公开(公告)号:DE19950229A1
公开(公告)日:2001-04-26
申请号:DE19950229
申请日:1999-10-19
Applicant: BASF AG
Inventor: SCHNELL KLAUS , KERBER MICHAEL , SCHUPP EBERHARD , WISTUBA ECKEHARDT
IPC: C08F218/08 , C08F226/10 , C08J3/03
Abstract: A copolymerisate comprises (wt.% of total) N-vinylpyrrolidone (30-79.5), vinyl acetate (20-69.5), a 4-20C monovinyl ester of a monocarboxylic acid (0.5-25), and another copolymerisable ethylenically unsaturated compound (0-40), is new. Independent claims are included for: (1) An aqueous solution or dispersion of copolymerisate as above; (2) an aqueous polymer dispersion containing the above copolymerisate as thickener.
-
公开(公告)号:DE50012996D1
公开(公告)日:2006-07-27
申请号:DE50012996
申请日:2000-10-10
Applicant: BASF AG
Inventor: SCHNELL KLAUS , KERBER MICHAEL , SCHUPP EBERHARD , WISTUBA ECKEHARDT
IPC: C08F226/10 , C08F218/08
Abstract: The invention relates to the aqueous preparation of a polymer. Said preparation contains a copolymer consisting of a) 30 to 79.5 wt. % N-vinylpyrrolidone, b) 20 to 69.5 wt. % vinylacetate, c) 0.5 to 25 wt % of a monovinyl ester of a C4 to C20 monocarboxylic acid and d) 0 to 40 wt. % of an additional, copolymerisable, ethylenically unsaturated compound.
-
公开(公告)号:DE4309081A1
公开(公告)日:1994-09-22
申请号:DE4309081
申请日:1993-03-20
Applicant: BASF AG
Inventor: KROENER HUBERTUS DR , SCHUPP EBERHARD DR , WISTUBA ECKEHARDT DR , AYDIN ORAL DR , SCHWARZENBACH ELMAR DR , SCHNELL KLAUS
IPC: C08F16/26 , C08F16/14 , C08F16/16 , C08F16/28 , C08F16/30 , C08F216/18 , C09J129/00 , C09J129/10
Abstract: Adhesives comprising polyvinyl ether copolymers having a weight-average molecular weight > 10,000, which are composed of a) from 0 to 95% by weight of vinyl ethers of the formula I H2C = CH-O-R, b) from 5 to 100% by weight of hydrophilic vinyl ethers of the formula II H2C = CH-O-R , and c) from 0 to 30% by weight of further monomers, in which R is a C1-C10-alkyl group and R1 is an aliphatic or cycloaliphatic radical which may be substituted by hydroxyl groups or interrupted by nonadjacent groups -Y-, where Y is an oxygen atom, a sulphur atom, a group NR or N R R X , in which R and R independently of one another are a hydrogen atom or a C1-C4-alkyl group, and X is a counteranion, and the molar ratio of carbon atoms to the sum of groups Y and hydroxyl groups in the aliphatic or cycloaliphatic radical is from 1.01:1 to 6.5:1.
-
公开(公告)号:DE3776212D1
公开(公告)日:1992-03-05
申请号:DE3776212
申请日:1987-06-26
Applicant: BASF AG
Inventor: UHL GUENTER , TOEX RUDOLF , SCHROEDER GERD DR , SCHNELL KLAUS
IPC: C08F220/12 , C08F20/52 , C08F26/00 , C08F26/10 , C08F220/10 , C08F220/56 , C08F226/06 , C08F226/10 , C09D11/10 , C09D11/106 , D06P5/00 , D06P5/28
Abstract: Binder for transfer printing comprises a copolymer (IA) of 5-95 (wt.)% N-vinylcaprolactam (II), 95-5% N-vinylpyrrolidone (III) and 0.30% 1-14C alkyl or 2-3C hydroxyalkyl (meth)acrylate, (meth)acrylic, maleic or itaconic acid, in the form of alkali or ammonium salt, and/or (meth)acrylamide; or a copolymer (IB) of 20-80% (II) and 80-20% 1-14C alkyl (meth)acrylate and/or acrylamide. If (I) contains 1-4C alkyl (meth)acrylate, the amt. of this is max. 30%. Pref. (IA) contains 20-80% (II), 80-20% (III) and 0-30% 1-8C alkyl or 2-3C hydroxyalkyl acrylate, vinyl-acetate, or -propionate and/or acrylamide. (IB) contains 30-60% (II) and 70-40% acrylamide. The inks and pastes contain 0.1-30% (I); (0.5-20% (I)) in inks and 1.5-30% (I) in pastes.
