ANTISTATIC SHOES
    21.
    发明专利

    公开(公告)号:JP2002248003A

    公开(公告)日:2002-09-03

    申请号:JP2001050556

    申请日:2001-02-26

    Applicant: KAO CORP

    Abstract: PROBLEM TO BE SOLVED: To provide an antistatic shoe sole having an excellent hydrolysis resistance, and excellent strength and appropriate conductivity as a whole, and antistatic shoes using the same. SOLUTION: The antistatic shoe sole having a molding density of 0.9 g/cm or more is formed by reacting a compound having two or more active hydrogen atoms per molecule and containing polyetherpolyol as the main component thereof with a polyisocyanate compound under the presence of an electrically conductive agent and a catalyst and subjecting the product to pressure work. The antistatic shoes comprise the antistatic shoe soles.

    CROSS-LINKED RESIN
    22.
    发明专利

    公开(公告)号:JPH10182818A

    公开(公告)日:1998-07-07

    申请号:JP34811596

    申请日:1996-12-26

    Applicant: KAO CORP

    Abstract: PROBLEM TO BE SOLVED: To obtain a cross-linked resin excellent in properties such as strengths and stability against various solvents by cross-linking a polymer having tert. amino groups in the molecular skeleton and having hydroxyl groups at both molecular terminals with a hydrocarbon having an anionic leaving group in the molecule. SOLUTION: A polymer of a compound represented by formula I (wherein R1 is a 1-24C alkyl or an aralkyl; m is 3-50 on the weight average; R2 is a 2-20C alkylene, an alicyclic alkylene, an aralkylene or the like) is cross-linked with a compound represented by the formula: R3 (-X)n (wherein R3 is an n-valent hydrocarbon group; X is an anionic leaving group; and n is an integer of 2 or greater) (e.g. 1,6-dibromohexane). The tert. alcohol is obtained by for example reacting a dihydric alcohol with a prim. amine. The dihydric alcohol is exemplified by 1,3-butanediol, and the prim. amine is exemplified by methylamine.

    PRODUCTION OF POLYURETHANE FOAM
    23.
    发明专利

    公开(公告)号:JPH0987351A

    公开(公告)日:1997-03-31

    申请号:JP26938495

    申请日:1995-09-21

    Applicant: KAO CORP

    Abstract: PROBLEM TO BE SOLVED: To obtain a polyurethane foam having yellowing resistance and showing unimpaired resin strength in mold release and excellent moldability even when the amount of the water-containing blowing agent is increased by reacting an isocyanato-reactive compound with a polyisocyanate in the presence of a specified catalyst. SOLUTION: In reacting a compound having two or more isocyanato-reactive hydrogen atoms and having a molecular weight of 400-10,000 with a polyisocyanate in the presence of a catalyst and a blowing agent, 0.1-3.0 pts. wt. compound (e.g. a compound of formula II or III) represented by formula I (wherein R1 and R2 are each H or a 1-4 C alkyl) is used per 100 pts.wt. isocyanato-reactive compound to produce a polyurethane foam having density of 0.20-0.40g/cm and a tensile strength of 20kg/cm or above. The use of the above catalyst makes it possible to obtain a polyurethane foam having unimpaired strength by virtue of its excellent gelation reactivity in mold release and excellent moldability, having yellowing resistance, and being suited for especially soles even when the amount of the water as the blowing agent is increased to lower the density of the foam.

    Binder for pavement and mixture for pavement
    24.
    发明专利
    Binder for pavement and mixture for pavement 有权
    用于摊铺和混合的粘合剂

    公开(公告)号:JP2014031649A

    公开(公告)日:2014-02-20

    申请号:JP2012172832

    申请日:2012-08-03

    Abstract: PROBLEM TO BE SOLVED: To provide a binder for pavement from which a mixture for pavement having a higher intensity than that of conventional petroleum asphalt for pavement and more excellent workability than that of cement concrete can be formed.SOLUTION: An inventive binder for pavement consists of polyamide resin only, or a binder mixture of polyamide resin and asphalt. In the case of the binder mixture, a mixing ratio of the polyamide resin is equal to or more than 90 mass% on the basis of the total amount of the polyamide resin and the asphalt, the softening point of the polyamide resin is equal to or more than 70°C and equal to or less than 100°C, and a melt viscosity of the polyamide resin at 180°C is equal to or less than 180 mPa*s.

