公开(公告)号:DE59407786D1
公开(公告)日:1999-03-25
申请号:DE59407786
申请日:1994-04-22
Applicant: HOECHST AG
Inventor: HOENEL MICHAEL DR , VOELKER ACHIM DR , WALZ GERD DR , ZIEGLER PETER DR
IPC: C08G18/08 , C08F2/16 , C08F2/18 , C08F2/44 , C08F283/00 , C08G18/00 , C08G18/63 , C08G18/64 , C08G18/70 , C08G18/80 , C08L63/00 , C08L75/00 , C08L75/04 , C09D5/44 , C09D163/00 , C09D175/00 , C09D175/04 , C25D15/02
Abstract: Aqueous synthetic resin dispersions containing A) an ionic resin, preferably a cationic resin, B) a masked polyisocyanate and C) a polymer comprising at least one free-radical-polymerizable ethylenically unsaturated monomer. These synthetic resin dispersions are used as binders in electrodeposition coating baths.
-
公开(公告)号:GR3020291T3
公开(公告)日:1996-09-30
申请号:GR960401456
申请日:1996-06-20
Applicant: HOECHST AG
Inventor: WALZ GERD DR , HOENEL MICHAEL DR , BRINDOEPKE GERHARD DR , SPRENGER WALTER , FINKE MANFRED DR , LENZ RUEDIGER DR
IPC: C07D317/36 , C07C67/00 , C07C239/00 , C07C269/00 , C07C271/20 , C07D303/28 , C08G18/06 , C08G18/32 , C08G18/64 , C08G18/70 , C08G18/80 , C08G18/83 , C08G59/02 , C08G59/40 , C08G71/04 , C09D5/44 , C09D175/04 , C09D175/12
Abstract: Amino-urethanes (I) claimed are of formula R3-N(Re)-A-R1-NH-C(O)-O-CH2-CH(OH)-CH2- R-CH2-CH(OH)-CH2-O-C(O)-NH- R1-A-N(R2)R3 R is residue of a diglycidyl ether or ester, or 2-18 alkylene gp.; R1 is opt. branched 2-18C alkylene; R2 is H, 1-8Calkyl, or 1-8C hydroxyalkyl; R3 is R2, or R3 with R2 can form cyclic ring, or, if R2 is H then R3 can be at least one gp. of formula (a) -C(O)-O-CH2-CH(R4)-CH2- (R-CH2-CH(R4)-CH2-OmB-(R4)n R4 is OH or -CONH-PI-NHCO R6; B is residue of a polyol; m is 1-3; n is 1-6; and PI is residue of a polyisocyanate and R6 is residue of (cylco)aliphatic, or alkylaromatic alcohol, an aminoalcohol, ketoxime, or a CH- or NH- acidic cpd.: b) R3 is gp. of formula (I) R5 is H or R4; R7 is 1-8Calkyl; and s is 1-6; c) -C(O)-NH-PI-NH-C(O)-O-B-d)R8-CHOH-CH2-O-CO-; e) R8-CHOH-CH2-; R8 is H, 1-18C alkyl, or residue of a glycidyl ester or ether; or f) PI'NHCO- PI' is residue of a partly capped polyisocyanate; and A 75 chemical bond or -R1NH)r-R1NH- r is 0-6. Prodn. of a (I) by heating an at least bifunctional 2-oxo-1,3-dioxolan (II) and a prim polyamine at 20-150 deg.C is claimed. Structural formulae are given for pref. R, viz. residues of a bisphenol diglycidyl ether opt. linked by residues of a diamine, diol, dicarboxylic acid, di-isocyanate, etc. Pref. (II) is bicyclic carbonate of specified formuls esp. derived from polyglycidyl ether of a polyphenol, or a epoxide-cyclic carbonate.
-
公开(公告)号:DK0547502T3
公开(公告)日:1995-08-07
申请号:DK92121047
申请日:1992-12-10
Applicant: HOECHST AG
Inventor: HOENEL MICHAEL DR , NEUMANN UWE DR , OBERRESSL PAUL , KELLER MARION
IPC: C08G59/14 , C08G59/18 , C08L63/00 , C08L67/00 , C09D163/00 , C09D167/00
-
公开(公告)号:DE4344510A1
公开(公告)日:1995-06-29
申请号:DE4344510
申请日:1993-12-24
Applicant: HOECHST AG
Inventor: HOENEL MICHAEL DR , PFEIL ARMIN DR , BUDNICK THOMAS , SCHWAN HEINER DR
IPC: B05D7/24 , B05C9/06 , B05D7/14 , C08G59/50 , C08G71/00 , C08G71/04 , C09D163/00 , C09D175/04 , B05D1/38 , B05D7/16 , C09D175/12
-
公开(公告)号:DE3850185D1
公开(公告)日:1994-07-21
申请号:DE3850185
申请日:1988-08-02
Applicant: HOECHST AG
Inventor: HOENEL MICHAEL DR , ZIEGLER PETER DR , FOEDDE HARTMUT
Abstract: Curable compounds carrying basic nitrogen groups and essentially comprising structural units derived from A) a compound containing on average at least one terminal 2-oxo-1,3-dioxolane group per molecule, with B) a disecondary amine containing hydroxyl groups in the beta -position to the secondary amino groups, it also being possible for this amine to contain blocked primary amino groups, and optionally C) a bifunctional amine containing at least one free primary amino group and optionally at least one secondary amino group, are used, in particular, in surface coating preparations, especially in electrodeposition coating compositions. The coatings obtainable using these compositions have, in particular optimised interlayer adhesion.
