公开(公告)号:ES2162468T3
公开(公告)日:2001-12-16
申请号:ES98946407
申请日:1998-08-21
Applicant: BASF AG
Inventor: GUTSCHE HERBERT , ANDERLIK RAINER , KRESS NORBERT , GRESS DIETER , BRIAN BERND , BAIERWECK PETRA
Abstract: A continuous process for preparing pigmented thermoplastic molding compositions in an extruder, comprisesI) in a first zoneA) metering in from 10 to 99.999% by weight of a thermoplastic polymer into an extruder andII) in a subsequent zone at temperatures below the respective glass transition temperature of the thermoplastic A)B) adding from 0.001 to 60% by weight of a colorant andthen heating the thermoplastic/colorant mixture in the subsequent zones, homogenizing the polymer melt and extruding the resultant mixture.
-
公开(公告)号:CA2302487A1
公开(公告)日:1999-03-18
申请号:CA2302487
申请日:1998-08-21
Applicant: BASF AG
Inventor: GUTSCHE HERBERT , ANDERLIK RAINER , BRANDT HERMANN , KRESS NORBERT , HEEL HELMUT , BRIAN BERND , BAIERWECK PETRA , GRESS DIETER , MOSNER HERBERT
Abstract: The invention relates to a continuous method for producing dyed thermoplastic moulding materials in an extruder, as follows: I) in a first area, A) 10 to 99.999 wt. % of a thermoplastic polymer is metered into an extruder. II) In a subsequent area, B) 0.001 to 60 wt. % of a dye is added at a temperature below the particular glass transition temperature of the thermoplastic A). In the subsequent areas, the thermoplastic/dye mixture is heated, the polymer melt is homogenised and the resulting mixture is extruded.
-
公开(公告)号:AT274028T
公开(公告)日:2004-09-15
申请号:AT99970101
申请日:1999-09-29
Applicant: BASF AG
Inventor: FISCHER MICHAEL , WEBER MARTIN , GINSS CHRISTOPHE , BERZ STEPHAN , KRESS NORBERT
IPC: C08J5/04 , C08F265/04 , C08F279/02 , C08K3/40 , C08K5/00 , C08K7/14 , C08L25/08 , C08L25/12 , C08L25/14 , C08L51/00 , C08L51/06 , C08L55/02 , C08L67/02 , C08L67/03 , C08L101/10 , C08L51/04
Abstract: The invention relates to a fiber-reinforced thermoplastic moulding material containing the following ingredients in relation to the sum of ingredients A-D and optionally E and F, representing a total of 100 wt. %: d) 10-97 wt. % of at least one aromatic polyester as ingredient A; e) 1-50 wt. % of at least one particle-shaped grafted copolymer with a soft phase glass transition temperature that is lower than 0 DEG C and an average particle size of 50-1000 nm as ingredient B; f) 1-50 wt. % of at least one copolymer made of monomers c1) 50-90 wt. % of at least one vinyl aromatic monomer as ingredient C1 and c2) 10-25 wt. % acrylonitrile and/or methacrylonitrile as ingredient C2, as ingredient C; 1-50 wt. % glass fibers as ingredient D; f) 0-25 wt. % other ingredients that are compatible, can be mixed in a homogenous manner with ingredients A and/or C and can be dispersed therein, as ingredient E; f) 0-10 wt. % usual additives such as UV stabilizers, oxidation retarders, lubricating agents and release agents as ingredient F. The invention also relates to moulded parts made from said moulding materials and used in the interiors of motor vehicles. The invention further relates to the use of moulding materials in the production of moulded parts.
-
公开(公告)号:DE59910301D1
公开(公告)日:2004-09-23
申请号:DE59910301
申请日:1999-09-29
Applicant: BASF AG
Inventor: FISCHER MICHAEL , WEBER MARTIN , GINSS CHRISTOPHE , BERZ STEPHAN , KRESS NORBERT
IPC: C08J5/04 , C08F265/04 , C08F279/02 , C08K3/40 , C08K5/00 , C08K7/14 , C08L25/08 , C08L25/12 , C08L25/14 , C08L51/00 , C08L51/06 , C08L55/02 , C08L67/02 , C08L67/03 , C08L101/10
Abstract: The invention relates to a fiber-reinforced thermoplastic moulding material containing the following ingredients in relation to the sum of ingredients A-D and optionally E and F, representing a total of 100 wt. %: d) 10-97 wt. % of at least one aromatic polyester as ingredient A; e) 1-50 wt. % of at least one particle-shaped grafted copolymer with a soft phase glass transition temperature that is lower than 0 DEG C and an average particle size of 50-1000 nm as ingredient B; f) 1-50 wt. % of at least one copolymer made of monomers c1) 50-90 wt. % of at least one vinyl aromatic monomer as ingredient C1 and c2) 10-25 wt. % acrylonitrile and/or methacrylonitrile as ingredient C2, as ingredient C; 1-50 wt. % glass fibers as ingredient D; f) 0-25 wt. % other ingredients that are compatible, can be mixed in a homogenous manner with ingredients A and/or C and can be dispersed therein, as ingredient E; f) 0-10 wt. % usual additives such as UV stabilizers, oxidation retarders, lubricating agents and release agents as ingredient F. The invention also relates to moulded parts made from said moulding materials and used in the interiors of motor vehicles. The invention further relates to the use of moulding materials in the production of moulded parts.
