公开(公告)号:JPS5865073A
公开(公告)日:1983-04-18
申请号:JP16238481
申请日:1981-10-12
Applicant: KAO CORP
Inventor: TSUNODA YUUZOU , MINEGISHI YUTAKA , YAMASHITA KAZUTAKA
IPC: D06M15/00 , D06M15/263
-
公开(公告)号:JPS52126427A
公开(公告)日:1977-10-24
申请号:JP4318576
申请日:1976-04-16
Applicant: KAO CORP
Inventor: TAKAMORI SHIGERU , YAMASHITA KAZUTAKA , KOUNO YOSHINAO
IPC: C09D5/03 , C08G59/00 , C08G63/668 , C08L63/00 , C08L67/00 , C09D163/00
Abstract: PURPOSE:A resinous composition for powder coating characterized by the excellent properties of surface evenness, adhesion, impact resistance, hardness, etc. comprises the certain polycarboxylic acid formulated with the epoxy compound.
-
公开(公告)号:JP2006305191A
公开(公告)日:2006-11-09
申请号:JP2005133412
申请日:2005-04-28
Inventor: HASEBE MANABU , ENOMOTO HARUOMI , YAMASHITA KAZUTAKA
IPC: A45D34/04
Abstract: PROBLEM TO BE SOLVED: To provide mascara cosmetic equipment in which deformation such as swelling hardly occurs even when a mascara applicator is immersed in a mascara agent for a long period of time and the degradation of a combing effect and the holdability of the mascara agent is prevented. SOLUTION: The mascara cosmetic equipment 33 is provided with a container 31 housing the mascara agent 30 containing water or alcohol, and the mascara applicator 10 whose application part 12 is immersed in the mascara agent. The application part 12 of the mascara applicator 10 is constituted of an application part shaft 21 and comb teeth 20. The comb teeth 20 are constituted of an elastomer material whose main component is a polyester elastomer or polyurethane elastomer and Shore hardness (A) is 45-85. COPYRIGHT: (C)2007,JPO&INPIT
Abstract translation: 要解决的问题:为了提供即使当睫毛膏涂抹器长时间浸入睫毛膏剂时也难以发生诸如溶胀等变形的睫毛膏化妆品设备,以及梳理效果的降低和梳理效果的保持性 防止睫毛膏剂。 解决方案:睫毛膏化妆品设备33设置有容纳含有水或醇的睫毛膏剂30的容器31和其施用部分12浸入睫毛膏剂中的睫毛膏涂抹器10。 睫毛膏涂敷器10的涂布部件12由涂敷部件轴21和梳齿20构成。梳齿20由主要成分为聚酯弹性体或聚氨酯弹性体的弹性体材料构成,肖氏硬度(A)为45 -85。 版权所有(C)2007,JPO&INPIT
-
公开(公告)号:JP2006271962A
公开(公告)日:2006-10-12
申请号:JP2006058564
申请日:2006-03-03
Inventor: IGAKI MICHIHITO , NAGASHIMA YOSHINAO , ISHIKAWA SHUJI , YAMASHITA KAZUTAKA
IPC: A61F7/08
CPC classification number: A61F2007/0062
Abstract: PROBLEM TO BE SOLVED: To provide a steam heating instrument for giving relaxation to a user.
SOLUTION: The steam heating instrument includes a heating part, so as to supply steam which is generated from the heating part under a situation where the instrument is abutted on a body surface by holding a sheet between the heating part and the body surface. The sheet includes at least a ventilation part having the moisture permeability of 150-2,000g/(m
2 ×24hr). The heating part of the steam heating instrument has a steam generating function of maximizing the evaporation amount of the steam per unit time in 0.5-25 minutes from the start of heat generation. It is preferable that the heating part of the steam heating instrument has the steam generating function of allowing the cumulative evaporation amount of the steam in 30 minutes from the start of heat generation to be the range of 0.1-0.5g per 1g of the heat generating part. The sheet is 0.05-1.5mm in total thickness, including a function of controlling the amount of air supply to the heat generating part and a function of transmitting the heat of the steam heating part to the body surface.
