公开(公告)号:US20170349498A1
公开(公告)日:2017-12-07
申请号:US15538877
申请日:2015-12-18
Applicant: LAFARGE
Inventor: Freddy BERNARD , Pierre-Henri JEZEQUEL , Sandrine REBOUSSIN
IPC: C04B38/02 , C04B14/28 , C04B22/12 , C04B24/26 , B05D1/26 , B05D3/00 , C04B28/04 , C04B103/10 , C04B103/30 , C04B103/42 , C04B111/40 , C04B111/52
CPC classification number: C04B38/02 , B05D1/26 , B05D3/002 , C04B14/28 , C04B22/124 , C04B24/26 , C04B28/02 , C04B28/04 , C04B2103/10 , C04B2103/302 , C04B2103/42 , C04B2111/40 , C04B2111/52 , C04B2201/30 , Y02W30/92 , Y02W30/94 , C04B20/008 , C04B22/068 , C04B38/10 , C04B14/06 , C04B14/14 , C04B18/08 , C04B18/141 , C04B22/08
Abstract: A method for the continuous production of a mineral foam of which the density in the dry state (d) is from 40 to 600 kg/m3, includes (i) mixing cement; a water reducing agent; 0.5 to 10%, % by weight with respect to the total weight of cement, of ultrafine particles having a liquid-solid contact angle comprised from 30° to 140°, and of which the D50 is from 10 to 600 nm; water, with a water/cement weight ratio from 0.3 to 2.5; (ii) adding to the mixture from 0.5 to 10% of a pore-forming agent, % by weight with respect to the weight of cement; (iii) applying the mixture obtained at step (ii) on a support; (iv) leaving the mixture to expand on the support.