公开(公告)号:MX9200249A
公开(公告)日:1992-10-01
申请号:MX9200249
申请日:1992-01-21
Applicant: BASF AG
Inventor: HAARDT UDO , SEILER ERHARD , TATZEL HERMANN , SCHWAGER HARALD , DOMAS FRIEDRICH
Abstract: Shock-absorbing propylene polymer composite moulded articles containing …… a. a layer of thickness 0.5 to 10 mm, containing a propylene polymer of melting point 130 to 165 DEG C, … b. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … c. a foam layer of thickness 3 to 200 mm having a density of 0.015 to 0.1 g/cm based on a propylene copolymer of melting point 125 to 155 DEG C, … d. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … e. a layer of thickness 0.5 to 10 mm containing a propylene polymer of melting point 130 to 165 DEG C. …
-
公开(公告)号:CA2059257A1
公开(公告)日:1992-07-24
申请号:CA2059257
申请日:1992-01-15
Applicant: BASF AG
Inventor: TATZEL HERMANN , DOMAS FRIEDRICH , SCHWAGER HARALD , SEILER ERHARD , HAARDT UDO
Abstract: O.Z. 0050/42154 A shock-absorbing propylene polymer composite molding contains a. a layer with a thickness of from 0.5 to 10 mm which contains a propylene polymer having a melting point of from 130 to 165.degree.C, b. an intermediate layer with a thickness of from 0.05 to 0.5 mm comprising a hot-melt adhesive based on an olefin copolymer having a melting point of from 90 to 140.degree.C, c. a foam layer with a thickness of from 3 to 200 mm and a density of from 0.015 to 0.1 g/cm3 based on a propylene copolymer having a melting point of from 125 to 155.degree.C, d. an intermediate layer with a thickness of from 0.05 to 0.5 mm comprising a hot-melt adhesive based on an olefin copolymer having a melting point of from 90 to 140.degree.C, e. a layer with a thickness of from 0.5 to 10 mm which contains a propylene polymer having a melting point of from 130 to 165.degree.C.
-
公开(公告)号:NL144966B
公开(公告)日:1975-02-17
申请号:NL6415189
申请日:1964-12-29
Applicant: BASF AG
Inventor: STASTNY FRITZ DR , HAARDT UDO , GAETH RUDOLF DR , SCHMITT BERNHARD DR
-
公开(公告)号:DE2262250A1
公开(公告)日:1974-07-04
申请号:DE2262250
申请日:1972-12-20
Applicant: BASF AG
Inventor: STASTNY FRITZ DR , GAETH RUDOLF DR , HAARDT UDO , KOERNER HEINZ-HERMANN
IPC: C08G18/00 , B29C39/00 , B29C39/24 , B29C39/26 , B29C67/20 , B29C70/66 , C08J9/22 , C08J9/35 , B29D27/00
Abstract: Composite soft and resilient foams are manufactured by injecting a foamable mixture of polyisocyanates, polyols, water or inert blowing agents and, if appropriate, auxiliaries, under pressure into a mold of which about 90 to 30% of the volume is filled with foamed, soft and resilient particles of olefin polymers of particle size from about 3 to 50 mm and bulk density from 5 to 100 g/l - these particles being in loose form or fused or stuck together - and allowing the reaction mixture to foam up.
-
公开(公告)号:FR1483398A
公开(公告)日:1967-06-02
申请号:FR65552
申请日:1966-06-15
Applicant: BASF AG
Inventor: STASTNY FRITZ , GAETH RUDOLF , SCHMITT BERNHARD , HAARDT UDO
-
公开(公告)号:CA753178A
公开(公告)日:1967-02-21
申请号:CA753178D
Applicant: BASF AG
Inventor: STASTNY FRITZ , HAARDT UDO , SCHMITT BERNHARD , GAETH RUDOLF
-
公开(公告)号:ES2212173T3
公开(公告)日:2004-07-16
申请号:ES98111950
申请日:1998-06-29
Applicant: BASF AG
Inventor: HAARDT UDO , TATZEL HERMANN
-
公开(公告)号:ES2098757T3
公开(公告)日:1997-05-01
申请号:ES93914709
申请日:1993-06-24
Applicant: BASF AG
Inventor: TATZEL HERMANN , HAARDT UDO
-
公开(公告)号:NO177341B
公开(公告)日:1995-05-22
申请号:NO920295
申请日:1992-01-22
Applicant: BASF AG
Inventor: HAARDT UDO , SEILER ERHARD , TATZEL HERMANN , SCHWAGER HARALD , DOMAS FRIEDRICH
Abstract: Shock-absorbing propylene polymer composite moulded articles containing …… a. a layer of thickness 0.5 to 10 mm, containing a propylene polymer of melting point 130 to 165 DEG C, … b. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … c. a foam layer of thickness 3 to 200 mm having a density of 0.015 to 0.1 g/cm based on a propylene copolymer of melting point 125 to 155 DEG C, … d. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … e. a layer of thickness 0.5 to 10 mm containing a propylene polymer of melting point 130 to 165 DEG C. …
-
公开(公告)号:DE59103836D1
公开(公告)日:1995-01-26
申请号:DE59103836
申请日:1991-03-02
Applicant: BASF AG
Inventor: LENZ WERNER , DOMAS FRIEDRICH , HAARDT UDO
Abstract: A construction element having a virtually rectangular force-movement characteristic, consisting of an elongated polymer foam body (1) of rectangular cross-section having the rectangular sides a and b, and having a recess (2), which extends over the complete longitudinal extent and on one side of the body, of width d and of height c, the said dimensions satisfying specific equations. … …
-
-
-
-
-
-
-
-
-