-
公开(公告)号:DE58906869D1
公开(公告)日:1994-03-17
申请号:DE58906869
申请日:1989-06-07
Applicant: HOECHST AG
Inventor: HOENEL MICHAEL DR , ZIEGLER PETER DR , SPRENGER WALTER , WENDT WOLFGANG
IPC: C08G73/00 , C08G18/08 , C08G18/64 , C08G18/71 , C08G18/80 , C08G18/83 , C08G71/04 , C08J3/20 , C09D5/44 , C09D17/00
Abstract: The invention relates to paste resins containing (a) quaternary ammonium groups, (b) OH groups, (c) isocyanate radicals and (d) groups of the formula (I) in which R to R , independently of one another are hydrogen or a hydrocarbon radical having 1 to 10 carbon atoms, and X is hydroxyl or an isocyanate radical, the mean molecular weight (Mn) of these paste resins being from 500 to 10000. The invention furthermore relates to the preparation of these paste resins, to their use for pigment pastes and to these pigment pastes. water-thinable surface coatings, in particular electrodeposition coatings, which contain the pigment pastes according to the invention give defect-free surfaces and comparable coating thicknesses, even on different substrates.
-
公开(公告)号:DE4128487A1
公开(公告)日:1993-03-04
申请号:DE4128487
申请日:1991-08-28
Applicant: HOECHST AG
Inventor: DREISCHHOFF HANS-DIETER , GEISLER JOERG-PETER DR , GODAU CLAUS DIPL ING , HOENEL MICHAEL DR
IPC: C08L63/00 , C08G59/00 , C08J3/03 , C09D163/00 , C09K23/52
Abstract: A process for the preparation of aqueous epoxy resin dispersions comprising (1) 20 to 75% by weight, based on the total dispersion, of an epoxy resin constituting a condensation product of a) epoxy compounds having at least one epoxy group per molecule and an epoxide equivalent weight of 90 to 3000 g/mol, and b) aromatic polyols; (2) 3 to 20% by weight, based on the total dispersion, of an emulsifier comprising a) a condensation product of an aliphatic polyol and an epoxy compound having at least two epoxy groups per molecule and an epoxide equivalent weight of 90 to 3000 g/mol, the equivalent ratio of the OH groups to the epoxy groups being 1:0.85 to 1:1.5 and the epoxide equivalent weight of this condensation product being between 5000 and 400,000 g/mol, b) an organic solvent, and c) water; (3) up to 10% by weight, based on the total dispersion, of organic solvents; and (4) water in an amount to make up to 100% by weight, which comprises stirring the epoxy resin (1) firstly with the emulsifier (2) and, if appropriate, organic solvents corresponding to (3), and then with water.
-
公开(公告)号:DE3644373A1
公开(公告)日:1988-07-07
申请号:DE3644373
申请日:1986-12-24
Applicant: HOECHST AG
Inventor: BRINDOEPKE GERHARD DR , HOENEL MICHAEL DR
IPC: C08F8/30 , C08F8/32 , C08F20/26 , C08F20/28 , C08G18/67 , C09D5/44 , C09D201/02 , C08F224/00 , C08F220/30 , C08F220/36 , C09D3/727
Abstract: Non-crosslinked reaction products of compounds (A) which contain structural units carrying 1,3-dioxolan-2-one groups in random distribution and compounds (B) which contain at least one primary aliphatic or cycloaliphatic amino group and additionally at least one further basic amino group. These reaction products are suitable, if appropriate together with conventional curing agents, especially as binders for coatings, above all electrodip coatings.
-
公开(公告)号:DK0530602T3
公开(公告)日:2000-08-28
申请号:DK92114212
申请日:1992-08-20
Applicant: HOECHST AG
Inventor: GODAU CLAUS DI , DREISCHHOFF DIETER , GEISLER JOERG-PETER DR , GLAUS DI GODAU , HOENEL MICHAEL DR
IPC: C08G59/00 , C08J3/03 , C08L63/00 , C09D163/00 , C09K23/52
Abstract: A process for the preparation of aqueous epoxy resin dispersions comprising (1) 20 to 75% by weight, based on the total dispersion, of an epoxy resin constituting a condensation product of a) epoxy compounds having at least one epoxy group per molecule and an epoxide equivalent weight of 90 to 3000 g/mol, and b) aromatic polyols; (2) 3 to 20% by weight, based on the total dispersion, of an emulsifier comprising a) a condensation product of an aliphatic polyol and an epoxy compound having at least two epoxy groups per molecule and an epoxide equivalent weight of 90 to 3000 g/mol, the equivalent ratio of the OH groups to the epoxy groups being 1:0.85 to 1:1.5 and the epoxide equivalent weight of this condensation product being between 5000 and 400,000 g/mol, b) an organic solvent, and c) water; (3) up to 10% by weight, based on the total dispersion, of organic solvents; and (4) water in an amount to make up to 100% by weight, which comprises stirring the epoxy resin (1) firstly with the emulsifier (2) and, if appropriate, organic solvents corresponding to (3), and then with water.
-
公开(公告)号:AT147419T
公开(公告)日:1997-01-15
申请号:AT90118375
申请日:1990-09-25
Applicant: HOECHST AG
Inventor: HOENEL MICHAEL DR , WALZ GERD DR , ZIEGLER PETER DR , KUBILLUS UWE DR
IPC: C09D7/12 , C08G59/50 , C08L63/00 , C08L101/00 , C09D5/02 , C09D5/44 , C09D163/00 , C09D201/00
Abstract: The invention relates to the use of crosslinked polymer microparticles having an average particle size of at most 5 mu m and a glass transition temperature (Tg) of at least +30 DEG C. in aqueous paint preparations as filler and/or as partial substitute of white pigments, in particular of titanium dioxide. Among other things, the corresponding paints show increased spreading power, less tendency for sedimentation and reduced crater formation.
-
-
-
-
-
-
-
-
-