公开(公告)号:AT256446B
公开(公告)日:1967-08-25
申请号:AT12065
申请日:1965-01-08
Applicant: BASF AG
Inventor: IKERT BORIS DR , STASTNY FRITZ DR
-
公开(公告)号:AT213063B
公开(公告)日:1961-01-25
申请号:AT693759
申请日:1959-09-24
Applicant: BASF AG
Inventor: KNOBLOCH HORST ERICH DR , MEYER FERDINAND DR , STASTNY FRITZ DR
-
公开(公告)号:DE857341C
公开(公告)日:1952-11-27
申请号:DEB0013207
申请日:1950-12-30
Applicant: BASF AG
Inventor: STASTNY FRITZ DR , TOEPEL TIM DR
-
公开(公告)号:DE855908C
公开(公告)日:1952-11-17
申请号:DEB0007084
申请日:1943-11-30
Applicant: BASF AG
Inventor: STASTNY FRITZ DR
IPC: B29C59/04
-
公开(公告)号:DE845391C
公开(公告)日:1952-07-31
申请号:DEB0008660
申请日:1950-08-10
Applicant: BASF AG
Inventor: STASTNY FRITZ DR
IPC: C08L21/00
-
公开(公告)号:NL144966B
公开(公告)日:1975-02-17
申请号:NL6415189
申请日:1964-12-29
Applicant: BASF AG
Inventor: STASTNY FRITZ DR , HAARDT UDO , GAETH RUDOLF DR , SCHMITT BERNHARD DR
-
公开(公告)号:DE2262250A1
公开(公告)日:1974-07-04
申请号:DE2262250
申请日:1972-12-20
Applicant: BASF AG
Inventor: STASTNY FRITZ DR , GAETH RUDOLF DR , HAARDT UDO , KOERNER HEINZ-HERMANN
IPC: C08G18/00 , B29C39/00 , B29C39/24 , B29C39/26 , B29C67/20 , B29C70/66 , C08J9/22 , C08J9/35 , B29D27/00
Abstract: Composite soft and resilient foams are manufactured by injecting a foamable mixture of polyisocyanates, polyols, water or inert blowing agents and, if appropriate, auxiliaries, under pressure into a mold of which about 90 to 30% of the volume is filled with foamed, soft and resilient particles of olefin polymers of particle size from about 3 to 50 mm and bulk density from 5 to 100 g/l - these particles being in loose form or fused or stuck together - and allowing the reaction mixture to foam up.
-
公开(公告)号:DE1769861A1
公开(公告)日:1971-09-16
申请号:DE1769861
申请日:1968-07-27
Applicant: BASF AG
-
-
公开(公告)号:DE1669648A1
公开(公告)日:1971-05-06
申请号:DE1669648
申请日:1966-05-27
Applicant: BASF AG
Inventor: STASTNY FRITZ DR , GAETH RUDOLF DR , TRIESCHMANN HANS-GEORG PROF DR , ZIZLSPERGER JOHANN DR
Abstract: 1,179,445. Moulding plastic material. BADISCHE ANILIN- & SODA-FABRIK A.G. 26 May, 1967 [27 May, 1966], No. 24598/67. Heading B5A. [Also in Division C3] Expanded olefin polymer mouldings are prepared by mixing particles of an expanded polymer of ethylene or propylene (whose X-ray crystallinity at 25 C. is more than 25%, the particles having a diameter of 3-50 mm. and a bulk density of 5-200 gm/litre) with a curable binder which is free of solvent, compressing the mixture by 5-70% of its original bulk volume in a mould and allowing to cure under pressure. In Example 1 expanded polyethylene particles are mixed with pentaerythritol triglycidyl ether and p,p-diaminodicyclohexylamine and is placed in a wooden mould lined with polyethylene sheeting (25 x 12À5 x 5 cm.) and having a lid of the same material. The contents of the mould are compressed to half their original volume and cured at room temperature. In Example 3 an elevated temperature (70 C.) is employed to cure the mixture. Instead of a mould the mixture may be fed between two conveyer belts to form a sheet, or to a channel provided by four conveyer belts to thereby provide a strand.
-
-
-
-
-
-
-
-
-