公开(公告)号:DE3902440A1
公开(公告)日:1990-08-02
申请号:DE3902440
申请日:1989-01-27
Applicant: BASF AG
Inventor: BOBAR GEORG , SCHNELL KLAUS , SCHROEDER GERD DR , WISTUBA ECKEHARDT DR
IPC: C08F2/00 , C08F2/04 , C08F2/06 , C08F2/38 , C08F20/00 , C08F20/12 , C08L33/08 , C09D7/12 , C09D133/06 , C09J11/08
Abstract: Low-molecular-weight polymers of acrylic acid esters are obtainable by subjecting a) from 80 to 100 % by weight of at least one acrylic acid ester of a C1- to C8-alkanol (monomers I) and b) from 0 to 20 % by weight of other copolymerisable monomers (monomers II) to free-radical polymerisation in a pressure vessel at temperatures of from 130 to 140 DEG C in isopropanol solution in such a manner that from 70 to 95 % by weight of a solvent is introduced into the vessel and the remainder of the polymerisation batch is fed in continuously over the course of from 3 to 7 hours in separate feeds, of which one contains the monomers, and, when the polymerisation is complete, the solvent is removed by vacuum distillation, the proportion by weight of the solvent, based on the monomers, being from 5 to 15 %, the proportion by weight of the initiators, based on the monomers, being from 0.5 to 3 %, and the half life period of the initiators at the polymerisation temperature being from 10 seconds to 3 hours. These low-molecular-weight polymers are suitable as external plasticisers in coating compositions based on synthetic resins.
-
公开(公告)号:DE102006056205A1
公开(公告)日:2007-06-28
申请号:DE102006056205
申请日:2006-11-29
Applicant: BASF AG
Inventor: DOBRAWA RAINER , WIDMAIER RALF , SCHUPP EBERHARD , SCHNELL KLAUS , STRUBE KARL-HERMANN
IPC: C08F226/06 , C08F2/06 , C08F218/04 , C08F220/00
Abstract: A method for the production of vinyl-lactam copolymers (I) by radical polymerisation of water-soluble N-vinyl-lactams (NVL) and hydrophobic comonomers in refluxing organic solvent in presence of initiators, involves adding NVL to the reflux.
-
公开(公告)号:DE102006056203A1
公开(公告)日:2007-06-28
申请号:DE102006056203
申请日:2006-11-29
Applicant: BASF AG
Inventor: DOBRAWA RAINER , WIDMAIER RALF , SCHUPP EBERHARD , SCHNELL KLAUS
IPC: C08F226/06 , C08F2/06 , C08F218/04 , C08F220/00
Abstract: A method for the production of vinyl-lactam copolymers (I) by radical polymerisation of water-soluble N-vinyl-lactams (NVL) and hydrophobic comonomers in refluxing organic solvent in presence of initiators, involves distilling off some of the solvent after 90-99 wt% conversion of the NVL and then continuing the polymerisation.
-
公开(公告)号:DE102006055851A1
公开(公告)日:2007-06-28
申请号:DE102006055851
申请日:2006-11-27
Applicant: BASF AG
Inventor: DOBRAWA RAINER , WIDMAIER RALF , SCHUPP EBERHARD , SCHNELL KLAUS
IPC: C08F226/06 , C08F2/06 , C08F218/04 , C08F220/00
Abstract: In the production of vinyl-lactam copolymers by free radical polymerization of water-soluble N-vinyl-lactam(s) and hydrophobic comonomer(s) in an organic solvent in the presence of an initiator under reflux conditions, the initiator is introduced into the polymerization mixture from below.
-
公开(公告)号:DE59002503D1
公开(公告)日:1993-10-07
申请号:DE59002503
申请日:1990-01-20
Applicant: BASF AG
Inventor: BOBAR GEORG , SCHNELL KLAUS , SCHROEDER GERD DR , WISTUBA ECKEHARDT DR
IPC: C08F2/00 , C08F2/04 , C08F2/06 , C08F2/38 , C08F20/00 , C08F20/12 , C08L33/08 , C09D7/12 , C09D133/06 , C09J11/08
Abstract: Low-molecular-weight polymers of acrylic acid esters are obtainable by subjecting a) from 80 to 100 % by weight of at least one acrylic acid ester of a C1- to C8-alkanol (monomers I) and b) from 0 to 20 % by weight of other copolymerisable monomers (monomers II) to free-radical polymerisation in a pressure vessel at temperatures of from 130 to 140 DEG C in isopropanol solution in such a manner that from 70 to 95 % by weight of a solvent is introduced into the vessel and the remainder of the polymerisation batch is fed in continuously over the course of from 3 to 7 hours in separate feeds, of which one contains the monomers, and, when the polymerisation is complete, the solvent is removed by vacuum distillation, the proportion by weight of the solvent, based on the monomers, being from 5 to 15 %, the proportion by weight of the initiators, based on the monomers, being from 0.5 to 3 %, and the half life period of the initiators at the polymerisation temperature being from 10 seconds to 3 hours. These low-molecular-weight polymers are suitable as external plasticisers in coating compositions based on synthetic resins.
-
公开(公告)号:AT71972T
公开(公告)日:1992-02-15
申请号:AT87109256
申请日:1987-06-26
Applicant: BASF AG
Inventor: UHL GUENTER , TOEX RUDOLF , SCHROEDER GERD DR , SCHNELL KLAUS
IPC: C08F220/12 , C08F20/52 , C08F26/00 , C08F26/10 , C08F220/10 , C08F220/56 , C08F226/06 , C08F226/10 , C09D11/10 , C09D11/106 , D06P5/00 , D06P5/28
-
-
-
-
-