11.
公开(公告)号:CA1069234A
公开(公告)日:1980-01-01
申请号:CA252418
申请日:1976-05-13
Applicant: BASF AG
Inventor: MITTNACHT HANS , ECHTE ADOLF , JENNE HELMUT , LIEB MANFRED , BRONSTERT KLAUS , ADLER HANSJOERG
IPC: C08L7/00 , C08L21/00 , C08L23/00 , C08L25/00 , C08L25/10 , C08L51/00 , C08L51/02 , C08L51/04 , C08L77/00 , C08L101/00
Abstract: Thermoplastic molding compositions, based on polymers of a monovinyl-aromatic compound which have been modified with rubber to increase their impact strength, which also exhibit increased stress crack resistance. The increased stress crack resistance is achieved if the proportion of the soft component in the polymer which has been modified to increase its impact strength, and the particle size and swelling index of the soft component phase, conform to particular values, and the tensile strength and yield stress of the thermoplastic molding compositions bear a particular ratio to one another. The molding compositions may in particular be used for the manufacture of internal liners of refrigerators and foodstuff packaging containers.
-
公开(公告)号:AU1390576A
公开(公告)日:1977-11-17
申请号:AU1390576
申请日:1976-05-13
Applicant: BASF AG
Inventor: MITTNACHT HANS , ECHTE ADOLF , JENNE HELMUT , LIEB MANFRED , BRONSTERT KLAUS , ADLER HANSJOERG
IPC: C08L7/00 , C08L21/00 , C08L23/00 , C08L25/00 , C08L25/10 , C08L51/00 , C08L51/02 , C08L51/04 , C08L77/00 , C08L101/00 , C08F279/02
Abstract: Thermoplastic molding compositions, based on polymers of a monovinyl-aromatic compound which have been modified with rubber to increase their impact strength, which also exhibit increased stress crack resistance.
-
公开(公告)号:CA1244567A
公开(公告)日:1988-11-08
申请号:CA470881
申请日:1984-12-21
Applicant: BASF AG
Inventor: HAMBRECHT JUERGEN , ILLERS KARL H , ECHTE ADOLF , SWOBODA JOHANN
Abstract: The invention relates to a thermoplastic molding material which contains a mixture of (I) from 95 to 5% by weight of a polyphenylene ether and (II) from 5 to 95% by weight of a copolymer consisting of A1) from 78 to 99 parts by weight of a monovinylaromatic compound, A2) from 1 to 12 parts by weight of (meth)acrylic acid and B) from 0 to 20 parts by weight of an elastomer component which has a glass transition temperature of ? 0.degree. C, the sum of the number of parts by weight being 100. This molding material processes appropriately high heat distortion resistance, good resistance to chemicals and well balanced mechanical properties.
-
公开(公告)号:CA1205594A
公开(公告)日:1986-06-03
申请号:CA407664
申请日:1982-07-20
Applicant: BASF AG
Inventor: HINSELMANN KLAUS , NAARMANN HERBERT , ECHTE ADOLF , HEIL EDUARD , NIKLES ALBERT , REFFERT RUDI W , HAMBRECHT JUERGEN
IPC: C08L7/00 , B29C35/00 , B29C45/00 , C08G65/46 , C08J3/00 , C08J3/20 , C08L21/00 , C08L23/00 , C08L33/00 , C08L33/02 , C08L71/00 , C08L71/12 , C08L101/00 , C08L71/04 , C08L25/04 , C08L51/04
Abstract: Molding materials containing high molecular weight polyphenylene ethers are produced by a process in which a solution of a polyphenylene ether in an organic solvent, together with another polymer, is freed of solvent by multi-stage evaporation. The solvent is preferably an aromatic compound from the class comprising the hydrocarbons, halohydrocarbons, ethers or esters, the ratio of the other polymer to the polyphenylene ether is advantageously from 99 : 1 to 20 : 80 parts by weight, the other polymer is, in particular, a homopolymer or copolymer of styrene or of a homolog thereof, which may be modified with rubber, and the multi-stage evaporation process preferably comprises not less than two and not more than four workingup stages. The evaporation is carried out in general at from 120 to 280.degree.C and under a pressure of from 1 to 3,000 mbar, advantageously in the presence of assistants which reduce the partial pressure, eg. water and/or methanol.
-
公开(公告)号:NO803491L
公开(公告)日:1981-05-21
申请号:NO803491
申请日:1980-11-19
Applicant: BASF AG
Inventor: ECHTE ADOLF , GAUSEPOHL HERMANN , JENNE HELMUT , MITTNACHT HANS
IPC: C08F212/06 , C08F255/06 , C08F279/02 , C08F
Abstract: Thermoplastic molding materials which contain a copolymer which has been made impact-resistant with a rubber. The copolymer is produced by polymerizing a mixture of a monovinyl-aromatic compound and an acrylic acid derivative or methacrylic acid derivative in the presence of a rubber. The folding materials contain a specific proportion of soft component. The diameter of the particles of the soft component, and the swelling index of the soft component, lie within a specific range, and the tensile strength of the molding material is higher than the yield strength.
