/00029 , B22F1/0059 , B22F3/24 , B22F2001/0066 , B22F2998/10 , Y10T428/12028 , B22F1/0096 , B22F3/04 , B22F3/225 , B22F3/02
Abstract: In one embodiment, the present invention may be a method of forming a porous and/or dense article from metal powder, including adding to a mold a first feedstock comprising an agglomerated metal powder and an agglomeration agent; forming said first feedstock into a green state dense article; and removing said agglomeration agent. Furthermore, the present invention may include a second feedstock including an agglomerated metal powder, a space filling material and an agglomeration agent which may be formed into a green state porous article. The present invention also includes a dense and/or porous article manufactured by various methods, as well as methods for creating the dense and porous feedstocks. Moreover, the present invention may include an article which may be a medical implant.
Abstract translation: 在一个实施方案中,本发明可以是从金属粉末形成多孔和/或致密制品的方法,包括向模具中加入包含附聚金属粉末和附聚剂的第一原料; 将所述第一原料形成绿色致密制品; 并除去所述附聚剂。 此外,本发明可以包括第二原料,其包括可以形成绿色多孔制品的附聚金属粉末,空间填充材料和附聚剂。 本发明还包括通过各种方法制造的致密和/或多孔制品,以及用于产生致密和多孔原料的方法。 此外,本发明可以包括可以是医疗植入物的物品。
-
2.
公开(公告)号:US09259784B2
公开(公告)日:2016-02-16
申请号:US13786892
申请日:2013-03-06
Applicant: Howmedica Osteonics Corp.
Inventor: John Lapszynski , Lionel Fuentes, Jr.
CPC classification number: B22F5/10 , A61F2/3094 , A61F2/34 , A61F2002/30957 , A61F2002/30968 , B22F3/03 , B30B11/04
Abstract: A method for manufacturing a titanium acetabular cup shell includes obtaining a titanium powder. A three part mold having a first part with a part-spherical inner surface, a second ram part with a part-spherical outer impact surface and a third ram part with an annular impact surface are provided to compact the titanium powder. The second and third parts are aligned along an axis within the first part. The second part is aligned along a center axis within the annular impact surface of the third part. The first mold part is filled with the titanium powder. The second mold part-spherical outer surface and the third part annular surface are moved towards the part-spherical inner surface of the first part into contact with the powder. The powder is compacted with the second part part-spherical outer impact surface and the third part annular impact surface to about 50% of its initial volume.
Abstract translation: 钛髋臼杯壳的制造方法包括获得钛粉末。 提供三部分模具,其具有具有部分球形内表面的第一部分,具有部分球形外部冲击表面的第二冲头部分和具有环形冲击表面的第三冲头部分,以压实钛粉末。 第二和第三部分沿着第一部分内的轴线排列。 第二部分沿着第三部分的环形冲击表面内的中心轴线排列。 第一个模具部分填充有钛粉末。 第二模具部分球形外表面和第三部分环形表面朝向第一部分的部分球形内表面移动以与粉末接触。 粉末与第二部分球形外部冲击表面和第三部分环形冲击表面压实成其初始体积的约50%。
-
3.
公开(公告)号:US20140255241A1
公开(公告)日:2014-09-11
申请号:US13786892
申请日:2013-03-06
Applicant: HOWMEDICA OSTEONICS CORP.
Inventor: John Lapszynski , Lionel Fuentes, JR.
IPC: B22F5/10
CPC classification number: B22F5/10 , A61F2/3094 , A61F2/34 , A61F2002/30957 , A61F2002/30968 , B22F3/03 , B30B11/04
Abstract: A method for manufacturing a titanium acetabular cup shell includes obtaining a titanium powder. A three part mold having a first part with a part-spherical inner surface, a second ram part with a part-spherical outer impact surface and a third ram part with an annular impact surface are provided to compact the titanium powder. The second and third parts are aligned along an axis within the first part. The second part is aligned along a center axis within the annular impact surface of the third part. The first mold part is filled with the titanium powder. The second mold part-spherical outer surface and the third part annular surface are moved towards the part-spherical inner surface of the first part into contact with the powder. The powder is compacted with the second part part-spherical outer impact surface and the third part annular impact surface to about 50% of its initial volume.
Abstract translation: 钛髋臼杯壳的制造方法包括获得钛粉末。 提供三部分模具,其具有具有部分球形内表面的第一部分,具有部分球形外部冲击表面的第二冲头部分和具有环形冲击表面的第三冲头部分,以压实钛粉末。 第二和第三部分沿着第一部分内的轴线排列。 第二部分沿着第三部分的环形冲击表面内的中心轴线排列。 第一个模具部分填充有钛粉末。 第二模具部分球形外表面和第三部分环形表面朝向第一部分的部分球形内表面移动以与粉末接触。 粉末与第二部分球形外部冲击表面和第三部分环形冲击表面压实成其初始体积的约50%。
-
-