公开(公告)号:DE4407628A1
公开(公告)日:1995-09-14
申请号:DE4407628
申请日:1994-03-08
Applicant: BASF AG
Inventor: TATZEL HERMANN , DOMAS FRIEDRICH , LAMBERT JUERGEN
IPC: B29C51/20 , B29C44/00 , B29C44/08 , B29C67/20 , B29K105/04
-
公开(公告)号:AU645388B2
公开(公告)日:1994-01-13
申请号:AU1038792
申请日:1992-01-22
Applicant: BASF AG
Inventor: HAARDT UDO , SEILER ERHARD , TATZEL HERMANN , SCHWAGER HARALD , DOMAS FRIEDRICH
Abstract: Shock-absorbing propylene polymer composite moulded articles containing …… a. a layer of thickness 0.5 to 10 mm, containing a propylene polymer of melting point 130 to 165 DEG C, … b. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … c. a foam layer of thickness 3 to 200 mm having a density of 0.015 to 0.1 g/cm based on a propylene copolymer of melting point 125 to 155 DEG C, … d. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … e. a layer of thickness 0.5 to 10 mm containing a propylene polymer of melting point 130 to 165 DEG C. …
-
公开(公告)号:DE4101806A1
公开(公告)日:1992-07-30
申请号:DE4101806
申请日:1991-01-23
Applicant: BASF AG
Inventor: HAARDT UDO , SEILER ERHARD , TATZEL HERMANN , SCHWAGER HARALD , DOMAS FRIEDRICH
Abstract: Shock-absorbing propylene polymer composite moulded articles containing …… a. a layer of thickness 0.5 to 10 mm, containing a propylene polymer of melting point 130 to 165 DEG C, … b. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … c. a foam layer of thickness 3 to 200 mm having a density of 0.015 to 0.1 g/cm based on a propylene copolymer of melting point 125 to 155 DEG C, … d. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … e. a layer of thickness 0.5 to 10 mm containing a propylene polymer of melting point 130 to 165 DEG C. …
-
公开(公告)号:NO920295A
公开(公告)日:1992-07-24
申请号:NO920295
申请日:1992-01-22
Applicant: BASF AG
Inventor: HAARDT UDO , SEILER ERHARD , TATZEL HERMANN , SCHWAGER HARALD , DOMAS FRIEDRICH
CPC classification number: B32B5/18 , B32B5/20 , B32B7/12 , B32B27/065 , B32B27/32 , B32B2266/025 , B32B2307/56 , B32B2323/10 , Y10T428/24967 , Y10T428/249981 , Y10T428/249986 , Y10T428/249988 , Y10T428/249992 , Y10T428/249993
-
公开(公告)号:DE3721742A1
公开(公告)日:1989-01-12
申请号:DE3721742
申请日:1987-07-01
Applicant: BASF AG
Inventor: SCHNEIDER NORBERT , NOWAK UWE DR , NICKOLAY GERD , KLEIN URSULA , LENZ WERNER DR , JAKUSCH HELMUT DR , KOCH VOLKER DR , DOMAS FRIEDRICH
-
公开(公告)号:CA1028049A
公开(公告)日:1978-03-14
申请号:CA186409
申请日:1973-11-21
Applicant: BASF AG
Inventor: SCHOETTLE KLAUS , WITTKAMP HEINRICH , DOMAS FRIEDRICH
IPC: G11B23/033 , G11B17/022 , G11B17/03 , G11B17/32 , G11B17/34 , G11B23/50 , G11B5/016
-
公开(公告)号:DE59503556D1
公开(公告)日:1998-10-22
申请号:DE59503556
申请日:1995-01-10
Applicant: BASF AG
Inventor: TATZEL HERMANN , HAARDT UDO , DOMAS FRIEDRICH
-
公开(公告)号:ES2116636T3
公开(公告)日:1998-07-16
申请号:ES95103040
申请日:1995-03-03
Applicant: BASF AG
Inventor: TATZEL HERMANN , DOMAS FRIEDRICH , LAMBERT JURGEN
IPC: B29C51/20 , B29C44/00 , B29C44/08 , B29C67/20 , B29K105/04
-
公开(公告)号:DE59502295D1
公开(公告)日:1998-07-02
申请号:DE59502295
申请日:1995-03-03
Applicant: BASF AG
Inventor: TATZEL HERMANN , DOMAS FRIEDRICH , LAMBERT JUERGEN
IPC: B29C51/20 , B29C44/00 , B29C44/08 , B29C67/20 , B29K105/04
-
公开(公告)号:ES2113871T3
公开(公告)日:1998-05-16
申请号:ES91122249
申请日:1991-12-27
Applicant: BASF AG
Inventor: HAARDT UDO , SEILER ERHARD , TATZEL HERMANN , SCHWAGER HARALD , DOMAS FRIEDRICH
Abstract: Shock-absorbing propylene polymer composite moulded articles containing …… a. a layer of thickness 0.5 to 10 mm, containing a propylene polymer of melting point 130 to 165 DEG C, … b. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … c. a foam layer of thickness 3 to 200 mm having a density of 0.015 to 0.1 g/cm based on a propylene copolymer of melting point 125 to 155 DEG C, … d. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … e. a layer of thickness 0.5 to 10 mm containing a propylene polymer of melting point 130 to 165 DEG C. …
-
-
-
-
-
-
-
-
-