BIAXIALLY STRETCHED POLYESTER FILM FOR CONTAINER MOLDING AND METHOD OF MANUFACTURING THE SAME
    152.
    发明公开
    BIAXIALLY STRETCHED POLYESTER FILM FOR CONTAINER MOLDING AND METHOD OF MANUFACTURING THE SAME 失效
    BIAXIAL GESTRECHTE POLYESTERFOLIE ZUM FORMEN VONBEHÄLTERNZOWIE HERSTELLUNSVERFAHREN

    公开(公告)号:EP0839854A4

    公开(公告)日:2000-08-16

    申请号:EP97922055

    申请日:1997-05-15

    Abstract: A biaxially stretched polyester film for forming a container, characterized by being formed of a polyester substantially consisting of an ethylene terephthalate unit and an ethylene naphthalate unit, the refractive index in the direction of thickness of the film being 1.5 or greater. This film is not only excellent in the formability during formation into cans or the like, but has excellent properties in taste property, particularly, the taste property after the retorting, and may be suitably used for containers produced by forming process and, particularly, for metallic cans.

    Abstract translation: 一种用于形成容器的双轴拉伸聚酯膜,其特征在于由基本上由对苯二甲酸乙二醇酯单元和萘二甲酸乙二醇酯单元组成的聚酯形成,膜的厚度方向的折射率为1.5以上。 这种膜不仅在成形罐等中的成形性方面是优异的,而且具有优异的味道特性,特别是蒸煮后的味道特性,并且可适用于通过成型方法生产的容器,特别是用于 金属罐

    POLYESTER FILM FOR MOLDING
    153.
    发明专利

    公开(公告)号:JP2002187964A

    公开(公告)日:2002-07-05

    申请号:JP2000388616

    申请日:2000-12-21

    Abstract: PROBLEM TO BE SOLVED: To prepare a polyester film for molding having excellent flexibility, moldability and stability of physical properties with time as well as excellent environmental properties. SOLUTION: This polyester film for molding comprises a polyester film containing a plasticizer, the crystalline melting energy (ΔHm) and the crystallization energy (ΔHc) by a DSC temperature rise measurement of the film satisfying the formula: ΔHm-ΔHc>=5(J/g).

    POLYESTER FILM FOR LAMINATION
    154.
    发明专利

    公开(公告)号:JP2002011788A

    公开(公告)日:2002-01-15

    申请号:JP2001109934

    申请日:2001-04-09

    Abstract: PROBLEM TO BE SOLVED: To provide a polyester film for lamination, which is excellent in not only environmental property but also in the protection as well as the workability of a pattern surface and a pigmented surface. SOLUTION: The stress upon 100% extension in the lengthwise direction (F100MD [Mpa]), the stress upon 100% extension in the widthwise direction (F100TD [MPa]) and the film thickness (d[μm]) at 25 deg.C of the polyester film for lamination satisfy the formulae of F100MD

    POLYESTER FILM FOR MOLDING AND MOLDED MEMBER USING THE SAME

    公开(公告)号:JP2001347565A

    公开(公告)日:2001-12-18

    申请号:JP2000174671

    申请日:2000-06-12

    Abstract: PROBLEM TO BE SOLVED: To provide a polyester film for molding and a molded member using the same which are excellent not only in environmental properties, but also in printing and processing properties and suitable for a switch, a printing base material and others. SOLUTION: In the polyester film for molding and the molded member using the same, an acid component constituting a polyester is a terephthalic acid unit by 95 mol% or more, and the total haze (Ht[%]) and the thickness (d [μm]) of the film and a 100% stretching stress (F100MD [Mpa]) in the longitudinal direction of the film and a 100% stretching stress (F100TD Mpa}) in the width direction thereof at 25 deg.C satisfy the following expressions I-III: 0.03