-
公开(公告)号:DE102006056204A1
公开(公告)日:2007-06-28
申请号:DE102006056204
申请日:2006-11-29
Applicant: BASF AG
Inventor: DOBRAWA RAINER , WIDMAIER RALF , SCHUPP EBERHARD , SCHNELL KLAUS , STRUBE KARL-HERMANN , FILGES ULRICH , NIEBERLE JUERGEN , NEUTZNER JOSEF , DIEING REINHOLD , GRUBER ANDREAS , BOUQUET WOLFGANG
IPC: C08F226/06 , C08F2/06 , C08F218/04 , C08F220/00
Abstract: In the production of vinyl-lactam copolymers by free radical polymerization of water-soluble N-vinyl-lactam(s) and hydrophobic comonomer(s) in an organic solvent in the presence of an initiator, polymerization is carried out under a superpressure high enough to prevent vaporization of the components.
-
公开(公告)号:DE102006056201A1
公开(公告)日:2007-06-28
申请号:DE102006056201
申请日:2006-11-29
Applicant: BASF AG
Inventor: DOBRAWA RAINER , WIDMAIER RALF , SCHUPP EBERHARD , SCHNELL KLAUS , MEISTER MARTIN
IPC: C08F226/06 , C08F2/06 , C08F218/04 , C08F220/00
Abstract: In the production of vinyl-lactam copolymers by free radical polymerization of water-soluble N-vinyl-lactam(s) and hydrophobic comonomer(s) in an organic solvent in the presence of an initiator under reflux conditions, the condensate formed in the reflux is recycled into the polymerization mixture from below.
-
公开(公告)号:DE102006056206A1
公开(公告)日:2007-06-28
申请号:DE102006056206
申请日:2006-11-29
Applicant: BASF AG
Inventor: DOBRAWA RAINER , WIDMAIER RALF , SCHUPP EBERHARD , SCHNELL KLAUS , STRUBE KARL-HERMANN , NIEBERLE JUERGEN , POTZOLLI BERND DE , GRUBER ANDREAS , DIEING REINHOLD
IPC: C08F226/06 , C08F2/06 , C08F218/04 , C08F220/00
Abstract: Free-radical polymerization of at least one of water-soluble N-vinyl lactam and at least one of hydrophobic comonomer, is carried out in an organic solvent, in presence of initiator under reflux conditions, such that at least 10 mol% of N-vinyl lactam is added to polymerization mixture after at least 90 mol% of hydrophobic monomer is completely reacted. Thus, a vinyl lactam copolymer is produced.
