Abstract:
Polyolefin compositions suitable for injection molded items e.g. for impact bumpers and car interiors comprising from 30% to 90% by weight of an heterophasic propylene polymer composition (A); and from 10% to 70% by weight of a multimodal ethylene/butene- 1 copolymer (B); having density from 0.850 to 0.935 g/cm 3 , total comonomer content from 6% to 30% by weight, Mw/Mn from 4 to 20; intrinsic viscosity in decalin at 135°C from 1.0 to 4.0 dL/g, and comprising an HDPE fraction (HDPE %wt) up to 30%wt; further comprising from 0 to 50 % by weight of a filler (C) and optionally, in amount up to 10% by weight with respect to the overall composition, an impact modifier masterbatch component D consisting of an ultra-soft heterophasic copolymer component.
Abstract:
Flexible polyolefin compositions with improved balance of properties particularly for applications where softness and ductility at low temperature is requested comprising: A) from 20 to 40% by weight of a crystalline polymer fraction consisting of a propylene homopolymer, or a copolymer of propylene, or mixtures thereof, said crystalline fraction having a xylene insoluble fraction at 25°C of at least 90% by weight,. B) from 60 to 80 % by weight of an elastomeric fraction consisting of a copolymeror blend of copolymers of propylene with one or more alpha-olefins, and optionally with minor quantities of a diene; said copolymer or blend containing ethylene in a quantity lower than 40% by weight. the fraction soluble in xylene at 25°C of said polyolefin composition having IVgpc lower than 2.5 dl/g, Mw/Mn (GPC) equal to or higher than 4, Mz/Mw (GPC) equal to or higher than 2.5. Said polyolefin composition optionally further comprising an inorganic filler (II) selected from flame-retardant inorganic fillers and inorganic oxides or salts.
Abstract:
Films especially suitable for the packaging of fresh foodstuff, like salad and vegetables, due to their valuable balance of high permeability to oxygen and optimal permeability to water vapour, comprising at least one layer A) and at least one layer B), wherein the layer A) comprises a copolymer of propylene with hexene-1 containing from 3 to 9% by weight of recurring units derived from hexene-1, said copolymer having a melting temperature from 125°C to 143°C, and the layer B) comprises a polyolefin composition containing (all percentages being by weight): a) 10-40% of one or more propylene homopolymers or copolymers containing over 85% of propylene and having a fraction insoluble in xylene at room temperature greater than 80%; and b) 60-90 of one or more copolymers of ethylene with α-olefin(s), containing ethylene in a quantity from 20 to 80%, and having solubility in xylene at room temperature greater than 70%.
Abstract:
A multilayer film in which at least one layer (A) comprises a copolymer (A1) of propylene with hexene-1 containing from 4 to 10% by weight of hexene-1 and having Melt Flow Rate from 1 to 10 g/10 min.; and at least one layer (B) comprises a copolymer (B1) of ethylene containing up to 20 mol % of CH 2 =CHR α-olefins and having a density from 0.88 to 0.945 g/cm 3 .
Abstract:
A polyolefin composition having unusually low values of flexural modulus and shore hardness andcomprising, in percent by weight: A) 15-40% of a copolymer of propylene with hexene-1 containing from 2.5 to 10% of hexene-1 and having Melt Flow Rate (MFR, measured according to ISO 1133, 230°C/2.16 Kg) from 0.5 to 100g/10 min.; and B) 60-85% of an ethylene copolymer containing ethylene in a quantity equal to or lower than 40%, and having solubility in xylene at room temperature greater than 70%.
Abstract:
A copolymer of propylene with hexene-1 containing from 5 to 9% by weight of recurring units derived from hexene-1, having a melting temperature from 125°C to 140°C and Melt Flow Rate (ASTM D1238, 230°C/2.16 Kg) from 0.1 to 3 g/10 min., is used to produce blown films having valuable mechanical and optical properties.
Abstract:
A polyolefin composition comprising, in percent by weight: A) 10-25% of a propylene homopolymer or copolymer with up to 8% of comonomer(s); B) 75-90% of a copolymer of ethylene and (i) propylene or (ii) CH 2 =CHR alpha- olefins, where R is a 2-8 carbon alkyl radical, or (iii) a combination thereof, optionally with minor amounts of a diene, containing from 54 to 65% of ethylene; wherein the weight ratio B/XS of the content B of copolymer component (B) to the fraction XS soluble in xylene at room temperature, both referred to the total weight of (A) + (B), is of 1.50 or less.
Abstract:
A polyolefin composition comprising, in percent by weight: A) 20-35% of a propylene homopolymer or copolymer with up to 8% of comonomer(s); B) 65-80% of a copolymer of ethylene and (i) propylene or (ii) CH 2 =CHR alpha- olefins, where R is a 2-8 carbon alkyl radical, or (iii) a combination thereof, optionally with minor amounts of a diene, containing from 40 to less than 54% of ethylene; wherein the weight ratio B/XS of the content B of copolymer component (B) to the fraction XS soluble in xylene at room temperature, both referred to the total weight of (A) + (B), is of 1.25 or less.
Abstract:
A masterbatch composition comprising (percent by weight): A) 15%-50% of a polypropylene component having a melt flow rate of from 1 to 250 g/10 min.; and B) 50%-85% of an olefin polymer partially soluble in xylene at room temperature, containing from 60% to 85% by weight of ethylene; said masterbatch composition having (i) a value of the intrinsic viscosity [rl] of the fraction soluble in xylene at room temperature ([rl] SO l) equal to or lower than 2.9 dl/g, and (ii) a value of the ratio MFR / [TI],,,, equal to or lower than 4, is added to polyolefin materials to obtain final compositions suitable for injection molding.
Abstract:
A propylene 1-hexene copolymer containing from 5.5 to 9.0% by weight, of 1-hexene derived units having: a) two peaks in the DSC plot having a difference in height ranging from 0 to 5 mW; b) the higher melting temperature, measured by DSC, ranging from 141.0 °C to 151.0 °C; c) Melt Flow Rate (MFR, measured according to ASTM D 1238, 230°C/2.16 kg, from 3.5 to 8.0 g/10 min.
Abstract translation:包含5.5至9.0重量%的1-己烯衍生单元的丙烯1-己烯共聚物具有:a)DSC曲线中的两个峰,其高度差为0至5mW ; b)由DSC测得的较高熔化温度范围为141.0℃至151.0℃; c)熔体流动速率(MFR,根据ASTM D 1238,230℃/ 2.16kg,3.5至8.0g / 10min测量)