Prepn. of vinyl] polymers of low mol. wt.

    公开(公告)号:DE4203277A1

    公开(公告)日:1993-08-12

    申请号:DE4203277

    申请日:1992-02-06

    Applicant: BASF AG

    Abstract: The continuous polymerisation of vinyl monomers by formation of vinyl polymers (I) with a mol. wt. of 1000-20,000 is claimed. The polymerisation is carried out at 110-270 deg. C in a ring slit (slit width 0.5-1.00 mm) that is bounded on the inner side by a rotor. Also claimed is the use of (I) as binding agents for paints, protective coatings, paper coating materials and printing inks. The reaction temp. is 150-270 deg. C and the polymer dispersivity (Mw/Mn) of (I) is less than 3.5. A portion of the volumetric flow is recirculated through the ring slit such that the recycle ratio of recirculated volumetric flow to throughput is 2-35. The rotor promotes reacton by thorough mixing and has a tangential avelocity of 0.5-2 m/s. The reaction is carried out in 0-40% of a solvent (w.r.t. monomer). The mixt. of monomers comprises 60-100 wt.% (meth)acrylic acid esters. Polymerisation initiator is added in a molar ratio of 0.0005:1 to 0.1:1 (w.r.t. monomer).

    12.
    发明专利
    未知

    公开(公告)号:DE19631365A1

    公开(公告)日:1998-02-05

    申请号:DE19631365

    申请日:1996-08-02

    Applicant: BASF AG

    Abstract: A process for the production of an essentially syndiotactic and partially crystalline polymer (I) containing vinyl aromatic monomers is claimed. (I) is prepared form a reaction mixture containing vinyl aromatic compounds (II), metallocene complexes (III) and one or co-catalysts (IV) consisting of strong, neutral Lewis acid or Bronsted acid cations. The components are mixed prior to addition to the reactor. An apparatus is also claimed comprising a reservoir to contain a mixture of (II) and (IV), a reservoir to contain (III) plus means to dose the contents of the 2 reservoirs to a pre-mixer that is connected to the reactor vessel.

Patent Agency Ranking