Abstract:
A thermoplastic composition comprises, based on the total weight of the thermoplastic composition, 10 to 45 wt. % of a poly(etherimide); 35 to 90 wt. % of a poly(carbonate-siloxane); 0.5 to 20 wt. % of compatibilizer polycarbonate component comprising a poly(carbonate-arylate ester); up to 15 wt. % of an ultraviolet light stabilizer; and 0 to 30 wt. % of TiO2; wherein a sample of the composition has a notched Izod impact energy of at least 200 J/m at 23° C. measured in accordance to ASTM D256; and an at least 50% higher notched Izod impact energy value compared to the composition without the compatibilizer component measured in accordance to ASTM D256.
Abstract:
A lens comprising a copolycarbonate comprising bisphenol A carbonate units and second carbonate units of the formula (I) and 2 to 40 ppm of an organosulfonic stabilizer of the formula (II), wherein the second carbonate units are present in an amount of 20 to 49 mol %, preferably 30 to 40 mol % based on the sum of the moles of the copolycarbonate and the bisphenol A homopolycarbonate; and the polycarbonate composition has: a Vicat B120 of 160° C. or higher measured according to ISO 306; and a yellowness index of less than 12, measured according to ASTM D1925.
Abstract:
A melt-blend composition is formed from, based on the total weight of the melt-blend composition, 0 to 5 wt. % of an additive; and 95 to 100 wt. % of a polymer composition, wherein the polymer composition comprises, based on the total weight of the polymer composition, 5 to 95 wt. % of a first copolycarbonate consisting of bisphenol A carbonate units and first additional second copolycarbonate consisting of bisphenol A carbonate units and second additional carbonate units (phthalimidine carbonate units); and 0.001 to 0.1 wt. % of a transesterification catalyst, wherein the melt-blended composition has a haze of less than 15% and a transmission greater than 75%, each measured using the color space CIE1931 (Illuminant C and a 2° observer) at a 3.2 mm thickness.
Abstract:
A thermoplastic composition comprises: a copolycarbonate comprising bisphenol A carbonate units and second carbonate units of the formula (I); and 2 to 40 ppm of an organosulfonic stabilizer of the formula (II); wherein the second carbonate units are present in an amount of 20 to 49 mol %, preferably 30 to 40 mol % based on the sum of the moles of the copolycarbonate and the bisphenol A homopolycarbonate, and optionally the copolycarbonate comprises less than 2 ppm by weight of each of an ion of lithium, sodium, potassium, calcium, magnesium, ammonium, chlorine, bromine, fluorine, nitrite, nitrate, phosphite, phosphate, sulfate, formate, acetate, citrate, oxalate, trimethylammonium, and triethylammonium, as measured by ion chromatography; and the thermoplastic composition has: a Vicat B120 of 160° C. or higher measured according to ISO 306; and a yellowness index of less than 12, measured according to ASTM D1925.
Abstract:
Seat components and claddings for railway molded or formed from a thermoplastic polymer composition comprising, based on the total weight of the composition, 50 to 93 wt. % of a specific polycarbonate; 4 to 30 wt. % of a poly(carbonate-siloxane) comprising bisphenol A carbonate units, and siloxane units; 3 to 20 wt. % of an organophosphorus compound in an amount effective to provide 0.1 to 2.0 wt. % of phosphorus, based on the total weight of the thermoplastic polymer composition; wherein an article having a thickness of 0.5 to 10 mm molded from the composition has a Ds-4 smoke density≦300 measured according to ISO 5659-2, and a MAHRE≦90 kW/m2 measured according to ISO 5660-1, a multiaxial impact energy≧100 J, and a ductility in multiaxial impact of 80 to 100% at +23° C. according to ISO 6603.