-
公开(公告)号:DE59801094D1
公开(公告)日:2001-08-30
申请号:DE59801094
申请日:1998-08-21
Applicant: BASF AG
Inventor: GUTSCHE HERBERT , ANDERLIK RAINER , KRESS NORBERT , GRESS DIETER , BRIAN BERND , BAIERWECK PETRA , MOSNER HERBERT , BRANDT HERMANN , HEEL HELMUT
Abstract: A continuous process for preparing pigmented thermoplastic molding compositions in an extruder, comprisesI) in a first zoneA) metering in from 10 to 99.999% by weight of a thermoplastic polymer into an extruder andII) in a subsequent zone at temperatures below the respective glass transition temperature of the thermoplastic A)B) adding from 0.001 to 60% by weight of a colorant andthen heating the thermoplastic/colorant mixture in the subsequent zones, homogenizing the polymer melt and extruding the resultant mixture.
-
公开(公告)号:CA2302487C
公开(公告)日:2006-11-28
申请号:CA2302487
申请日:1998-08-21
Applicant: BASF AG
Inventor: GUTSCHE HERBERT , BRIAN BERND , KRESS NORBERT , MOSNER HERBERT , BRANDT HERMANN , GRESS DIETER , HEEL HELMUT , BAIERWECK PETRA , ANDERLIK RAINER
Abstract: The invention relates to a continuous method for producing dyed thermoplasti c moulding materials in an extruder, as follows: I) in a first area, A) 10 to 99.999 wt. % of a thermoplastic polymer is metered in to an extruder. II) In a subsequent area, B) 0.001 to 60 wt. % of a dye is added at a temperature below the particular glass transition temperature of the thermoplastic A). In the subsequent areas, the thermoplastic/dye mixture is heated, the polymer melt is homogenised and the resulting mixture is extruded.
-
公开(公告)号:BR9914113A
公开(公告)日:2001-06-12
申请号:BR9914113
申请日:1999-09-29
Applicant: BASF AG
Inventor: FISCHER MICHAEL , WEBER MARTIN , GINSS CHRISTOPHE , BERZ STEPHAN , KRESS NORBERT
IPC: C08J5/04 , C08F265/04 , C08F279/02 , C08K3/40 , C08K5/00 , C08K7/14 , C08L25/08 , C08L25/12 , C08L25/14 , C08L51/00 , C08L51/06 , C08L55/02 , C08L67/02 , C08L67/03 , C08L101/10
Abstract: The invention relates to a fiber-reinforced thermoplastic moulding material containing the following ingredients in relation to the sum of ingredients A-D and optionally E and F, representing a total of 100 wt. %: d) 10-97 wt. % of at least one aromatic polyester as ingredient A; e) 1-50 wt. % of at least one particle-shaped grafted copolymer with a soft phase glass transition temperature that is lower than 0 DEG C and an average particle size of 50-1000 nm as ingredient B; f) 1-50 wt. % of at least one copolymer made of monomers c1) 50-90 wt. % of at least one vinyl aromatic monomer as ingredient C1 and c2) 10-25 wt. % acrylonitrile and/or methacrylonitrile as ingredient C2, as ingredient C; 1-50 wt. % glass fibers as ingredient D; f) 0-25 wt. % other ingredients that are compatible, can be mixed in a homogenous manner with ingredients A and/or C and can be dispersed therein, as ingredient E; f) 0-10 wt. % usual additives such as UV stabilizers, oxidation retarders, lubricating agents and release agents as ingredient F. The invention also relates to moulded parts made from said moulding materials and used in the interiors of motor vehicles. The invention further relates to the use of moulding materials in the production of moulded parts.
