MINERAL FILLED POLYPROPYLENE COMPOSITION
    1.
    发明申请
    MINERAL FILLED POLYPROPYLENE COMPOSITION 审中-公开
    矿物填充聚丙烯组合物

    公开(公告)号:WO2015091372A1

    公开(公告)日:2015-06-25

    申请号:PCT/EP2014/077790

    申请日:2014-12-15

    Abstract: A polypropylene composition for the production of molded articles, such as finished parts for the automotive industry, has melt flow rate (230°C, 2.16 Kg) of at least 25 g /10 min and comprises: (A) 50-95% of a composition having an intrinsic viscosity of the fraction soluble in xylene at 25 °C of 3.0-5.0 dl/g and comprising: (Al) 70-95% of a propylene homopolymer having a Polydispersity Index (PI) of 4.3-10, a fraction insoluble in xylene at 25 °C higher than 90% and a MFR (230°C, 2.16 Kg) of 100- 250 g/10 min; (A2) 5-30% of a copolymer of propylene with 36-44% of ethylene-derived units; (B) optionally up to 45% of a heterophasic propylene polymer, having MFR (230°C, 2.16 Kg) of 10-25 g/10 min, flexural modulus higher than 1400 MPa, and comprising 5-20% of a copolymer rubber component and 80-95% of a matrix propylene polymer component; (C) 2-10% of an ethylene based elastoplastic copolymer; and (D) optionally up to 20% of talc.

    Abstract translation: 用于生产模制品的聚丙烯组合物,例如用于汽车工业的成品,其熔体流动速率(230℃,2.16Kg)为至少25g / 10min,包括:(A)50-95% 在25℃下可溶于二甲苯的馏分的特性粘度为3.0-5.0dl / g的组合物,其组成为:(Al)70-95%的多分散指数(PI)为4.3-10的丙烯均聚物, 在25℃下不溶于二甲苯的馏分高于90%,MFR(230℃,2.16Kg)为100-250g / 10min; (A2)5-30%丙烯与36-44%乙烯衍生单元的共聚物; (B)任选多达45%的多相丙烯聚合物,MFR(230℃,2.16Kg)为10-25g / 10min,弯曲模量高于1400MPa,并且包含5-20%的共聚物橡胶 组分和80-95%的基质丙烯聚合物组分; (C)2-10%的乙烯基弹性共聚物; 和(D)任选地最多20%的滑石。

    POLYMER COMPOSITION FOR BUMPERS AND INTERIORS AND POLYETHYLENE-BASED RESIN PRECURSOR
    3.
    发明申请
    POLYMER COMPOSITION FOR BUMPERS AND INTERIORS AND POLYETHYLENE-BASED RESIN PRECURSOR 审中-公开
    用于缓冲和内部聚合物和聚乙烯基树脂前体的聚合物组合物

    公开(公告)号:WO2013068273A1

    公开(公告)日:2013-05-16

    申请号:PCT/EP2012/071443

    申请日:2012-10-30

    Abstract: Polyolefin compositions suitable for injection moulded items e.g. for impact bumpers and car interiors comprising from 30% to 90% by weight of an heterophasic propylene polymer composition (A); and from 10% to 70% by weight of a multimodal ethylene/C6-C12 alpha olefin copolymer (B); having density from 0.850 to 0.920 g/cm 3 , total comonomer content from 6% to 30% by weight, Mw/Mn from 4 to 20; intrinsic viscosity in decalin at 135°C from 1.0 to 4.0 dL/g, and comprising an HDPE fraction (HDPE %wt) up to 30%wt; further comprising up to 50 % by weight of a filler (C) and optionally, in amount up to 10% by weight with respect to the overall composition, an impact modifier masterbatch component (D) consisting of a ultra-soft heterophasic copolymer component.

    Abstract translation: 适用于注射成型物品的聚烯烃组合物 用于冲击保险杠和汽车内饰,其包含按重量计30%至90%的异相丙烯聚合物组合物(A); 和10重量%至70重量%的多峰乙烯/ C 6 -C 12α-烯烃共聚物(B); 密度为0.850〜0.920g / cm3,总共聚单体含量为6〜30重量%,Mw / Mn为4〜20; 十氢萘在135℃下的特性粘度为1.0至4.0dL / g,并且包含高达30%wt的HDPE级分(HDPE%wt); 进一步包含至多50重量%的填料(C),并且任选地,相对于整个组合物,其量为至多10重量%,由超软多相共聚物组分组成的抗冲改性剂母料组分(D)。

    POLYPROPYLENE COMPOSITIONS CONTAINING GLASS FIBER FILLERS
    4.
    发明申请
    POLYPROPYLENE COMPOSITIONS CONTAINING GLASS FIBER FILLERS 审中-公开
    含玻璃纤维填料的聚丙烯组合物