-
公开(公告)号:ES2108317T3
公开(公告)日:1997-12-16
申请号:ES94103760
申请日:1994-03-11
Applicant: BASF AG
Inventor: KROENER HUBERTUS DR , SCHUPP EBERHARD DR , WISTUBA ECKEHARDT DR , AYDIN ORAL DR , SCHWARZENBACH ELMAR DR , SCHNELL KLAUS
IPC: C08F16/14 , C08F16/26 , C08F16/16 , C08F16/28 , C08F16/30 , C08F216/18 , C09J129/00 , C09J129/10
Abstract: Adhesives comprising polyvinyl ether copolymers having a weight-average molecular weight > 10,000, which are composed of a) from 0 to 95% by weight of vinyl ethers of the formula I H2C = CH-O-R, b) from 5 to 100% by weight of hydrophilic vinyl ethers of the formula II H2C = CH-O-R , and c) from 0 to 30% by weight of further monomers, in which R is a C1-C10-alkyl group and R1 is an aliphatic or cycloaliphatic radical which may be substituted by hydroxyl groups or interrupted by nonadjacent groups -Y-, where Y is an oxygen atom, a sulphur atom, a group NR or N R R X , in which R and R independently of one another are a hydrogen atom or a C1-C4-alkyl group, and X is a counteranion, and the molar ratio of carbon atoms to the sum of groups Y and hydroxyl groups in the aliphatic or cycloaliphatic radical is from 1.01:1 to 6.5:1.
-
公开(公告)号:DE59404381D1
公开(公告)日:1997-11-27
申请号:DE59404381
申请日:1994-03-11
Applicant: BASF AG
Inventor: KROENER HUBERTUS DR , SCHUPP EBERHARD DR , WISTUBA ECKEHARDT DR , AYDIN ORAL DR , SCHWARZENBACH ELMAR DR , SCHNELL KLAUS
IPC: C08F16/26 , C08F16/14 , C08F16/16 , C08F16/28 , C08F16/30 , C08F216/18 , C09J129/00 , C09J129/10
Abstract: Adhesives comprising polyvinyl ether copolymers having a weight-average molecular weight > 10,000, which are composed of a) from 0 to 95% by weight of vinyl ethers of the formula I H2C = CH-O-R, b) from 5 to 100% by weight of hydrophilic vinyl ethers of the formula II H2C = CH-O-R , and c) from 0 to 30% by weight of further monomers, in which R is a C1-C10-alkyl group and R1 is an aliphatic or cycloaliphatic radical which may be substituted by hydroxyl groups or interrupted by nonadjacent groups -Y-, where Y is an oxygen atom, a sulphur atom, a group NR or N R R X , in which R and R independently of one another are a hydrogen atom or a C1-C4-alkyl group, and X is a counteranion, and the molar ratio of carbon atoms to the sum of groups Y and hydroxyl groups in the aliphatic or cycloaliphatic radical is from 1.01:1 to 6.5:1.
-
公开(公告)号:ES2043124T3
公开(公告)日:1993-12-16
申请号:ES90101149
申请日:1990-01-20
Applicant: BASF AG
Inventor: BOBAR GEORG , SCHNELL KLAUS , SCHROEDER GERD DR , WISTUBA ECKEHARDT DR
IPC: C08F2/00 , C08F2/04 , C08F2/06 , C08F2/38 , C08F20/00 , C08F20/12 , C08L33/08 , C09D7/12 , C09D133/06 , C09J11/08
Abstract: Low-molecular-weight polymers of acrylic acid esters are obtainable by subjecting a) from 80 to 100 % by weight of at least one acrylic acid ester of a C1- to C8-alkanol (monomers I) and b) from 0 to 20 % by weight of other copolymerisable monomers (monomers II) to free-radical polymerisation in a pressure vessel at temperatures of from 130 to 140 DEG C in isopropanol solution in such a manner that from 70 to 95 % by weight of a solvent is introduced into the vessel and the remainder of the polymerisation batch is fed in continuously over the course of from 3 to 7 hours in separate feeds, of which one contains the monomers, and, when the polymerisation is complete, the solvent is removed by vacuum distillation, the proportion by weight of the solvent, based on the monomers, being from 5 to 15 %, the proportion by weight of the initiators, based on the monomers, being from 0.5 to 3 %, and the half life period of the initiators at the polymerisation temperature being from 10 seconds to 3 hours. These low-molecular-weight polymers are suitable as external plasticisers in coating compositions based on synthetic resins.
-
-
-
-
-
-
-
-
-