Abstract:
A cast part includes an outermost wall, at least one inner wall defining at least two internal passages and at least one cast cooling fin extending from an outer surface. The cooling fin includes a ratio of fin height to an average fin thickness that is greater than 2.0 and no more than 18.0. A method is also disclosed.
Abstract:
A method of fabricating a casting is provided. The method includes creating a mixture of ceramic powder and a binder, pouring the mixture around sacrificial patterns, executing a first thermal treatment to set the mixture into a solid mold without damaging the sacrificial patterns, executing a second thermal treatment to remove the sacrificial patterns without removing any of the binder from the solid mold, executing at least one of a third thermal treatment and a chemical treatment to remove a quantity of the binder to transform the solid mold into a solid breakaway mold and pouring molten metallic material into the solid breakaway mold.
Abstract:
An alloy part is cast in a mold (280) having a part-forming cavity (292, 294, 296). The method comprises pouring a first alloy into the mold. The pouring causes: a surface (550) of the first alloy in the part-forming cavity to raise relative to the part-forming cavity; a branch flow of the poured first alloy to pass upwardly through a first portion (304) of a passageway; and the branch flow to pass downwardly through a second portion (310), of the passageway; solidifying some of the first alloy in the passageway to block the passageway while at least some of the first alloy in the part-forming cavity remains molten. A second alloy is poured into the mold atop the first alloy and solidified.
Abstract:
A process for casting a single crystal axis-symmetric thick walled tube comprising forming a axisymmetric single crystal ring seed around a circular internal core, wherein the ring seed has an inner diameter and a taper on the inner diameter, and wherein the internal core has an outer diameter and a matching taper on the outer diameter, the matching taper matching the taper of the inner diameter of the ring seed, and the internal core being free to translate in a vertical direction relative to the ring seed; and heating the ring seed so as to expand the ring seed relative to the internal core, and allowing the circular internal core to translate relative to the ring seed in a direction of the force of gravity, thereby maintaining contact between the circular internal core and the ring seed.
Abstract:
A method comprises: providing a spiral metallic workpiece having a cast structure associated with such spiral; and at least partially flattening the workpiece.
Abstract:
A foam for use in a lost-foam casting process utilized in the manufacture of a component for a gas turbine engine, the foam having a void fraction less than or equal to ninety five percent, is disclosed. The foam may include a first layer comprising polymer foam having an open-cell structure and a void fraction greater than ninety five percent. A second layer, comprising adhesive, may be adhered to the first layer. A third layer comprising particulate material may be adhered to the second layer.
Abstract:
A method for die casting a component includes inserting at least one sacrificial core into a die cavity of a die comprised of a plurality of die elements. Molten metal is injected into the die cavity. The molten metal is solidified within the die cavity to form the component. The plurality of die elements are disassembled from the component, and the at least one sacrificial core is destructively removed from the component.
Abstract:
A method to manufacture reticulated metal foam via a dual investment, includes pre-investment of a precursor with a diluted pre-investment ceramic plaster then applying an outer mold to the encapsulated precursor as a shell-mold.
Abstract:
A casting mold assembly includes an airfoil defining section and a casting core. The airfoil defining section includes an outer mold wall and a direct-shelled inner mold wall. The direct-shelled inner mold wall is disposed within a forward chordwise portion of the airfoil defining section. The direct-shelled inner mold wall includes an aft end having an external radius measuring more than about 0.075 in. (1.9 mm). The casting core is secured within an aft chordwise portion of the airfoil defining section, and includes an aft end with an external radius measuring less than about 0.075 in. (1.9 mm). A cast component and a method for making the casting mold assembly are also disclosed.
Abstract:
A high-temperature die casting die includes a first die plate with a first recess and a second die plate with a second recess, the first and second recesses defining a main part cavity and gating. A grain selector is in fluid communication with the main cavity, and an in situ zone refining apparatus is adapted to apply a localized thermal gradient to at least one of the first and second die plates. The localized thermal gradient and the at least one die plate are movable relative to each other so as to apply the localized thermal gradient along a first direction extending from the grain selector longitudinally across the main part cavity.