    POLYESTER FILM FOR LAMINATION AND DECORATIVE SHEET

    公开(公告)号:JP2001164001A

    公开(公告)日:2001-06-19

    申请号:JP34755699

    申请日:1999-12-07

    Abstract: PROBLEM TO BE SOLVED: To provide a polyester film for lamination and a decorative sheet, having good processability, generating no noxious gas in incineration, insusceptible to influence by hue of substrates, capable of appearing highly developed design and pattern and excellent in heat shrinkage characteristics, that is, excellent in environmental resistance, printability, highly designing properties and embossing processability. SOLUTION: This polyester film for lamination is a polyester film containing colorant and characterized by satisfying the following formula 1 to formula 4 [wherein T1( deg.C) is the highest temperature of changing inclination of expansion curve from plus to minus in warming; T2( deg.C) is a temperature of 25% elongation in warming]. T1-T2>=8 formula 1 10

    BIAXIALLY ORIENTED POLYESTER FILM FOR MOLDING FABRICATION AND FABRICATED LAMINATE

    公开(公告)号:JP2001072841A

    公开(公告)日:2001-03-21

    申请号:JP2000200633

    申请日:2000-07-03

    Abstract: PROBLEM TO BE SOLVED: To obtain a biaxially oriented polyester film having excellent molding fabrication property, shock resistance and beauty in appearance, and suitable as a material for molding fabrication by using a polyester having a melting point in a specific range as the main constituting component, and specifying the breaking elongations in the longitudinal direction and the lateral direction so that they satisfy a specific relation. SOLUTION: The objective film is obtained by using a polyester having a melting point of 210-280 deg.C as the main constituting component, and specifying the breaking elongation (%) in the longitudinal direction and that (%) in the lateral direction so that the following relation is satisfied (S1+S2)/2>=300%, here S1 and S2 are the values of the breaking elongation in the longitudinal direction and that in the lateral direction, respectively, when their sum becomes maximum determined at 20 deg.C to (melting point-60) deg.C. The film is fabricated by itself or in a laminar constitution with a nonmetal material (e.g. nonwoven fabric). The polyester is preferably obtained by polycondensing a dicarboxylic acid component (e.g. terephthalic acid) and a glycol component (e.g. ethylene glycol), and its intrinsic viscosity is preferably 0.5-1.5 g/dl.

    LAMINATE
    159.
    发明专利
    LAMINATE 失效

    公开(公告)号:JP2001058372A

    公开(公告)日:2001-03-06

    申请号:JP2000179708

    申请日:2000-06-15

    Abstract: PROBLEM TO BE SOLVED: To facilitate separation/recovery while enabling recycling by forming a laminate from a layer partially or wholly dissolvable at a time of the treatment and a polymer layer separable and recoverable from the dissolvable layer. SOLUTION: A laminate is formed from a layer partially or wholly dissolvable by the treatment with an acid or alkali aq.soln. and a separable and recoverable polymer layer different in solubility from the dissolvable layer. As the aq.soln., an acidic aq.soln. and an alkaline aq.soln. can be designated and the temp. thereof is pref. 0-200 deg.C in usual. As a material constituting the partially or wholly dissolvable layer, a resin based on polylactic acid is especially pref. and the content of polylactic acid is set to 5-100 wt. %. The mol.wt. holding ratio of the polymer layer after immersed in a 1N sodium hydroxide aq.soln. at 25 deg.C is pref. 50% or more and, for example, a thermoplastic resin such as a polyester resin, a polyolefin resin, a polyvinyl chloride resin or a polystyrene resin is used for the polymer layer.

    BIAXIALLY DRAWN FILM FOR BARRIER AND BARRIER FILM

    公开(公告)号:JP2001038867A

    公开(公告)日:2001-02-13

    申请号:JP21860399

    申请日:1999-08-02

    Abstract: PROBLEM TO BE SOLVED: To obtain a barrier film excellent in recycling properties. SOLUTION: A biaxially drawn film for barrier wherein a biaxially drawn film prepd. by laminating a layer B on at least one face of a polyester layer (a layer A) contg. at least 80 mole % ethylene terephthalate and/or ethylene naphthalate units is used and at least 70% resin constituting the layer B is dissolved in a water soln. with a pH of 8-14 and a barrier material is laminated on the layer B face and a barrier film prepd. by depositing a metal or a metal oxide on the layer B face of the biaxially drawn film comprising the polyester layer (the layer A) contg. at least 80 mole % ethylene terephthalate and/or ethylene naphthalate units and the layer (the layer B) comprising the resin at least 70% of which is dissolved with the water soln. with a pH 8-14, are provided.