公开(公告)号:CA2756023A1
公开(公告)日:2010-09-30
申请号:CA2756023
申请日:2009-03-26
Applicant: BAXTER INT , BAXTER HEALTHCARE SA
Inventor: CHANG MOH-CHING O , DING YUANPANG S , LING MICHAEL T , PUTNAM JOHN W , BONTE JEAN-CLAUDE , BALTEAU PATRICK R
Abstract: Films having peel seal layers and/or barrier layers are provided. In a general embodiment, the present disclosure provides a film comprising a peel seal layer comprising a blend of a polypropylene random copolymer having a melting temperature greater than 145°C, a styrene-ethylene-butylene-styrene block copolymer, and an LLDPE having a melting temperature greater than 120°C.
-
公开(公告)号:AT430021T
公开(公告)日:2009-05-15
申请号:AT02708965
申请日:2002-01-04
Applicant: BAXTER INT
Inventor: LING MICHAEL T , HURST WILLIAM , WOO LECON , BINDOKAS ALGIRDAS , RYAN PATRICK , EDWARDS SCOTT , BLOM HENK , KHARE ATUL
IPC: B32B1/08 , F16L11/04 , A61J1/10 , A61J1/14 , A61L29/12 , A61L31/00 , B29C35/08 , B29C65/04 , B32B25/08 , B32B27/08 , B32B27/32 , C08L23/08 , C08L23/10 , C08L23/12 , C08L23/14 , C08L51/00 , C08L53/02 , C08L75/04 , C08L77/00 , C08L101/00
Abstract: The present invention provides a flowable material container assembly having a membrane tube disposed coaxially within a port tube. The membrane tube has an outer layer, a core layer, and an inner layer. The outer layer is a blend of a polyolefin and a thermoplastic elastomer. The core layer is a blend of a polyolefin and a thermoplastic elastomer. The inner layer is a blend of a polyolefin, a radio frequency susceptible polymer, and a thermoplastic elastomer.
-
公开(公告)号:DE60129208T2
公开(公告)日:2008-03-06
申请号:DE60129208
申请日:2001-02-07
Applicant: BAXTER INT
Inventor: LING MICHAEL T , WOO LECON , WOJNAROWSKI ROBERT , SHAH KETAN , NEBGEN GREGG , DING YUAN-PANG SAMUEL , KALYANKAR VARSHA , ANDERSON KEITH M , ZAKARIJA LILLIAN G , CRAMER COLLEEN S , SCHARF MICHAEL , ROSENBAUM LARRY A
Abstract: The present invention provides a multiple layer thermoplastic structure of a (1) skin layer selected from the group consisting of polypropylene, ethylene homopolymers having a density of from about 0.930 g/cc to about 0.960 g/cc, and ethylene homopolymers having a density of from about 0.930 g/cc to about 0.960 g/cc blended with an ethylene and a-olefin copolymers having a density less than about 0.930 g/cc, the skin layer having a thickness of greater than about 3.0 mils; (2) a radio frequency susceptible layer adhered to the skin layer, the radio frequency susceptible layer having a dielectric loss greater than 0.05 at 1-60 MHz and at temperatures of ambient to 250° C., the radio frequency susceptible layer having: (a) a first polyolefin selected from the group consisting of polypropylene and polypropylene copolymers, (b) a second polyolefin selected from the group consisting of ethylene copolymers, ultra-low density polyethylene, polybutene, and butene ethylene copolymers; (c) a radio frequency susceptible polymer selected from the group consisting of (i) ethylene copolymers having 50-85% ethylene content with comonomers selected from a first group consisting of acrylic acid, methacrylic acid, ester derivatives of acrylic acid with alcohols having 1-10 carbons, ester derivatives of methacrylic acid with alcohols having 1-10 carbons, vinyl acetate, and vinyl alcohol (ii) homopolymers and copolymers containing at least one segment of urethanes, esters, ureas, imides, sulfones, and amides, and (d) a compatibilizing agent of a styrene and hydrocarbon copolymer; wherein the structure when fabricated into a 50 ml container has a water vapor transmission rate of less than 8% by weight after the container has been autoclaved at 121° C. for 20 minutes and stored for 90 days in an environmentally regulated compartment having 15% relative humidity at 40° C.
-
公开(公告)号:DE60129208D1
公开(公告)日:2007-08-16
申请号:DE60129208
申请日:2001-02-07
Applicant: BAXTER INT
Inventor: LING MICHAEL T , WOO LECON , WOJNAROWSKI ROBERT , SHAH KETAN , NEBGEN GREGG , DING YUAN-PANG SAMUEL , KALYANKAR VARSHA , ANDERSON KEITH M , ZAKARIJA LILLIAN G , CRAMER COLLEEN S , SCHARF MICHAEL , ROSENBAUM LARRY A
Abstract: The present invention provides a multiple layer thermoplastic structure of a (1) skin layer selected from the group consisting of polypropylene, ethylene homopolymers having a density of from about 0.930 g/cc to about 0.960 g/cc, and ethylene homopolymers having a density of from about 0.930 g/cc to about 0.960 g/cc blended with an ethylene and a-olefin copolymers having a density less than about 0.930 g/cc, the skin layer having a thickness of greater than about 3.0 mils; (2) a radio frequency susceptible layer adhered to the skin layer, the radio frequency susceptible layer having a dielectric loss greater than 0.05 at 1-60 MHz and at temperatures of ambient to 250° C., the radio frequency susceptible layer having: (a) a first polyolefin selected from the group consisting of polypropylene and polypropylene copolymers, (b) a second polyolefin selected from the group consisting of ethylene copolymers, ultra-low density polyethylene, polybutene, and butene ethylene copolymers; (c) a radio frequency susceptible polymer selected from the group consisting of (i) ethylene copolymers having 50-85% ethylene content with comonomers selected from a first group consisting of acrylic acid, methacrylic acid, ester derivatives of acrylic acid with alcohols having 1-10 carbons, ester derivatives of methacrylic acid with alcohols having 1-10 carbons, vinyl acetate, and vinyl alcohol (ii) homopolymers and copolymers containing at least one segment of urethanes, esters, ureas, imides, sulfones, and amides, and (d) a compatibilizing agent of a styrene and hydrocarbon copolymer; wherein the structure when fabricated into a 50 ml container has a water vapor transmission rate of less than 8% by weight after the container has been autoclaved at 121° C. for 20 minutes and stored for 90 days in an environmentally regulated compartment having 15% relative humidity at 40° C.
-
-
-