公开(公告)号:CA2461675C
公开(公告)日:2010-09-21
申请号:CA2461675
申请日:2002-09-30
Applicant: BASF AG
Inventor: MANDERS LAMBERTUS , WIRTH THOMAS , GASCHLER WOLFGANG , KROENER HUBERTUS
IPC: C08F2/22 , C08F212/08 , C08F2/16 , C08F2/38 , C08F212/00 , C08F236/00 , C08F236/10
Abstract: The invention relates to a method for producing an aqueous styrene-butadiene polymer dispersion by the radical aqueous emulsion-polymerisation of a monomer mixture M, containing: between 40 and 80 wt. % styrene as monomer M1; between 20 and 60 wt. % butadiene as monomer M2 and between 0 and 40 wt. %, (in relation to l00 wt. % monomers), of ethylenically unsaturated comonomers M3 that differ from styrene and butadiene, according to a monomer feed process in the presence of between 0.05 and 0.5 wt. %, (in relation to l00 wt. % monomers), of at least one hydrocarbon KW comprising between 6 and 20 C atoms, selected from compounds, which form a pentadienyl or a 1-phenylallyl radical during the abstraction of a hydrogen atom, or from .alpha.-methylstyrene dimers. Said method is characterised in that the concentration of the butadiene in the monomer feed is increased by at least 10 wt. % in relation to the monomers in the feed process, for a period of at least 1 % of the entire feed duration, when at least 70 % of the monomers to be polymerised have been fed to the polymerisation reaction.
-
公开(公告)号:AU2007263813A1
公开(公告)日:2008-01-03
申请号:AU2007263813
申请日:2007-06-19
Applicant: BASF AG
Inventor: GASCHLER WOLFGANG , MANDERS LAMBERTUS , GUBAYDULLIN ILSHAT
Abstract: A process for preparing an aqueous polymer dispersion using flush water.
-
公开(公告)号:DE50207217D1
公开(公告)日:2006-07-27
申请号:DE50207217
申请日:2002-09-30
Applicant: BASF AG
Inventor: GASCHLER WOLFGANG , SCHAEDLER VOLKER , MANDERS LAMBERTUS , WIRTH THOMAS , KROENER HUBERTUS
IPC: C08F212/08 , C08F2/38 , C08F220/04 , C08F220/44 , C08F236/06 , C08F236/10 , C08F291/00 , C09D5/02 , C09D109/06 , C09D109/08 , C09D125/10 , D21H17/35 , D21H19/58
Abstract: A process for preparing an aqueous styrene-butadiene polymer dispersion by free-radical aqueous emulsion polymerization of a monomer mixture M comprising styrene, butadiene, and if desired up to 30% by weight, based on 100% by weight of monomers, of ethylenically unsaturated comonomers other than styrene and butadiene; in a polymerization vessel by a monomer feed technique in the presence of a regulator system containing, based on 100% by weight of monomers, from 0.02 to 0.5% by weight of at least one hydrocarbon HC having from 6 to 20 carbon atoms, selected from compounds which on abstraction of a hydrogen atom form a pentadienyl radical or 1-phenylallyl radical, and alpha-methylstyrene dimer, and from 0.3 to 2% by weight of an organic compound S containing at least one SH group wherein at least 30%, preferably at least 50%, in particular at least 80%, and with particular preference the entirety (or >95%) of hydrocarbon HC is included in the initial charge to the polymerization vessel.