    Abstract translation: 要解决的问题:提供一种用于路面的粘合剂,由此可以形成比用于路面的常规石油沥青强度高的路面混合物,并且可以形成比水泥混凝土更好的可加工性。解决方案:本发明的路面粘合剂包括 的聚酰胺树脂,或聚酰胺树脂和沥青的粘合剂混合物。 在粘合剂混合物的情况下,基于聚酰胺树脂和沥青的总量,聚酰胺树脂的混合比等于或大于90质量%,聚酰胺树脂的软化点等于或等于 大于70℃且等于或小于100℃,聚酰胺树脂在180℃下的熔融粘度等于或小于180mPa·s。

    Method for manufacturing hydraulic powder
    25.
    发明专利
    Method for manufacturing hydraulic powder 有权
    制造液压粉末的方法

    公开(公告)号:JP2010184818A

    公开(公告)日:2010-08-26

    申请号:JP2009028056

    申请日:2009-02-10

    CPC classification number: C04B24/023 C04B2103/52

    Abstract: PROBLEM TO BE SOLVED: To provide a method for manufacturing a hydraulic powder, whereby a time to achieve a desired particle diameter can be shortened due to superior pulverizing efficiency and the hydraulic powder capable of suppressing strength deterioration caused by degradation can be obtained.
    SOLUTION: The hydraulic powder is manufactured through a step wherein a hydraulic compound is pulverized in the presence of a compound (a) which is an ether of a polyhydric alcohol and 1-5C monohydric alcohol.
    COPYRIGHT: (C)2010,JPO&INPIT

    Abstract translation: 要解决的问题:为了提供一种制造水硬性粉末的方法,由于优异的粉碎效率可以缩短达到期望粒径的时间,并且可以获得能够抑制由劣化引起的强度劣化的水硬性粉末 。 解决方案:通过在作为多元醇的醚和1-5C一元醇的化合物(a)的存在下将水硬性化合物粉碎的步骤制造水硬性粉末。 版权所有(C)2010,JPO&INPIT

    Water-reducing agent for hydraulic composition
    26.
    发明专利
    Water-reducing agent for hydraulic composition 有权
    减水剂用于液压组合物

    公开(公告)号:JP2010059045A

    公开(公告)日:2010-03-18

    申请号:JP2009183231

    申请日:2009-08-06

    CPC classification number: C04B24/226 C04B2103/302 C08G16/0237

    Abstract: PROBLEM TO BE SOLVED: To provide a naphthalene-based water-reducing agent capable of giving outstanding flow retention effectiveness and strength development effectiveness for a hydraulic composition.
    SOLUTION: The water-reducing agent for a hydraulic composition includes a naphthalenesulfonic acid-formaldehyde condensate which has a weight average molecular weight of 1,900-24,000 as determined by GPC and in which the peak area of a molecular weight of 4,000 or below as determined by GPC is 17 to 38% of the whole peak area as determined thereby.
    COPYRIGHT: (C)2010,JPO&INPIT

    Abstract translation: 要解决的问题:提供一种能够赋予液压组合物优异的流动保持效果和强度显影效果的萘系减水剂。 解决方案:用于水硬性组合物的减水剂包括通过GPC测定的重均分子量为1900-24,000的萘磺酸 - 甲醛缩合物,其中分子量为4,000或更低的峰面积 通过GPC测定,由此确定的峰面积的17〜38%。 版权所有(C)2010,JPO&INPIT

    Hydraulic composition
    27.
    发明专利
    Hydraulic composition 有权
    液压组合物

    公开(公告)号:JP2010037130A

    公开(公告)日:2010-02-18

    申请号:JP2008200927

    申请日:2008-08-04

    Abstract: PROBLEM TO BE SOLVED: To provide a hydraulic composition which can suppress blackening generated in the skin face of a hardened body in a blend system more containing black particle components.
    SOLUTION: The hydraulic composition comprises: a polymer (A) composed of a structural unit including the structural unit derived from a monomer expressed by formula (1): H
    2 C=CHCOOCH
    2 CH
    2 OH by ≥70 wt.%; a formaldehyde naphthalenesulfonate condensate (B); hydraulic powder (C); powder (X) containing black fine powder; fine aggregate; coarse aggregate; and water, and in which the ratio between the hydraulic powder (C) and the powder (X) containing black fine powder satisfies (C)/(X)=95/5 to 20/80 (by volume ratio), and the content of the polymer (A) to 100 pts.wt. total of the hydraulic powder (C) and the powder (X) containing black fine powder is 0.02 to 0.3 pts.wt.
    COPYRIGHT: (C)2010,JPO&INPIT