COPYRIGHT: (C)2007,JPO&INPITAbstract translation: 要解决的问题:提供一种用于给用户放松的蒸汽加热仪器。 解决方案:蒸汽加热仪器包括加热部件,以便在仪器通过在加热部件和主体表面之间保持片材而将仪器抵靠在体表表面的情况下供应由加热部件产生的蒸汽 。 该片材至少具有透湿度为150-2,000g /(m 2 / SP>×24hr)的通风部件。 蒸汽加热装置的加热部件具有蒸发发生功能,其在从发热开始的0.5-25分钟内使单位时间内蒸汽的蒸发量达到最大。 蒸汽加热装置的加热部分优选具有允许从发热开始起30分钟内的蒸汽的累积蒸发量为每1g生热量为0.1-0.5g的蒸汽发生功能 部分。 片材的总厚度为0.05-1.5mm,包括控制向发热部件供应的空气量的功能和将蒸汽加热部件的热传递到体表的功能。 版权所有(C)2007,JPO&INPIT
-
公开(公告)号:JP2005152146A
公开(公告)日:2005-06-16
申请号:JP2003392871
申请日:2003-11-21
Inventor: WATANABE TOSHIO , MORIWAKA HIROBUMI , ENOMOTO HARUOMI , YAMASHITA KAZUTAKA
Abstract: PROBLEM TO BE SOLVED: To provide a mixture attachment of a simple constitution capable of preventing such malfunctions as to open a raw water inflow path with a chemical injection port open when the chemical injection port is opened and closed. SOLUTION: By sliding and moving a cover body 28 mounted to the outer circumference of an outside tube body 20 in axial directions X, the chemical injection port 27 formed in the circumferential surface of the outside tube body 20 is opened and closed. By rotating and moving the outside tube body 20 integrally with the cover body 28 in circumferential directions with respect to an inside tube body 19, the raw water inlet port 16 formed in an upstream-side blocking part 22 and an outflow path 17 formed in a downstream-side blocking part 23 are opened and closed. The mixture attachment is provide with a lock mechanism for preventing the rotation and movement of the outside tube body 20 with respect to the inside tube body 19 when the cover body 28 is slid and moved in an axial direction X to bring the chemical injection port 27 into an open state and preventing the slide and movement of the cover body 28 in the axial directions when the outside tube body 20 is rotated and moved to bring the raw water inflow path 16 and the outflow path 17 into an open state. COPYRIGHT: (C)2005,JPO&NCIPI
Abstract translation: 要解决的问题:提供一种简单的构造的混合物附着,其能够在化学品喷射口打开和关闭时能够防止化学喷射口打开时打开原水流入路径的故障。 解决方案:通过将安装在外管体20的外周的盖体28沿轴向X滑动移动,形成在外筒体20的周面的化学喷射口27打开和关闭。 通过使外管体20与盖体28相对于内管体19在圆周方向一体地旋转移动,形成在上游侧阻塞部22和流出路17中的原水入口16形成为 下游侧阻挡部23打开和关闭。 当盖主体28沿轴向方向X滑动并移动时,混合物附件设置有用于防止外管体20相对于内管体19旋转和移动的锁定机构,以使化学品喷射口27 处于打开状态,并且当外管主体20旋转移动以防止原水流入路径16和流出路径17处于打开状态时,防止盖体28沿轴向的滑动和移动。 版权所有(C)2005,JPO&NCIPI
-
公开(公告)号:JP2003277234A
公开(公告)日:2003-10-02
申请号:JP2002075981
申请日:2002-03-19
Inventor: ATSUGI TAKESHI , YAMASHITA KAZUTAKA , NAKAYAMA HIDEHIKO , KASHIMOTO AKIO , TSUGO KAZUICHI , KOBAYASHI SHINICHI
Abstract: PROBLEM TO BE SOLVED: To provide a process for producing a solid powder cosmetic which may easily and uniformly yield a solid powder cosmetic which is formed from a mixture of a powder, an oil and a polymer dispersion and shows an excellent impact resistance and impression at use.
SOLUTION: In the process for producing the solid powder cosmetic, a mixture prepared by mixing the powder and the oil is left still for ≥5 hours, the mixture is mixed with the polymer dispersion to form a granulated substance, and the granulated substance is subjected to pressure molding within 100 hours to obtain the solid powder cosmetic. The polymer dispersion is preferably a mixture obtained by mixing and dispersing a coating film-forming polymer in an aqueous volatile solvent. The powder is preferably hydrophobic or hydrophobed, and the polymer composing the polymer dispersion is preferably a coating film-forming polymer having an elastic modulus of 0.3-200 kg/cm
2 .
