公开(公告)号:ES2191178T3
公开(公告)日:2003-09-01
申请号:ES97925012
申请日:1997-05-28
Applicant: BASF AG
Inventor: GUNTHERBERG NORBERT , WEBER MARTIN
Abstract: Thermoplastic molding materials containA) polycarbonatesB) elastomeric graft copolymers,C+D) two different, thermoplastic copolymers based on styrene or alpha-methylstyrene,E) copolymers based on alkyl(meth)acrylate andF) polymeric, OH-containing compounds.
-
公开(公告)号:DE10155157A1
公开(公告)日:2003-05-22
申请号:DE10155157
申请日:2001-11-12
Applicant: BASF AG
Inventor: ALIG INGO , HOLST MARCO , WEBER MARTIN
Abstract: The invention relates to moulding materials containing A) between 40 and 99 wt. % of at least one epoxy resin, B) between 1 and 60 wt. % of at least one polyarylene ether sulfone containing side groups or terminal groups selected from the group of carboxyl and anhydride groups, C) between 0 and 60 wt. % of at least one polyarylene ether sulfone containing essentially no side groups or terminal groups selected from the group of carboxyl and anhydride groups, D) between 0 and 60 wt. % of at least one filling material, and E) between 0 and 40 wt. % of one addition agent or a plurality of different addition agents, the total weight percent of constituents A to E amounting to 100 %. The invention also relates to a method for producing said moulding materials, to the use thereof and to moulded parts which can be obtained from the inventive moulding materials.
-
公开(公告)号:AT231533T
公开(公告)日:2003-02-15
申请号:AT97925012
申请日:1997-05-28
Applicant: BASF AG
Inventor: GUENTHERBERG NORBERT , WEBER MARTIN
Abstract: Thermoplastic molding materials containA) polycarbonatesB) elastomeric graft copolymers,C+D) two different, thermoplastic copolymers based on styrene or alpha-methylstyrene,E) copolymers based on alkyl(meth)acrylate andF) polymeric, OH-containing compounds.
-
114.
公开(公告)号:MXPA02005636A
公开(公告)日:2002-09-02
申请号:MXPA02005636
申请日:2000-12-06
Applicant: BASF AG
Inventor: WEBER MARTIN
IPC: C08K3/00 , C08K5/09 , C08K5/49 , C08K7/02 , C08J5/00 , C08L25/12 , C08L33/06 , C08L51/00 , C08L51/04 , C08L67/00 , C08L69/00 , D01F6/92 , C08L67/02
Abstract: Se describe un material de moldeo termoplastico que contiene: a) de 1 a 97.5% en peso de al menos un policarbonato aromatico, b) de 1 a 97.5% en peso de al menos un polimero de injerto de b1) de 40 a 80% en peso de una base de injerto elaborada de un polimero de hule- elastico, b2) de 20 a 60% en peso de una capa de injerto de b21) de 60 a 95% en peso de estireno o de estirenos substituidos con alquilo y b22) de 5 a 40% en peso de al menos un nitrilo insaturado, c) de 1 a 97.5% en peso de al menos un copolimero termoplastico de c1) de 60 a 85% en peso de estireno o estirenos substituidos con alquilo y c2) de 15 a 40% en peso de al menos un nitrilo insaturado, d) de 0.5 a 25% en peso de una mezcla que consiste de d1) de 5 a 95% en peso de al menos un relleno o carga mineral en particulas y d2) de 5 a 95% en peso de rellenos o cargas fibrosas, en donde al menos 50% en peso de los rellenos o cargas fibrosas se proporcionan con una longitud de al menos 50 ?m, y opcionalmente contenidos adicionales.
-
公开(公告)号:DE59804926D1
公开(公告)日:2002-08-29
申请号:DE59804926
申请日:1998-11-06
Applicant: BASF AG
Inventor: WEBER MARTIN , FISCHER MICHAEL , BLINNE GERD
Abstract: The thermoplastic molding composition comprises, based on the total weight of components A, C and, if desired, B and D to G, which is 100% by weight in total,a: as component A, from 1 to 99% by weight of at least one polyester,b: as component B, from 0 to 98% by weight of at least one polycarbonate,c: from 1 to 80% by weight of a specific graft copolymer C,d: as component D, from 0 to 80% by weight of at least one styrene copolymer,e: as component E, from 0 to 30% by weight of at least one rubber,f: as component F, from 0 to 60% by weight of at least one fibrous or particulate filler, andg: as component G, from 0 to 20% by weight of other additives.
-
公开(公告)号:DE10020785A1
公开(公告)日:2001-10-31
申请号:DE10020785
申请日:2000-04-28
Applicant: BASF AG
Inventor: WEBER MARTIN , QUEISSER JOACHIM
IPC: C08J5/00 , C08G59/24 , C08K3/16 , C08K7/02 , C08L77/00 , C08L77/02 , C08L77/06 , C08L81/06 , D01F6/76 , D01F6/90 , C08J5/04 , C08J5/18 , C08L21/00 , C08L63/00
Abstract: The invention relates to a thermoplastic moulding compound containing the components A, C, D, E, and optionally B, F and G, whose total weight constitutes 100 % by weight, and component H, said components being: a) 5-94.8 wt.- % of at least one polyarylether sulphone as component A, b) 0-20 wt.- % of at least one functionalised polyarylether sulphone as component B, c) 5-94.8 wt.- % of at least one polyamide as component C, d) 0.1-10 wt.- % of at least one epoxy resin as component D, e) 0.1-60 wt.- % fibre or particle-type filler or mixtures thereof as component E, f) 0-40 wt.- % of rubbers, whose resistance to impact has been modified and which contain functional groups, as component F, g) 0-40 wt.- % of additional conventional additives and processing aids as component G, h) 100 ppm-0.5 wt.- %, in relation to the quantities of components A to G, of copper bromide and/or copper iodide as component H.
