Abstract:
The disclosure provides a coating composition, a film made of the coating composition, and method for preparing the coating composition. The coating composition includes a product prepared from cross-linking a (a) polysilsesquioxane with a (b) compound with the structure represented by Formula (I): wherein R is independently a hydroxyl group, or C1-8 alkoxy group, R1 is a C3-12 epoxy group, C3-12 acrylate group, C3-12 alkylacryloxy group, C3-12 aminoalkyl group, C3-12 isocyanate-alkyl group, C3-12 alkylcarboxylic acid group, C3-12 alkyl halide group, C3-12 mercaptoalkyl group, C3-12 alkyl group, or C3-12 alkenyl group, and R2 is a hydroxyl group, C1-8 alkyl group, or C1-8 alkoxy group.
Abstract:
A method for manufacturing a water-based coating material is provided, including: (a) reacting tetraalkoxysilane, acidic aqueous solution of vanadium salt, and trialkoxyalkylsilane to form an oligomer; (b) reacting the oligomer with colloidal silica particles to form a modified oligomer; and (c) reacting the modified oligomer with trialkoxyepoxysilane to obtain a water-based coating material.
Abstract:
A resin composition formed by reacting a polyester-polyacid oligomer with a poly-epoxy oligomer is provided. The functionality of the resin composition is between 4 and 10. The weight average molecular weight of the resin composition is between 3,000 and 20,000 g/mol.
Abstract:
A method of manufacturing a hydrophobic antifouling coating material, including: (a) mixing a sol-gel precursor, water, an aqueous colloidal silica suspension, and a catalyst to perform a sol-gel reaction to form a solution having particles therein, wherein the sol-gel reaction is performed without addition of any organic solvent; (b) chemically modifying the particles with a hydrophobic agent to form surface-modified particles; and (c) adding a surfactant to the solution containing the surface-modified particles to form a hydrophobic antifouling coating material. The hydrophobic antifouling coating material can be dispersed in an aqueous solution, and has properties such as low VOC (Volatile organic compound) value, high solid content, and high stability.
Abstract:
A method for forming an inorganic passivation material is provided. The method includes mixing about 5 to 80 parts by weight of trialkoxysilane, about 10 to 80 parts by weight of tetraalkoxysilane, and about 1 to 30 parts by weight of catalyst to perform a reaction at pH of about 0.05 to 4 to form an inorganic resin material. The inorganic resin material is modified by phosphate ester to form an inorganic passivation material, wherein phosphate ester is about 0.1-10 parts by weight based on 100 parts by weight of the inorganic resin material. An inorganic passivation material and a passivation protective film produced therefrom are also provided.
Abstract:
An electrostatic chuck is provided, the electrostatic chuck includes a base; and an insulating layer, an electrode layer, a first dielectric layer, and a second dielectric layer sequentially stacked on the base. The first dielectric layer is aluminum oxide (Al2O3) or aluminum nitride (AlN). A material of the second dielectric layer is different from a material of the first dielectric layer, and the second dielectric layer includes titanium element, IVA group element, and oxygen element.
Abstract:
A polymer is provided, which is formed by reacting a diol having hydrogenated bisphenol group with a bis-epoxy compound. The diol having hydrogenated bisphenol group may have a chemical structure of wherein each of R1 is independently H or methyl, and m and n are independently integers of 1 to 4. The bis-epoxy compound can be or a combination thereof, wherein each of R2 is independently H or methyl, and each of R3 is independently H or methyl.
Abstract:
An organic-inorganic hybrid resin is formed by reacting a polyol organic resin with a polysilsesquioxane polymer. The organic-inorganic hybrid resin has T0, T1, T2, and T3 signals of 29Si-NMR, wherein a ratio of the sum of 3 times the integral value of T0 signal and 2 times the integral value of T1 signal and the integral value of T2 signal and the integral value of T3 signal ((3T0+2T1+T2)/T3) is from 0.3 to 1.2, wherein the T0 signal range is 35 ppm to 40 ppm, the T1 signal range is 48 ppm to 53 ppm, the T2 signal range is 55 ppm to 62 ppm, and the T3 signal range is 63 ppm to 72 ppm.
Abstract:
A compound serving as coalescing agent and a coating composition employing the compound are provided. The compound has a structure represented by Formula (I) wherein n is 0, 1, 2, or 3; m is 0, 1, 2, or 3; R1 is R2 is R3, R4, R5, and R6 are independently C1-12 alkyl group; and, R1 is distinct from R2 when n is equal to m.
Abstract:
The embodiments of the present disclosure provide a coating composition, including: polysilsesquioxane polymer modified organic resin represented by Formula (1): Wherein, R1 is C3-12 epoxy group, C3-12 acrylate group, C3-12 alkylacryloxy group, C3-12 aminoalkyl group, C3-12 isocyanate-alkyl group, C3-12 alkylcarboxylic acid group, C3-12 alkyl halide group, C3-12 mercaptoalkyl group, C3-12 alkyl group, or C3-12 alkenyl group; R2 is half oxygen(O1/2), hydroxyl group, C1-8 alkyl group, or C1-8 alkoxy group; R3 is halide group, C1-8 alkyl halide group, C1-8 alkoxy group, C1-12 alkyl group, or C5-20 aromatic ring; R4 is hydrogen or C1-8 alkyl group; R5 is modified or unmodified carbonyl compound moiety; n is a positive integer from 1 to 200; m is a positive integer from 10 to 500, and s is an integer from 0 to 250.