    公开(公告)号:WO2018086959A1

    公开(公告)日:2018-05-17

    申请号:PCT/EP2017/077854

    申请日:2017-10-31

    Abstract: The present invention concerns polypropylene compositions containing glass fiber fillers, having a high Melt Flow Rate (MFR) and a good balance of mechanical properties. In particular, the compositions of the present invention show excellent mechanical (high stiffness and ductility) and thermal properties (low shrinkage), while displaying a boost of the final MFR, notwithstanding the presence of glass fibers

    Abstract translation: 本发明涉及含有玻璃纤维填料的聚丙烯组合物,其具有高熔体流动速率(MFR)和良好的机械性能平衡。 特别地,尽管存在玻璃纤维,本发明的组合物显示出优异的机械性能(高刚性和延展性)和热性能(低收缩率),同时显示出最终MFR的增强。

    POLYPROPYLENE COMPOSITIONS CONTAINING GLASS FIBER FILLERS
    8.
    发明申请
    POLYPROPYLENE COMPOSITIONS CONTAINING GLASS FIBER FILLERS 审中-公开
    包含玻璃纤维填料的聚丙烯组合物

    公开(公告)号:WO2015000738A1

    公开(公告)日:2015-01-08

    申请号:PCT/EP2014/063236

    申请日:2014-06-24

    Abstract: Composition comprising (A) from 30 to 60 by weight, of a soft polyolefin composition comprising, 10-50 % by weight of a copolymer (a) of propylene, which copolymer contains from 1 to 8 % of comonomer content; 50-90 wt % of a copolymer (b) of ethylene and other alpha-olefin(s), containing from 57 to 80 % of ethylene; wherein the weight ratio of the content of copolymer component (b) to the fraction XS soluble in xylene at room temperature (about 25 °C), both (b and XS) referred to the total weight of (a) + (b), is of 1.5 or less, and the intrinsic viscosity [η] of the said XS fraction is of 3 dl/g or more; and the total quantity of copolymerized ethylene is preferably from 30 % to 65 % by weight; (B) from 5 to 30 wt % of a glass fiber filler; (C) from 0 to 5 % by weight of a compatibilizer; (D) from 10 to 40 by weight of a polypropylene component selected from propylene homopolymers, propylene copolymers containing up to 5 % by moles of ethylene and/or C 4 -C 10 α-olefin(s) and combinations of such homopolymers and copolymers, wherein the Melt Flow Rate, of the polypropylene component D) is generally from 0.3 to 2500 g/10 min.

    Abstract translation: 组合物,其包含(A)30至60重量%的软质聚烯烃组合物,其包含10-50重量%的丙烯共聚物(a),该共聚物含有1至8重量%的共聚单体含量; 50-90重量%的乙烯和其它α-烯烃的共聚物(b),其含有57-80%的乙烯; 其中共聚物组分(b)的含量与在室温(约25℃)下可溶于二甲苯的级分XS的重量比(b和XS)以(a)+(b)的总重量计, 为1.5以下,所述XS馏分的特性粘度[ηe]为3dl / g以上, 共聚乙烯的总量优选为30〜65重量%。 (B)5〜30重量%的玻璃纤维填料; (C)0〜5重量%的增容剂; (D)10至40重量份的选自丙烯均聚物的聚丙烯组分,含有至多5摩尔%乙烯和/或C 4 -C 10α-烯烃的丙烯共聚物以及这些均聚物和共聚物的组合,其中 聚丙烯组分D)的熔体流动速率通常为0.3至2500g / 10min。

    POLYPROPYLENE COMPOSITION AND LIGHT-SOURCE COVERING MADE THEREFROM

    公开(公告)号:WO2022258218A1

    公开(公告)日:2022-12-15

    申请号:PCT/EP2021/087180

    申请日:2021-12-22

    Abstract: The present disclosure provides a covering for a light-source comprising a polyolefin composition comprising: (A) 50-80% by weight, of a propylene polymer comprising up to and including 40% by weight, based on the weight of (A), of units deriving from ethylene and/or at least one alpha-olefin of formula CH2=CHR1, where R1 is a linear or branched C2-C8 alkyl; (B) 15-35% by weight of an elastomeric component selected from the group consisting of: (B1) ethylene copolymers with at least one alpha-olefin of formula CH2=CHR2, where R2 is a linear or branched C1-C8 alkyl, (B2) saturated or unsaturated styrene or alpha-methylstyrene block copolymers, and (B3) combinations thereof; (C) 5-30% by weight of glass fibers, and (D) 0-5.0% by weight of a compatibilizer, wherein the amounts of (A), (B), (C) and (D) are based on the total weight of (A)+(B)+(C)+(D), the total weight being 100%.