Abstract:
tic composition includes: a high heat polycarbonate comprising optional bisphenol A carbonate units and high heat carbonate units of the formula (1), (2), (3), or a combination thereof; optionally a bisphenol A homopolycarbonate; and 2 to 40 ppm of an organosulfonic stabilizer of the formula (a) wherein the high heat carbonate units are present in an amount of 20 to 49 mol %, preferably 30 to 40 mol % based on the sum of the moles of the high heat polycarbonate and the bisphenol A homopolycarbonate, and optionally the high heat polycarbonate comprises less than 2 ppm by weight of each of an ion of lithium, sodium, potassium, calcium, magnesium, ammonium, chlorine, bromine, fluorine, nitrite, nitrate, phosphite, phosphate, sulfate, formate, acetate, citrate, oxalate, trimethylammonium, and triethylammonium, as measured by ion chromatography; and the thermoplastic composition has: a Vicat B120 of 160° C. or higher measured according to ISO 306; and a yellowness index of less than 12, measured according to ASTM D1925.
Abstract:
A poly(carbonate-ester) copolymer including carbonate units of the formula (I); and ester units of the formula (II) wherein: T is a C2-20 alkylene, a C6-20 cycloalkylene, or a C6-20 arylene; and R1 and J are each independently a bisphenol A divalent group, or a phthalimidine divalent group or a third divalent group of the formula (III), (IV), (V), (VI) or (VII) wherein Xa is a C6-12 polycyclic aryl, C3-18 mono- or polycycloalkylene, C3-18 mono- or polycycloalkylidene, -(Q1)x-G-(Q2)y- group wherein Q1 and Q2 are each independently a C1-3 alkylene, G is a C3-10 cycloalkylene, x is 0 or 1, and y is 1, provided that the at least one bisphenol A divalent group, at least one phthalimidine divalent group, and at least one third divalent group are present in the poly(carbonate-ester) copolymer.
Abstract:
A thermoplastic composition comprises, based on the total weight of the thermoplastic composition, 10 to 45 wt. % of a poly(etherimide); 35 to 90 wt. % of a polycarbonate component comprising a polycarbonate homopolymer, a poly(carbonate-siloxane), or a combination thereof; 0.5 to 20 wt. % of a compatibilizer polycarbonate component comprising a poly(carbonate-arylate ester), a phthalimidine copolycarbonate, or a combination thereof; up to 5 wt. % of an ultraviolet light stabilizer; and 0 to 20 wt. % of TiO2, wherein a sample of the composition has a 50% higher notched Izod impact energy value compared to the composition without the compatibilizer component.
Abstract:
A thermoplastic composition comprises: a copolycarbonate comprising bisphenol A carbonate units and second carbonate units of the formula (I) and optionally, a bisphenol A homopolycarbonate; wherein the second carbonate units are present in an amount of 10 to 49 mol % based on the sum of the moles of the copolycarbonate and the bisphenol A homopolycarbonate, the copolycarbonate comprises less than 2 ppm by weight of each of an ion of lithium, sodium, potassium, calcium, magnesium, ammonium, chlorine, bromine, fluorine, nitrite, nitrate, phosphite, phosphate, sulfate, formate, acetate, citrate, oxalate, trimethylammonium, and triethylammonium, as measured by ion chromatography, and the thermoplastic composition has a bisphenol A purity of at least 99.6%, or at least 99.7% as determined by high performance liquid chromatography. The thermoplastic composition has a Vicat B120 of 155° C. or higher; and an increase in yellowness index of less than 10 during 1000 hours of heat aging at 155° C.
Abstract:
A copolycarbonate lens formed from a polycarbonate composition comprising: a copolycarbonate comprising bisphenol A carbonate units and of phthalimide carbonate and optionally, a bisphenol A homopolycarbonate; wherein the second carbonate units are present in an amount of 18 to 35 mol % based on the sum of the moles of the copolycarbonate and the bisphenol A homopolycarbonate, the copolycarbonate comprises less than 2 ppm by weight of each of an ion of lithium, sodium, potassium, calcium, magnesium, ammonium, chlorine, bromine, fluorine, nitrite, nitrate, phosphite, phosphate, sulfate, formate, acetate, citrate, oxalate, trimethylammonium, and triethylammonium, as measured by ion chromatography, and the polycarbonate composition has a bisphenol A purity of at least 99.7% as determined by high performance liquid chromatography. The polycarbonate composition has: a Vicat B120 of 155° C. or higher; and an increase in yellowness index of less than 10 during 1000 hours of heat aging at 155° C.