    Abstract: The invention relates to a method for producing a field emission layer (3), preferably for luminescent screen applications, according to which in order to improve the serviceable life and long-time stability, a mixture consisting of a polymer (11) and carbon nanofibers (4), which are hardened in a low-oxygen, in particular, oxygen-free atmosphere at temperatures greater than 2000° C., particularly greater than 2500° C., preferably, approximately 3000° C., are applied to a cathode electrode (8) assigned to a cathode (1), and the cathode electrode (8), together with the carbon nanofibers (4)/polymer (11) mixture is heated to a temperature ranging from 300° C. to 500° C., preferably from 380° C. to 480° C., in particular, from 420° C. to 450° C. in an atmosphere at least containing oxygen, e.g. air, a consequence of the oxygen results in a pyrolysis and/or to a hardening of the polymeric base (7), and at least a portion of the carbon nanofibers (4) is exposed over at least a portion of the spatial extension of the carbon nanofibers (4), particularly at least over a portion of the length of the carbon nanofibers (4), in particular, at least over half the length.

    Abstract translation: 本发明涉及一种用于制造场致发射层(3)的方法,优选用于荧光屏应用,为了提高使用寿命和长时间的稳定性,由聚合物(11)和碳纳米纤维组成的混合物 (4),其在低氧下硬化,特别是在大于2000℃,特别是大于2500℃,优选约3000℃的温度下的无氧气氛被施加到阴极 将分配给阴极(1)的电极(8)和阴极电极(8)与碳纳米纤维(4)/聚合物(11)混合物一起加热至300℃至500℃的温度。 ,优选380℃至480℃,特别是420℃至450℃,至少含氧气氛,例如 空气,氧气的结果导致聚合物基质(7)的热解和/或硬化,并且至少一部分碳纳米纤维(4)暴露在空气延伸部分的至少一部分上 碳纳米纤维(4),特别是碳纳米纤维(4)的至少一部分长度,特别是至少长度的一半以上。

Patent Agency Ranking