12.
    发明专利
    未知

    公开(公告)号:DE10206103A1

    公开(公告)日:2003-08-21

    申请号:DE10206103

    申请日:2002-02-13

    Applicant: BASF AG

    Abstract: An apparatus suitable for producing shaped bodies comprising thermoplastic polymers from monomers which form such polymers in a batch process comprises a) at least one reactor suitable for the batchwise preparation of a melt of a thermoplastic polymer from monomers which form such a polymer, b) a piping system suitable as circulation line for the melt of the thermoplastic polymer and c) at least one apparatus suitable for the production of shaped bodies from the melt of a thermoplastic polymer, wherein the reactor or reactors a) is/are connected to the piping system b) and the apparatus or apparatuses c) is/are connected to the piping system b), and an apparatus for producing shaped bodies comprising thermoplastic polymers in such an apparatus.

    13.
    发明专利
    未知

    公开(公告)号:DE3775164D1

    公开(公告)日:1992-01-23

    申请号:DE3775164

    申请日:1987-10-10

    Applicant: BASF AG

    Abstract: Ethylene is homopolymerised, or copolymerised with minor amts. of 3-8C alpha-monoolefins, at 30-200 deg.C and 0.1-200 bar, with a Ziegler catalyst comprising (1) a new transition metal catalyst component, (2) an organo-Al component and (3) an organo-halogen component. (1) The component is prepd. by (1.1) first (1.1.1) contracting (I) finely divided porous SiO2.Al2O3 with particle dia. 1-1000 microns, pore vol. 0.3-3 cc/g and surface 100-1000 square m/g and (1.1.2) a soln. (II) obtd. by mixing (IIa) 100 pts. of 4-18C satd. aliphatic or satd. aliphatic/ aromatic oxahydrocarbon with 1-2 oxa O atoms, and (IIb) 0.01-50 pts. of a mixt. of (IIb1) 100 mols. of VY3.nZ-OH, (IIb2) 0.2-300 mols. of TiCl3 and/or tiBr3 or a complex of formula TiY3.nZ-OH and opt. (IIb3) 1-400 mols. of ZrCl4 and/or ZrBr4, to form a suspension (III), and evaporating the suspension at below 200 deg.C and above the m.pt. of (IIa), to give a solid intermediate (IV), (1.2) contacting (IV) with a soln. in an organic solvent of AlRmX3-m (V), to form a suspension of a solid prod. (VI) and (1.3) contacting the solid (VI), opt. suspended in an inert hydrocarbon with O2 at -25 to 100 deg. C for 5-500 mins., and recovering component (1). a = 0-2; Y = Cl or Br; n = 1-6; Z = monovalent, not more than 10C, satd. aliphatic or satd. aliphatic/aromatic hydrocarbon gp.; X = OR, Cl, Br or H; R = 1-18C hydrocarbon gp.; m = 1-3. (2) The component is AlRmX'3-m.. X' = OR, Cl or H. Ratios by wt. are (I):(IIb) = 1:0.01-2; (IV):(V) = 1:0.05-2. Atomic ratios are transition metal in (1):Al in (2) = 1:0.1-500; transition metal in (VI):O2 = 1:0.01-10. Molar ratio of (2):(3) = 1:0.001-50.

