Abstract:
A headset device (400) comprising: an earbud housing (610) including an earbud through-hole (612) and a first neck engaging surface (614); a primary housing (630) including a housing through-hole (632) and a second neck engaging surface (634); a threaded neck (620) including first and second neck surfaces, wherein the first neck surface is mated to the first neck engaging surface (614) and the second neck surface is mated to the second neck engaging surface (634); an earbud screw (690) that fits through the earbud through-hole (612) and is interlocked with the threaded neck (620) to fix the earbud housing (610) to the threaded neck (620); and a primary housing screw that fits through the housing through-hole (632) and is interlocked with the threaded neck (620) to fix the primary housing (630) to the threaded neck (620).
Abstract:
Apparatus, systems and methods for improving strength of a thin glass member for an electronic device are disclosed. In one embodiment, the glass member can have improved strength characteristics in accordance with a predetermined stress profile. The predetermined stress profile can be formed through multiple stages of chemical strengthening. The stages can, for example, have a first ion exchange stage where larger ions are exchanged into the glass member, and a second ion exchange stage where some of the larger ions are exchanged out from the glass member. In one embodiment, the glass member can pertain to a glass cover for a housing for an electronic device. The glass cover can be provided over or integrated with a display.
Abstract:
Anodized electroplated aluminum structures and methods for making the same are disclosed. Cosmetic structures according to embodiments of the invention are provided by electroplating a non-cosmetic structure with aluminum and then anodizing the electroplated aluminum. This produces cosmetic structures that may possess desired structural and cosmetic properties and that may be suitable for use a housing or support members of electronic devices.
Abstract:
Apparatus, systems and methods for improving chemical strengthening behavior in glass members are disclosed. According to one aspect, a method for processing a glass part formed using a fusion process or a float process includes annealing the glass part and then chemically strengthening the glass part. Annealing the glass part includes at least heating the glass part at a first temperature, maintaining the first temperature, and cooling the glass part to a second temperature using a controlled cooling process. Chemically strengthening the glass part includes facilitating an ion exchange between ions included in the glass part and ions included in a chemical strengthening bath.
Abstract:
Apparatus, systems and methods for characteristics of glass components through use of one or more coatings are disclosed. The coatings are typically thin coatings, such as thin film coatings. The coatings can serve to increase strength of the glass components and/or provide durable user interfacing surfaces. Accordingly, glass articles that have received coatings are able to be not only thin but also sufficiently strong so as to resist damage from impact events. The coated glass articles are well suited for use in consumer products, such as consumer electronic devices.
Abstract:
Apparatus, systems and methods for improving strength of a thin glass cover for an electronic device are disclosed. In one embodiment, the glass member can have improved strength by forming its edges with a predetermined geometry and/or by chemically strengthening the edges. Advantageously, the glass member can be not only thin but also adequately strong to limit susceptibility to damage. In one embodiment, the glass member can pertain to a glass cover for a housing for an electronic device. The glass cover can be provided over or integrated with a display, such as a Liquid Crystal Display (LCD) display.