-
公开(公告)号:TR200002493T2
公开(公告)日:2001-07-23
申请号:TR200002493
申请日:1999-02-26
Applicant: BASF AG
Inventor: MOHRSCHLADT RALF , WEBER MARTIN , HILDEBRANT VOLKER
IPC: C08G69/00 , C08G69/04 , C08L25/04 , C08L51/04 , C08L71/00 , C08L71/12 , C08L77/00 , C08L79/08 , C08L81/06 , C08L101/00
Abstract: The process for producing polymer blends by reacting at least one aminonitrile with water in the presence of thermoplastic polymers and optionally further polyamide-forming monomers comprises the following steps:(1) reacting at least one aminonitrile with water at a temperature from 90 to 400° C. and a pressure from 0.1 to 35x106 Pa to obtain a reaction mixture,(2) further reacting the reaction mixture at a temperature from 150 to 400° C. and a pressure which is lower than the pressure in step 1, the temperature and pressure being selected so as to obtain a first gas phase and a first liquid or a first solid phase or a mixture of first solid and first liquid phase and the first gas phase is separated from the first liquid or the first solid phase or the mixture of first liquid and first solid phase, and(3) admixing the first liquid or the first solid phase or the mixture of first liquid and first solid phase with a gaseous or liquid phase comprising water, which phase may contain thermoplastic polymers and optionally further polyamide-forming monomers, at a temperature from 150 to 370° C. and a pressure from 0.1 to 30x106 Pa to obtain the polymer blend,wherein in one or more of the steps the thermoplastic polymers and optionally further polyamide-forming monomers are added.
-
公开(公告)号:DE19941444A1
公开(公告)日:2001-03-01
申请号:DE19941444
申请日:1999-08-30
Applicant: BASF AG
Inventor: GOTTSCHALK AXEL , GEPRAEGS MICHAEL , WUENSCH JOSEF , WEBER MARTIN
-
公开(公告)号:DE10027161A1
公开(公告)日:2001-01-11
申请号:DE10027161
申请日:2000-05-31
Applicant: BASF AG
Inventor: WEBER MARTIN , QUEISSER JOACHIM
IPC: C08F265/04 , C08F265/08 , C08F279/02 , C08F285/00 , C08G67/02 , C08L51/00 , C08L51/04 , C08L55/02 , C08L67/00 , C08L67/02 , C08L69/00 , C08L73/00 , C08J5/18 , C08L47/00 , C08L51/06
Abstract: Thermoplastic molding composition comprises: (A) functionalized carbon monoxide copolymers; (B) thermoplastic polyesters; Thermoplastic molding composition comprises: (A) 1-99 wt.% functionalized carbon monoxide copolymers; (B) 10-99 wt.% thermoplastic polyesters; (C) 0-98 wt.% unfunctionalized carbon monoxide copolymers; and (D) 0-80 wt.% further additives. An Independent claim is included for molded articles made from the above composition.
-
公开(公告)号:CZ20003127A3
公开(公告)日:2000-12-13
申请号:CZ20003127
申请日:1999-02-26
Applicant: BASF AG
Inventor: MOHRSCHLADT RALF , WEBER MARTIN , HILDEBRANDT VOLKER
IPC: C08G69/00 , C08G69/04 , C08L25/04 , C08L51/04 , C08L71/00 , C08L71/12 , C08L77/00 , C08L79/08 , C08L81/06 , C08L101/00
Abstract: The process for producing polymer blends by reacting at least one aminonitrile with water in the presence of thermoplastic polymers and optionally further polyamide-forming monomers comprises the following steps:(1) reacting at least one aminonitrile with water at a temperature from 90 to 400° C. and a pressure from 0.1 to 35x106 Pa to obtain a reaction mixture,(2) further reacting the reaction mixture at a temperature from 150 to 400° C. and a pressure which is lower than the pressure in step 1, the temperature and pressure being selected so as to obtain a first gas phase and a first liquid or a first solid phase or a mixture of first solid and first liquid phase and the first gas phase is separated from the first liquid or the first solid phase or the mixture of first liquid and first solid phase, and(3) admixing the first liquid or the first solid phase or the mixture of first liquid and first solid phase with a gaseous or liquid phase comprising water, which phase may contain thermoplastic polymers and optionally further polyamide-forming monomers, at a temperature from 150 to 370° C. and a pressure from 0.1 to 30x106 Pa to obtain the polymer blend,wherein in one or more of the steps the thermoplastic polymers and optionally further polyamide-forming monomers are added.
-
-
-
-
-
-
-
-
-