COPYRIGHT: (C)2004,JPOAbstract translation: 要解决的问题:提供一种固体粉末化妆品的制造方法,其可以容易且均匀地得到由粉末,油和聚合物分散体的混合物形成的固体粉末化妆品,并显示出优异的耐冲击性 和使用印象。 解决方案:在制备固体粉末化妆品的方法中,将通过混合粉末和油制备的混合物静置≥5小时,将混合物与聚合物分散体混合以形成颗粒状物质,并将颗粒状 在100小时内对物质进行加压成型,得到固体粉末化妆品。 聚合物分散体优选是通过将涂膜形成聚合物混合并分散在水性挥发性溶剂中而获得的混合物。 粉末优选为疏水性或疏水性的,构成聚合物分散体的聚合物优选为弹性模量为0.3-200kg / cm 2的涂膜形成聚合物。 版权所有(C)2004,JPO
-
公开(公告)号:JPH11238230A
公开(公告)日:1999-08-31
申请号:JP4069598
申请日:1998-02-23
Applicant: KAO CORP
Inventor: YAMASHITA KAZUTAKA , NAKAYAMA HIDEHIKO , TAKESHIGE YUICHI , KOBAYASHI HIDEYUKI
IPC: B32B27/30 , C09D5/23 , C09D127/06 , C09D175/04 , G11B5/70 , G11B5/73 , G11B5/738 , G11B5/842 , G11B5/704
Abstract: PROBLEM TO BE SOLVED: To provide a producing method of a magnetic record medium which has improved dispersibility of a powder having a small particle size compounded in a lower layer, which has excellent travelling durability and electromagnetic conversion characteristics and which is suitable for high recording density. SOLUTION: As for the binders in the coating material for a lower layer 3 and in the coating material for an upper magnetic layer 4, a vinyl chloride resin containing epoxy groups, sulfonate groups or sulfate groups and a polyurethane resin containing sulfonate groups are used for both. As for the inorg. powder incorporated into the coating material for the lower layer 3, an inorg. powder having >=25 m /g BET specific surface area is included by >=40 wt.% of the total amt. of the inorg. powder. Water is incorporated by 0.05 to 0.8 wt.% into the coating material for the lower layer.
-
公开(公告)号:JPH11175949A
公开(公告)日:1999-07-02
申请号:JP34176697
申请日:1997-12-11
Applicant: KAO CORP
Inventor: YAMASHITA KAZUTAKA , NAKAYAMA HIDEHIKO , ISHIKAWA AKIRA
Abstract: PROBLEM TO BE SOLVED: To provide a magnetic recording medium of high density and high capacity which has good electromagnetic conversion characteristics and which hardly causes deterioration in the characteristics even when it is travelled at a high speed for a long time. SOLUTION: This magnetic recording medium has the following features. An acicular ferromagnetic powder having
-
公开(公告)号:JPH11154322A
公开(公告)日:1999-06-08
申请号:JP4506698
申请日:1998-02-26
Applicant: KAO CORP
Inventor: KUBO HIROKI , KOBAYASHI HIDEYUKI , YAMASHITA KAZUTAKA
Abstract: PROBLEM TO BE SOLVED: To provide a high-density magnetic recording medium with which low surface electric resistance, electromagnetic conversion characteristics and preservation stability are simultaneously attained without increasing carbon black. SOLUTION: This magnetic recording medium is constituted by coating the surface of a nonmagnetic base with an intermediate layer contg. at least magnetic powder having Moh's hardness of >=3 and an average grain size of =3, carbon black and binder and coating the surface thereof with a magnetic layer as the uppermost layer contg. at least ferromagnetic metallic powder and binder. In such a case, the center line average height (Ra) of the magnetic layer after the magnetic recording medium is subjected to an immersion treatment in an aq. soln. is 10 to 30 nm.
-
公开(公告)号:JPH11120556A
公开(公告)日:1999-04-30
申请号:JP28551697
申请日:1997-10-17
Applicant: KAO CORP
Inventor: NAKAYAMA HIDEHIKO , YAMASHITA KAZUTAKA , ISHIKAWA AKIRA
Abstract: PROBLEM TO BE SOLVED: To provide a magnetic recording medium formed an intermediate layer consisting of a coating material having excellent thixotropic property and which enables high recording density and which has excellent light- transmitting property, antistatic property, productivity and travelling stability. SOLUTION: This magnetic recording medium consists of a support 2, a magnetic layer 3 as the uppermost layer, and an intermediate layer 4 adjacent to the magnetic layer 3. The intermediate layer 4 is formed by applying a coating material for formation of the intermediate layer containing a binder, solvent, hardening agent and org. tin compd. within 20 min after the hardening agent is added.
-
-
-
-
-
-
-
-
-