-
公开(公告)号:AT329945T
公开(公告)日:2006-07-15
申请号:AT02779444
申请日:2002-09-30
Applicant: BASF AG
Inventor: GASCHLER WOLFGANG , SCHAEDLER VOLKER , MANDERS LAMBERTUS , WIRTH THOMAS , KROENER HUBERTUS
IPC: C08F2/38 , C08F212/08 , C08F220/04 , C08F220/44 , C08F236/06 , C08F236/10 , C09D5/02 , C09D109/06 , C09D109/08 , C09D125/10 , D21H19/58 , C08F291/00 , D21H17/35
Abstract: A process for preparing an aqueous styrene-butadiene polymer dispersion by free-radical aqueous emulsion polymerization of a monomer mixture M comprising styrene, butadiene, and if desired up to 30% by weight, based on 100% by weight of monomers, of ethylenically unsaturated comonomers other than styrene and butadiene; in a polymerization vessel by a monomer feed technique in the presence of a regulator system containing, based on 100% by weight of monomers, from 0.02 to 0.5% by weight of at least one hydrocarbon HC having from 6 to 20 carbon atoms, selected from compounds which on abstraction of a hydrogen atom form a pentadienyl radical or 1-phenylallyl radical, and alpha-methylstyrene dimer, and from 0.3 to 2% by weight of an organic compound S containing at least one SH group wherein at least 30%, preferably at least 50%, in particular at least 80%, and with particular preference the entirety (or >95%) of hydrocarbon HC is included in the initial charge to the polymerization vessel.
-
公开(公告)号:BR0212879A
公开(公告)日:2004-10-13
申请号:BR0212879
申请日:2002-09-30
Applicant: BASF AG
Inventor: MANDERS LAMBERTUS , WIRTH THOMAS , GASCHLER WOLFGANG , NER HUBERTUS KR
IPC: C08F2/38 , C08F212/08 , C08F236/06
Abstract: A process for preparing an aqueous styrene-butadiene polymer dispersion by free-radical aqueous emulsion polymerization of a monomer mixture M containing from 40 to 80% by weight of styrene as monomer M1, from 20 to 60% by weight of butadiene as monomer M2, and from 0 to 40% by weight, based on 100% by weight of monomers, of ethylenically unsaturated comonomers M3 other than styrene and butadiene by a monomer feed technique in the presence of from 0.05 to 0.5% by weight, based on 100% by weight of monomers, of at least one hydrocarbon HC selected from compounds having 6 to 20 carbon atoms which on abstraction of a hydrogen atom form a pentadienyl radical or a 1-phenylallyl radical and from alpha-methylstyrene dimer comprises supplying the monomers to be polymerized to the polymerization reaction over the course of 3 hours.
-
公开(公告)号:BR0212875A
公开(公告)日:2004-10-13
申请号:BR0212875
申请日:2002-09-30
Applicant: BASF AG
Inventor: GASCHLER WOLFGANG , SCHODLER VOLKER , MANDERS LAMBERTUS , WIRTH THOMAS , NER HUBERTUS KR
IPC: C08F2/38 , C08F212/08 , C08F220/04 , C08F220/44 , C08F236/06 , C08F236/10 , C09D5/02 , C09D109/06 , C09D109/08 , C09D125/10 , D21H19/58 , C08F291/00 , D21H17/35
Abstract: A process for preparing an aqueous styrene-butadiene polymer dispersion by free-radical aqueous emulsion polymerization of a monomer mixture M comprising styrene, butadiene, and if desired up to 30% by weight, based on 100% by weight of monomers, of ethylenically unsaturated comonomers other than styrene and butadiene; in a polymerization vessel by a monomer feed technique in the presence of a regulator system containing, based on 100% by weight of monomers, from 0.02 to 0.5% by weight of at least one hydrocarbon HC having from 6 to 20 carbon atoms, selected from compounds which on abstraction of a hydrogen atom form a pentadienyl radical or 1-phenylallyl radical, and alpha-methylstyrene dimer, and from 0.3 to 2% by weight of an organic compound S containing at least one SH group wherein at least 30%, preferably at least 50%, in particular at least 80%, and with particular preference the entirety (or >95%) of hydrocarbon HC is included in the initial charge to the polymerization vessel.