    Abstract translation: 要解决的问题:提供一种水硬性组合物,其可以抑制更多含有黑色颗粒组分的共混体系中的硬化体的皮肤表面产生的黑化。 水溶液组合物包含:由包含由式(1)表示的单体衍生的结构单元的结构单元组成的聚合物(A):H SB 2 C = CHCOOCH SB < 2 2 OH≥70重量%; 甲醛萘磺酸盐缩合物(B); 水硬粉(C); 粉末(X)含黑色细粉; 细骨料 粗骨料 和水,其中水硬性粉末(C)和含有黑色细粉末的粉末(X)的比例满足(C)/(X)= 95/5〜20/80(体积比),含量 的聚合物(A)至100重量份 水硬性粉末(C)和含有黑色细粉末的粉末(X)的总和为0.02〜0.3重量份。 版权所有(C)2010,JPO&INPIT

    Method for producing foamed polyurethane
    28.
    发明专利
    Method for producing foamed polyurethane 有权
    生产泡沫聚氨酯的方法

    公开(公告)号:JP2007297418A

    公开(公告)日:2007-11-15

    申请号:JP2006123809

    申请日:2006-04-27

    Abstract: PROBLEM TO BE SOLVED: To provide a method for producing foamed polyurethane by which formation of fine foam diameter and increase of foam number density are achieved. SOLUTION: A gas is dissolved in a composition containing a polyurethane resin and a hydrophobic silica under pressure and foam is generated in the composition under reduced pressure to produce the foamed polyurethane. In the polyurethane foam obtained by the method, average foam diameter is preferably ≤1.5 μm and volume content of the gas is preferably ≥1%. COPYRIGHT: (C)2008,JPO&INPIT

    Abstract translation: 待解决的问题:提供一种生产发泡聚氨酯的方法,其通过形成细泡沫直径和提高泡沫数密度来实现。 解决方案:在压力下将气体溶解在含有聚氨酯树脂和疏水性二氧化硅的组合物中,并在组合物中在减压下产生泡沫以制备发泡聚氨酯。 在通过该方法获得的聚氨酯泡沫中,平均泡沫直径优选为≤1.5μm,气体的体积含量优选为≥1%。 版权所有(C)2008,JPO&INPIT

    Method for producing polyurethane foam
    29.
    发明专利
    Method for producing polyurethane foam 有权
    生产聚氨酯泡沫的方法

    公开(公告)号:JP2006182874A

    公开(公告)日:2006-07-13

    申请号:JP2004376481

    申请日:2004-12-27

    Inventor: OKUBO MAKOTO

    Abstract: PROBLEM TO BE SOLVED: To provide a polyester polyol capable of giving a polyuretahne foam having a low density, having a good outward appearance, and excellent in mechanical strength, such as tensile strength, tear strength, and elongation at break, and to provide a method for producing the polyurethane foam using the same.
    SOLUTION: This polyester polyol is given by subjecting (A) an acid component containing succinic acid and sebacic acid and (B) a polyhydric alcohol to condensation polymerization and has a viscosity at 40°C of ≤10,000 mPa×s. The method for producing the polyurethane foam comprises together reacting a polyisocyanate component and a polyol component containing the polyester polyol and making the components foam.
    COPYRIGHT: (C)2006,JPO&NCIPI

    Abstract translation: 解决问题的方法:提供一种聚酯多元醇,其能够提供低密度聚氨酯泡沫,外观良好,机械强度优异,如拉伸强度,撕裂强度和断裂伸长率,以及 以提供使用其制造聚氨酯泡沫的方法。 解决方案:该聚酯多元醇通过(A)含有琥珀酸和癸二酸的酸成分和(B)多元醇进行缩聚而得到,并且在40℃下的粘度为≤10,000mPa·s。 制备聚氨酯泡沫的方法包括使多异氰酸酯组分和含有聚酯多元醇的多元醇组分反应并使组分发泡。 版权所有(C)2006,JPO&NCIPI

    THERMOSETTING POLYURETHANE COMPOSITION

    公开(公告)号:JP2002161125A

    公开(公告)日:2002-06-04

    申请号:JP2000360515

    申请日:2000-11-28

    Applicant: KAO CORP

    Abstract: PROBLEM TO BE SOLVED: To provide a one-pack thermosetting polyurethane composition which is serviceable to sealing material use and has a high tenacity and a rubber elasticity curing characteristic. SOLUTION: This thermosetting polyurethane composition contains a polyurethane prepolymer and/or a polyisocyanate compound having an isocyanate group blocked with a blocking agent and a polyamine expressed in a general formula(1) (wherein R is a 8-22C linear or branched hydrocarbon; x is an integer of 1-5; y and z are each an integer of 0-5 but they never are 0 simultaneously).

Patent Agency Ranking