-
公开(公告)号:NO803491A
公开(公告)日:1981-05-21
申请号:NO803491
申请日:1980-11-19
Applicant: BASF AG
Inventor: ECHTE ADOLF , GAUSEPOHL HERMANN , JENNE HELMUT , MITTNACHT HANS
IPC: C08F255/06 , C08F279/02 , C08F
CPC classification number: C08F255/06 , C08F279/02 , C08F212/06
-
公开(公告)号:GB1049665A
公开(公告)日:1966-11-30
申请号:GB3560263
申请日:1963-09-10
Applicant: BASF AG
Inventor: BRONSTERT KLAUS , WILD HANS , ECHTE ADOLF , BOECK EDMUND , KRAUSE HANS-JOACHIM
IPC: B29C51/00 , C08F279/02 , C08F287/00 , C08L21/00 , C08L51/00 , C08L51/04 , C08L55/02
Abstract: Impact-resistant polystyrene having improved surface properties is made by first polymerizing styrene in which is dissolved a substantially uncrosslinked rubber, and then mechanically mixing the product with a crosslinked or crosslinkable rubber. Up to 35% of the styrene in the first stage of the process may be replaced by a comonomer, e.g. acrylonitrile, alkylstyrenes and halostyrenes. The examples describe polymerizing styrene with: (1) a butadiene-styrene copolymer, and mixing the product with a butadiene-styrene copolymer, (2) a butadiene-styrene copolymer, and mixing the product with a butadiene-butyl fumarate copolymer, (3) cis-1,4-polybutadiene, and mixing the product with a butadiene-butyl fumarate copolymer, (4-5) acrylonitrile, a butylacrylate-acrylonitrile copolymer and cis-1,4-polybutadiene, and mixing the product with a butadiene-acrylonitrile copolymer.
-
公开(公告)号:CA1263992A
公开(公告)日:1989-12-19
申请号:CA495489
申请日:1985-11-15
Applicant: BASF AG
Inventor: BRANDT HERMANN , FISCHER HERMANN , DREHER HERMANN , HEIL EDUARD , HAMBRECHT JUERGEN , NAARMANN HERBERT , ECHTE ADOLF , GAUSEPOHL HERMANN , SIEBEL PETER , SWOBODA JOHANN , SCHWOEBEL GERD , NIKLES ALBERT
Abstract: Disclosed is a process of preparation of polyphenylene ethers from monohydric phenols, which possess alkyl substituents in the two ortho-positions and, if desired, in the meta-position, but not in the para-position, by an oxidative coupling reaction with oxygen at from 15 to 50.degree.C and under from 1 to 10 bar in the presence of a catalyst complex, of a solvent and, if required, of an activator. In this process,the conversion of the phenols is carried out in two or more reaction zones. Some or all of the solvent, catalyst complex phenols and where relevant, activator are initially added to one of the reaction zones and are circulated in the other reaction zone and about 60-100% of the stoichiometric amount of oxygen required for the oxidative coupling is introduced into the first reaction zone and from 0 to about 40% of the said stoichiometric amount is introduced into the second reaction zone. This process is interesting in that it makes it possible to carry out oxidative coupling of phenols with oxygen in a very economic and reliable manner, with very high space-time yields, formation of only a small amount of by-products, and minimum emissions of gas and volatile components.
-
公开(公告)号:CA1239746A
公开(公告)日:1988-07-26
申请号:CA478833
申请日:1985-04-11
Applicant: BASF AG
Inventor: MUENCH VOLKER , HAMBRECHT JUERGEN , HIMMELE WALTER , ECHTE ADOLF , SWOBODA JOHANN
Abstract: High molecular weight polyphenylene ethers are prepared from monohydric phenols by an oxidative coupling reaction with oxygen in the presence of a solvent and of a catalyst complex consisting of a copper salt and an organic amine of the general formula where R1 is C2-C20-alkylidene, preferably C2-C12-alkylid-ene, or alkenylidene, R2 is H or C1-C12-alkyl, preferably C1-C4-alkyl, or C5-C8-cycloalkyl, each of which is unsubstituted or substituted by functional groups, and n is an integer from 1 to 4, preferably 1 or 2. Preferred functional groups are -OR3, -NHR3 or -SR3, in which R3 is H C1-C12-alkyl or C5-C8-cycloalkyl, and the most suitable amines are 3-tert.-butoxypropylamine, 4-tert.-butoxy-butylamine, 3-tert.-butoxy-2-methylpropylamine, 3-tert.-butoxy-2,3-dimethylpropylamine, 3-tert.-butoxy-2-methyl-octylamine and N-methyl-N-(4-tert.-butoxybutyl)-amine. The polyphenylene ethers can be processed to moldings by a thermoplastic method.
-
公开(公告)号:CA1185730A
公开(公告)日:1985-04-16
申请号:CA397337
申请日:1982-03-01
Applicant: BASF AG
Inventor: BRANDSTETTER FRANZ , ECHTE ADOLF , HAMBRECHT JUERGEN , ILLERS KARL H , PRIEBE EDMUND
Abstract: The invention relates to thermoplastic molding materials based on impact resistant polystyrene and polyphenylene ethers. The molding materials of this invention contain a flexible component having a glass temperature below -70.degree.C and a flexible component having a glass temperature in the range of 0 to -70.degree.C.
-
-
-
-
-
-
-
-
-