-
公开(公告)号:BR0212869A
公开(公告)日:2004-09-14
申请号:BR0212869
申请日:2002-09-30
Applicant: BASF AG
Inventor: MANDERS LAMBERTUS , WIRTH THOMAS , GASCHLER WOLFGANG , NER HUBERTUS KR
IPC: C08F2/22 , C08F2/16 , C08F2/38 , C08F212/00 , C08F236/00 , C08F236/10 , C08F212/08
-
公开(公告)号:DE10148497A1
公开(公告)日:2003-04-17
申请号:DE10148497
申请日:2001-10-01
Applicant: BASF AG
Inventor: MANDERS LAMBERTUS , WIRTH THOMAS , GASCHLER WOLFGANG , KROENER HUBERTUS
IPC: C08F2/38 , C08F212/08 , C08F236/06
Abstract: The invention relates to a method for producing an aqueous styrene-butadiene polymer dispersion by carrying out a radical aqueous emulsion polymerization of a monomer mixture M containing: 40 to 80 wt. % of styrene depicted as Monomer M1; 20 to 60 wt. % of butadiene depicted as monomer M2, and; 0 to 40 wt. %, with regard to 100 wt. % of the monomers, of ethylenically unsaturated comonomers M3 that differ from styrene and butadiene. The polymerization is carried out according to a monomer feeding method in the presence of 0.05 to 0.5 wt. %, with regard to 100 wt. % of the monomers, of at least one hydrocarbon KW selected among compounds having 6 to 20 C atoms that form a pentadienyl radical or a 1-phenylallyl radical when a hydrogen atom is abstracted, and the alpha -methylstyrene dimer. The inventive method is characterized in that the monomers to be polymerized are introduced within three hours of the polymerization reaction.
-
公开(公告)号:DE10148494A1
公开(公告)日:2003-04-17
申请号:DE10148494
申请日:2001-10-01
Applicant: BASF AG
Inventor: GASCHLER WOLFGANG , SCHAEDLER VOLKER , MANDERS LAMBERTUS , WIRTH THOMAS , KROENER HUBERTUS
IPC: C08F2/22 , C08F2/38 , C08F212/00 , C08F212/08 , C08F236/00 , C08F236/10 , C08F236/06
Abstract: The invention relates to a method for producing an aqueous styrene-butadiene polymer dispersion by the radical aqueous emulsion-polymerisation of a monomer mixture M, containing: between 40 and 80 wt. % styrene as monomer M1; between 20 and 60 wt. % butadiene as monomer M2 and between 0 and 40 wt. %, (in relation to l00 wt. % monomers), of ethylenically unsaturated comonomers M3 that differ from styrene and butadiene, according to a monomer feed process in the presence of between 0.05 and 0.5 wt. %, (in relation to l00 wt. % monomers), of at least one hydrocarbon KW comprising between 6 and 20 C atoms, selected from compounds, which form a pentadienyl or a 1-phenylallyl radical during the abstraction of a hydrogen atom, or from alpha -methylstyrene dimers. Said method is characterised in that at least 30 % of the hydrocarbon KW is already present in the polymerisation vessel and the residual quantity of the hydrocarbon KW is fed to the polymerisation reaction during the course of the latter.
-
公开(公告)号:DE10046930A1
公开(公告)日:2002-04-18
申请号:DE10046930
申请日:2000-09-21
Applicant: BASF AG
Inventor: SCHAEDLER VOLKER , MANDERS LAMBERTUS , ETTL ROLAND , WIRTH THOMAS
IPC: C08F2/38 , C08F212/08 , C08F236/10 , D21H19/58 , C08F236/06 , C08F220/42
Abstract: A method for the production of aqueous styrene-butadiene polymer dispersions by radical emulsion polymerisation (monomer addition method) of a mixture of styrene, butadiene and up to 30 wt% other olefinic monomers, in which a regulator system comprising 0.02-0.4 wt% terpinols and 0.5-2 wt% organic compound (S) with SH group(s) is added during polymerisation. Independent claims are also included for (a) aqueous polymer dispersions obtained by this method; (b) paper coating materials containing inorganic pigment(s), 5-20 parts by weight (pts. wt.) polymer dispersion as above and 0.1-5 pts. wt. conventional additives (all based on 100 pts. wt. pigment).
-
-
-
-
-
-
-
-
-