    14.
    发明专利
    未知

    公开(公告)号:NO159492B

    公开(公告)日:1988-09-26

    申请号:NO813566

    申请日:1981-10-22

    Applicant: BASF AG

    Abstract: 1. A finely divided polymer dispersion which contains polymerized units of nitrogen-containing monomers, and is obtained by a two-stage polymerization reaction, wherein, in the first polymerization stage, a low molecular weight prepolymer, which has a viscosity of from 1.06 to 1.40 (measured in an Ubbelohde viscometer) in a 1% strength solution of a mixture of 99 parts by weight of dimethyl formamide and 1 part by weight of glacial acetic acid at 20 degrees C, is prepared in a water-miscible solvent, which may contain up to 15% by weight of water, in the manner of a solution copolymerization from a monomer mixture which contains (a) per mole of a nitrogen-containing monomer of the formula see diagramm : EP0051144,P13,F1 or see diagramm : EP0051144,P13,F3 where A is O or NH, B is Cn H2n , n being from 1 to 8, R**1 and R**2 are each Cm H2m+1 , m being from 1 to 4, R**3 is H or CH3 , X4 **- is OH**- , Cl**- , Br**- or CH3 -OSO3 H**- , and R**4 is Cm H2m+1 , m being from 1 to 4, (b) 2.5 to 10 moles of at least one nonionic, hydrophobic, ethylenically unsaturated monomer which, if it is polymerized on its own, forms a hydrophobic polymer, (c) 0.5 to 1.5 moles of an ethylenically unsaturated carboxylic acid or maleic anhydride, and (d) 0 to 7 moles of a nonionic, hydrophilic, ethylenically unsaturated monomer, the solution of the prepolymer is diluted with water in a weight ratio of from 1:3 to 1:50 and, in the second polymerization stage, 1 to 32 parts by weight of at least one nonionic, hydrophobic, ethylenically unsaturated monomer, which is the same as monomer (b) of the prepolymer, are polymerized per part by weight of the solution polymer in this polymer solution in the manner of an emulsion polymerization in the presence of a usual amount of a water-soluble polymerization initiator.

    15.
    发明专利
    未知

    公开(公告)号:FI812751L

    公开(公告)日:1982-04-24

    申请号:FI812751

    申请日:1981-09-04

    Applicant: BASF AG

    Abstract: 1. A finely divided polymer dispersion which contains polymerized units of nitrogen-containing monomers, and is obtained by a two-stage polymerization reaction, wherein, in the first polymerization stage, a low molecular weight prepolymer, which has a viscosity of from 1.06 to 1.40 (measured in an Ubbelohde viscometer) in a 1% strength solution of a mixture of 99 parts by weight of dimethyl formamide and 1 part by weight of glacial acetic acid at 20 degrees C, is prepared in a water-miscible solvent, which may contain up to 15% by weight of water, in the manner of a solution copolymerization from a monomer mixture which contains (a) per mole of a nitrogen-containing monomer of the formula see diagramm : EP0051144,P13,F1 or see diagramm : EP0051144,P13,F3 where A is O or NH, B is Cn H2n , n being from 1 to 8, R**1 and R**2 are each Cm H2m+1 , m being from 1 to 4, R**3 is H or CH3 , X4 **- is OH**- , Cl**- , Br**- or CH3 -OSO3 H**- , and R**4 is Cm H2m+1 , m being from 1 to 4, (b) 2.5 to 10 moles of at least one nonionic, hydrophobic, ethylenically unsaturated monomer which, if it is polymerized on its own, forms a hydrophobic polymer, (c) 0.5 to 1.5 moles of an ethylenically unsaturated carboxylic acid or maleic anhydride, and (d) 0 to 7 moles of a nonionic, hydrophilic, ethylenically unsaturated monomer, the solution of the prepolymer is diluted with water in a weight ratio of from 1:3 to 1:50 and, in the second polymerization stage, 1 to 32 parts by weight of at least one nonionic, hydrophobic, ethylenically unsaturated monomer, which is the same as monomer (b) of the prepolymer, are polymerized per part by weight of the solution polymer in this polymer solution in the manner of an emulsion polymerization in the presence of a usual amount of a water-soluble polymerization initiator.

    DEVICE AND METHOD FOR PRODUCING MOULDED BODIES FROM THERMOPLASTIC POLYMERS

    公开(公告)号:AU2003218970A1

    公开(公告)日:2003-09-04

    申请号:AU2003218970

    申请日:2003-02-04

    Applicant: BASF AG

    Abstract: An apparatus suitable for producing shaped bodies comprising thermoplastic polymers from monomers which form such polymers in a batch process comprises a) at least one reactor suitable for the batchwise preparation of a melt of a thermoplastic polymer from monomers which form such a polymer, b) a piping system suitable as circulation line for the melt of the thermoplastic polymer and c) at least one apparatus suitable for the production of shaped bodies from the melt of a thermoplastic polymer, wherein the reactor or reactors a) is/are connected to the piping system b) and the apparatus or apparatuses c) is/are connected to the piping system b), and an apparatus for producing shaped bodies comprising thermoplastic polymers in such an apparatus.