-
公开(公告)号:ES2226499T3
公开(公告)日:2005-03-16
申请号:ES99970101
申请日:1999-09-29
Applicant: BASF AG
Inventor: FISCHER MICHAEL , WEBER MARTIN , GINSS CHRISTOPHE , BERZ STEPHAN , KRESS NORBERT
IPC: C08J5/04 , C08F265/04 , C08F279/02 , C08K3/40 , C08K5/00 , C08K7/14 , C08L25/08 , C08L25/12 , C08L25/14 , C08L51/00 , C08L51/06 , C08L55/02 , C08L67/02 , C08L67/03 , C08L101/10
Abstract: Empleo de masas de moldeo termoplásticas reforzadas por fibra de vidrio, que contienen, referido a la suma de los componentes A hasta D y, en caso dado, E y F, resultando la totalidad de un 100 % en peso, a) de un 10 hasta un 97 % en peso de al menos un poliéster aromático como componente A, b) de un 1 hasta un 50 % en peso de al menos un copolímero de injerto en forma de partículas con una temperatura de transición vítrea de la fase elástica por debajo de los 0ºC y un tamaño de partículas medio de 50 hasta 1000 nm como componente B, c) de un 1 hasta un 50 % en peso de al menos un copolímero, formado por los monómeros c1) de un 50 hasta un 90 % en peso de al menos un monómero vinilaromático como componente c1, y c2) de un 10 hasta un 25 % en peso de acrilonitrilo y/o metacrilonitrilo como componente C2, como componente C, d) de un 1 hasta un 50 % en peso de fibras de vidrio como componente D, e) de un 0 hasta un 25 % en peso de otros polímeros compatibles con los componentes A y/o C homogéneamente miscibles o dispersables en estos como componente E, y f) de un 0 hasta un 10 % en peso de aditivos habituales, como estabilizantes de UV, hollín, pigmentos, retardantes de la oxidación, lubricantes y agentes de desmoldeo como componente F, para la obtención de piezas moldeadas para el espacio interno de vehículos.
-
公开(公告)号:CZ20011174A3
公开(公告)日:2001-11-14
申请号:CZ20011174
申请日:1999-09-29
Applicant: BASF AG
Inventor: FISCHER MICHAEL , WEBER MARTIN , GINSS CHRISTOPHE , BERZ STEPHAN , KRESS NORBERT
IPC: C08J5/04 , C08F265/04 , C08F279/02 , C08K3/40 , C08K5/00 , C08K7/14 , C08L25/08 , C08L25/12 , C08L25/14 , C08L51/00 , C08L51/06 , C08L55/02 , C08L67/02 , C08L67/03 , C08L101/10
Abstract: The invention relates to a fiber-reinforced thermoplastic moulding material containing the following ingredients in relation to the sum of ingredients A-D and optionally E and F, representing a total of 100 wt. %: d) 10-97 wt. % of at least one aromatic polyester as ingredient A; e) 1-50 wt. % of at least one particle-shaped grafted copolymer with a soft phase glass transition temperature that is lower than 0 DEG C and an average particle size of 50-1000 nm as ingredient B; f) 1-50 wt. % of at least one copolymer made of monomers c1) 50-90 wt. % of at least one vinyl aromatic monomer as ingredient C1 and c2) 10-25 wt. % acrylonitrile and/or methacrylonitrile as ingredient C2, as ingredient C; 1-50 wt. % glass fibers as ingredient D; f) 0-25 wt. % other ingredients that are compatible, can be mixed in a homogenous manner with ingredients A and/or C and can be dispersed therein, as ingredient E; f) 0-10 wt. % usual additives such as UV stabilizers, oxidation retarders, lubricating agents and release agents as ingredient F. The invention also relates to moulded parts made from said moulding materials and used in the interiors of motor vehicles. The invention further relates to the use of moulding materials in the production of moulded parts.
-
公开(公告)号:AU5982499A
公开(公告)日:2000-04-26
申请号:AU5982499
申请日:1999-09-29
Applicant: BASF AG
Inventor: FISCHER MICHAEL , WEBER MARTIN , GINSS CHRISTOPHE , BERZ STEPHAN , KRESS NORBERT
IPC: C08J5/04 , C08F265/04 , C08F279/02 , C08K3/40 , C08K5/00 , C08K7/14 , C08L25/08 , C08L25/12 , C08L25/14 , C08L51/00 , C08L51/06 , C08L55/02 , C08L67/02 , C08L67/03 , C08L101/10
Abstract: The invention relates to a fiber-reinforced thermoplastic moulding material containing the following ingredients in relation to the sum of ingredients A-D and optionally E and F, representing a total of 100 wt. %: d) 10-97 wt. % of at least one aromatic polyester as ingredient A; e) 1-50 wt. % of at least one particle-shaped grafted copolymer with a soft phase glass transition temperature that is lower than 0 DEG C and an average particle size of 50-1000 nm as ingredient B; f) 1-50 wt. % of at least one copolymer made of monomers c1) 50-90 wt. % of at least one vinyl aromatic monomer as ingredient C1 and c2) 10-25 wt. % acrylonitrile and/or methacrylonitrile as ingredient C2, as ingredient C; 1-50 wt. % glass fibers as ingredient D; f) 0-25 wt. % other ingredients that are compatible, can be mixed in a homogenous manner with ingredients A and/or C and can be dispersed therein, as ingredient E; f) 0-10 wt. % usual additives such as UV stabilizers, oxidation retarders, lubricating agents and release agents as ingredient F. The invention also relates to moulded parts made from said moulding materials and used in the interiors of motor vehicles. The invention further relates to the use of moulding materials in the production of moulded parts.
-
-
-
-
-
-
-
-
-