公开(公告)号:BR0211162A
公开(公告)日:2004-08-10
申请号:BR0211162
申请日:2002-07-05
Applicant: BASF AG
Inventor: FINK RALF , SCHUMACHER KARL-HEINZ , STERWALD UWE D , ERHARDT ULRICH , MEYER HARALD
IPC: C08K5/13 , C09J133/08 , C09J133/00
Abstract: A composition containing a melt-processing water-free, solvent-free polyacrylate and an anti-oxidizing agent which contains at least one aromatically bonded hydroxyl group and which is exclusively comprised of hydrogen, carbon and oxygen atoms.
-
公开(公告)号:DE10223615A1
公开(公告)日:2003-12-11
申请号:DE10223615
申请日:2002-05-27
Applicant: BASF AG
Inventor: WULFF DIRK , FELDTHUSEN JENSEN JESPER , AUCHTER GERHARD , WILDBURG GERALD , FINK RALF
IPC: C08F2/22 , C08F257/02 , C08F265/04 , C08F285/00 , C08F291/00 , C08L51/00 , C09J151/00 , C08F220/18 , C08F212/08 , C08F236/06 , C08F214/04 , C08F210/02 , C08F218/04 , C04B24/26 , C09D5/02 , C09D5/12 , C09J133/10
Abstract: The invention relates to a method for producing an aqueous polymer dispersion having a polymer solids content of >=50% by weight by carrying out the radically initiated aqueous emulsion polymerization of ethylenically unsaturated compounds (monomers). The inventive method is characterized in that: a) a mixture is provided in a polymerization vessel and contains a partial quantity 1 consisting of: deionized water, 0.001 to 0.5 parts by weight of a polymer with a weighted average particle diameter of =80% [polymerization step A], and; b) afterwards, a monomer emulsion containing partial quantity 2, which consists of deionized water, 0.1 to 5 parts by weight of dispersants and 90 to 99.5 parts by weight of monomers, is fed under polymerization conditions to the obtained reaction mixture [polymerization step B], whereby; c) the total amount of the monomers used for the polymerization is equal to 100 parts by weight, and the total amount of deionized water is
-
公开(公告)号:DE10110837A1
公开(公告)日:2002-09-12
申请号:DE10110837
申请日:2001-03-06
Applicant: BASF AG
Inventor: FINK RALF , CENTNER ALEXANDER
Abstract: A method for bonding formed parts comprises: (a) at least one of the joint surfaces consists of aluminum; (b) at least one of the joint surfaces is precoated with a polymer containing at least 40 wt.% 1-16C alkyl (meth)acrylate units (polyacrylate); and (c) an epoxy adhesive is used for bonding. An Independent claim is also included for formed parts bonded by this method.
-
公开(公告)号:DE19946898A1
公开(公告)日:2001-04-05
申请号:DE19946898
申请日:1999-09-30
Applicant: BASF AG
Inventor: MEYER-ROSCHER BERND , SCHUMACHER KARL-HEINZ , BARWICH JUERGEN , FINK RALF , DUESTERWALD UWE
IPC: C09J7/02 , C09J133/12 , C09J5/04
Abstract: The invention relates to the use of radically polymerised polymers that are crosslinkable by means of UV-light and consists of at least 50 wt. % C2 to C18 alkyl(meth)acrylates and are used as an adhesive for gluing together carriers on substrates, whereby said carriers are coated with the polymers. Said polymers are built-up by monomers. The invention is characterised in that 0.1 to 30 wt. % of said monomers are monomers A without carboxylic acid- or carboxylic acid anhydride groups and with a water solubility greater than 5 g monomers per litre of water. The substrates are humid, especially frozen substrates.
-
公开(公告)号:ES2289321T3
公开(公告)日:2008-02-01
申请号:ES03755108
申请日:2003-05-21
Applicant: BASF AG
Inventor: WULFF DIRK , FELDTHUSEN JENSEN JESPER , AUCHTER GERHARD , WILDBURG GERALD , FINK RALF
IPC: C08F285/00 , C08F2/22 , C08F257/02 , C08F265/04 , C08F291/00 , C08L51/00 , C09J151/00
Abstract: Procedimiento para la obtención de una dispersión acuosa de polímero con un contenido en producto sólido polímero >= 50 % en peso mediante polimerización en emulsión acuosa iniciada a través de radicales de compuestos con insaturación etilénica (monómeros), caracterizado porque a) se dispone en un recipiente de polimerización una mezcla que contiene Cantidad parcial 1 de agua desionizada 0, 001 a 0, 5 partes en peso de semilla de polímero con un diámetro de partícula promedio en peso
-
公开(公告)号:DE50307656D1
公开(公告)日:2007-08-23
申请号:DE50307656
申请日:2003-05-21
Applicant: BASF AG
Inventor: WULFF DIRK , FELDTHUSEN JENSEN JESPER , AUCHTER GERHARD , WILDBURG GERALD , FINK RALF
IPC: C08F285/00 , C08F2/22 , C08F257/02 , C08F265/04 , C08F291/00 , C08L51/00 , C09J151/00
Abstract: The invention relates to a method for producing an aqueous polymer dispersion having a polymer solids content of >=50% by weight by carrying out the radically initiated aqueous emulsion polymerization of ethylenically unsaturated compounds (monomers). The inventive method is characterized in that: a) a mixture is provided in a polymerization vessel and contains a partial quantity 1 consisting of: deionized water, 0.001 to 0.5 parts by weight of a polymer with a weighted average particle diameter of =80% [polymerization step A], and; b) afterwards, a monomer emulsion containing partial quantity 2, which consists of deionized water, 0.1 to 5 parts by weight of dispersants and 90 to 99.5 parts by weight of monomers, is fed under polymerization conditions to the obtained reaction mixture [polymerization step B], whereby; c) the total amount of the monomers used for the polymerization is equal to 100 parts by weight, and the total amount of deionized water is
-
公开(公告)号:DE50014146D1
公开(公告)日:2007-04-19
申请号:DE50014146
申请日:2000-09-15
Applicant: BASF AG
Inventor: MEYER-ROSCHER BERND , SCHUMACHER KARL-HEINZ , BARWICH JUERGEN , FINK RALF , DUESTERWALD UWE
IPC: C09J7/02
Abstract: The use of free-radically polymerized, UV-crosslinkable polymers which consist to the extent of at least 50% by weight of C2 to C18alkyl(meth)acrylates as adhesives for the bonding of carriers coated with the polymer on substrates, wherein from 0.1 to 30% by weight of the monomers of which said polymer is composed are monomers A without carboxylic acid or carboxylic anhydride groups and with a water solubility of more than 5 g of monomers per liter of water and said substrates are moist substrates, especially refrigerated substrates.
-
公开(公告)号:AT356177T
公开(公告)日:2007-03-15
申请号:AT00966021
申请日:2000-09-15
Applicant: BASF AG
Inventor: MEYER-ROSCHER BERND , SCHUMACHER KARL-HEINZ , BARWICH JUERGEN , FINK RALF , DUESTERWALD UWE
IPC: C09J7/02
Abstract: The use of free-radically polymerized, UV-crosslinkable polymers which consist to the extent of at least 50% by weight of C2 to C18alkyl(meth)acrylates as adhesives for the bonding of carriers coated with the polymer on substrates, wherein from 0.1 to 30% by weight of the monomers of which said polymer is composed are monomers A without carboxylic acid or carboxylic anhydride groups and with a water solubility of more than 5 g of monomers per liter of water and said substrates are moist substrates, especially refrigerated substrates.
-
公开(公告)号:AU2003247284A1
公开(公告)日:2003-12-12
申请号:AU2003247284
申请日:2003-05-21
Applicant: BASF AG
Inventor: WULFF DIRK , JENSEN JESPER FELDTHUSEN , AUCHTER GERHARD , WILDBURG GERALD , FINK RALF
IPC: C08F2/22 , C08F257/02 , C08F265/04 , C08F285/00 , C08F291/00 , C08L51/00 , C09J151/00
Abstract: The invention relates to a method for producing an aqueous polymer dispersion having a polymer solids content of >=50% by weight by carrying out the radically initiated aqueous emulsion polymerization of ethylenically unsaturated compounds (monomers). The inventive method is characterized in that: a) a mixture is provided in a polymerization vessel and contains a partial quantity 1 consisting of: deionized water, 0.001 to 0.5 parts by weight of a polymer with a weighted average particle diameter of =80% [polymerization step A], and; b) afterwards, a monomer emulsion containing partial quantity 2, which consists of deionized water, 0.1 to 5 parts by weight of dispersants and 90 to 99.5 parts by weight of monomers, is fed under polymerization conditions to the obtained reaction mixture [polymerization step B], whereby; c) the total amount of the monomers used for the polymerization is equal to 100 parts by weight, and the total amount of deionized water is
-
公开(公告)号:DE10158420A1
公开(公告)日:2003-06-12
申请号:DE10158420
申请日:2001-11-29
Applicant: BASF AG
Inventor: FINK RALF , CENTNER ALEXANDER
IPC: C09J7/00 , C08F220/12 , C08F220/32 , C09J5/02 , C09J133/06 , C09J163/00 , C09J4/02 , C09J7/02 , B32B7/12
Abstract: A process for adhesive bonding of shaped parts by (A) pre coating of at least one surface of the shaped part, prior to adhesive bonding, with a polymer comprising at least 5 wt.% glycidyl(meth)acrylate and (B) polymer containing up to 10-50 wt.% of glycidyl (meth)acrylate is new. Independent claims are included for: (1) A polymer obtained by radical polymerization of glass transition temperature -60 to +50 degrees C and comprising 5-50 wt.% glycidyl (meth)acrylate, of gel content 10-60 wt.%; (2) a removable support film coated with glycidyl (meth)acrylate; (3) a shaped part bonded with an adhesive obtained as above
-
-
-
-
-
-
-
-
-