ALUMINUM ALLOY SHEET COMPOSITION AND PRODUCTS
    31.
    发明申请
    ALUMINUM ALLOY SHEET COMPOSITION AND PRODUCTS 审中-公开
    铝合金板材组合物和产品

    公开(公告)号:WO1995027805A1

    公开(公告)日:1995-10-19

    申请号:PCT/US1995004270

    申请日:1995-04-07

    Abstract: An aluminum alloy composition for sheet product consists essentially of 0.3 to 1.1 wt. % silicon, 0.4 to 1.0 wt. % iron, 0.009 to 0.25 wt. % copper and optionally, minor amounts of manganese, magnesium, chromium, zinc, titanium and other incidental impurities with the balance aluminum. In making aluminum sheet from this composition, the aluminum alloy is continuously cast into an intermediate gauge sheet product and directly cold rolled without an intermediate thermal treatment to final gauge. Optionally, the final gauge sheet product can be subjected to a known temper practice. Using the iron, silicon and copper- containing aluminum alloy composition, a sheet product is produced which has acceptable mechanical properties for use as general purpose aluminum sheet, semi-rigid aluminum container stock, consumer wrap container, cutter bars and the like. The figure shows the method steps of fabricating a sheet product.

    Abstract translation: 用于片材产品的铝合金组合物基本上由0.3至1.1wt。 %硅,0.4〜1.0wt。 %铁,0.009〜0.25wt。 %铜和任选的少量锰,镁,铬,锌,钛和其他附带的杂质与余量的铝。 在从该组合物制造铝片时,将铝合金连续铸造成中间规格片材产品,并直接冷轧而不进行中间热处理至最终规格。 可选地,最终的规格片产品可以经受已知的回火实践。 使用含铁,硅和含铜的铝合金组合物,制造具有可接受的机械性能的片材产品,用作通用铝板,半刚性铝容器坯料,消费包装容器,切割棒等。 该图示出了制造片材产品的方法步骤。

    HEAT TREATMENT FOR THICK ALUMINUM PLATE
    32.
    发明申请
    HEAT TREATMENT FOR THICK ALUMINUM PLATE 审中-公开
    厚铝板热处理

    公开(公告)号:WO1995024514A1

    公开(公告)日:1995-09-14

    申请号:PCT/US1995002705

    申请日:1995-03-10

    CPC classification number: C22F1/053

    Abstract: A method for the heat treatment of thick 7000 series aluminum alloy products which results in superb corrosion resistance and strength is disclosed. The inventive method consists of processing a 7000 series aluminum alloy to a semi-finished product in the quenched (-W) condition and then aging by: controlled heating to a high elevated temperature (from about 335 degrees to 450 degrees F); holding at this elevated temperature; cooling to a lower elevated temperature (from about 235 degrees to 310 degrees F); holding at this lower elevated temperature; and finally cooling to room temperature. The resulting product has exfoliation and stress corrosion resistance vastly superior to -T6X tempered products at strength levels much greater than conventional -T7X tempered products. The figure is a schematic illustration of the thermal history for prior art aging practices and aging practices in accordance with the present invention.

    Abstract translation: 公开了一种用于热处理厚7000系列铝合金产品的方法,其具有极好的耐腐蚀性和强度。 本发明的方法包括在淬火(-W)条件下将7000系列铝合金加工成半成品,然后通过以下方式老化:控制加热到高的高温(从约335度至450华氏度); 在这个高温下保持; 冷却至较低的升高温度(约235度至310华氏度); 保持在较低的高温; 最后冷却至室温。 所得产品的剥离和抗应力腐蚀性能优于-T6X回火产品,其强度远远高于常规-T7X回火产品。 该图是根据本发明的现有技术的老化实践和老化实践的热历史的示意图。

    ALUMINUM FOIL LAMINATE AND RECYCLING METHOD
    33.
    发明申请
    ALUMINUM FOIL LAMINATE AND RECYCLING METHOD 审中-公开
    铝箔层压板和回收方法

    公开(公告)号:WO1994027818A1

    公开(公告)日:1994-12-08

    申请号:PCT/US1994005838

    申请日:1994-05-24

    Abstract: An aluminum foil laminate (10) comprising an aluminum foil layer (1), an adhesive (3) and a film layer (5) is adapted for recycling in aluminum beverage container recycling streams. The organic content of the aluminum foil laminate is controlled to a maximum of 20 % by weight of the overall weight of the laminate to permit safe recycling. The aluminum foil laminate can be used as a substitute for plastic films or film/paper composites in intimate wrap applications or pouches or enclosures for food and non-food items. The aluminum foil laminate permits printing and/or embossing on the foil component to enhance the product enclosure packaging and improve machine performance during foiling, wrapping, sealing and filling operations.

    Abstract translation: 包括铝箔层(1),粘合剂(3)和膜层(5)的铝箔层压板(10)适于在铝饮料容器再循环流中循环使用。 将铝箔层压板的有机含量控制在最大为层压板总重量的20重量%以允许安全回收。 铝箔层压板可用作塑料薄膜或膜/纸复合材料的替代品,用于密封包装应用或用于食品和非食品的袋或外壳。 铝箔层压板允许在箔​​部件上进行印刷和/或压花以增强产品外壳的包装,并在成型,包装,密封和填充操作期间提高机器性能。

    IMPROVING MECHANICAL PROPERTIES OF ALUMINUM-LITHIUM ALLOYS
    34.
    发明申请
    IMPROVING MECHANICAL PROPERTIES OF ALUMINUM-LITHIUM ALLOYS 审中-公开
    改善铝合金的机械性能

    公开(公告)号:WO1994020646A1

    公开(公告)日:1994-09-15

    申请号:PCT/US1994002532

    申请日:1994-03-09

    CPC classification number: C22F1/04

    Abstract: Strength and ductility for aluminum-lithium alloy wrought product in the transverse direction is improved by subjecting these types of alloys to improved T8 temper practice. The wrought product, after solution heat treating and quenching is subjected to a multiple step stretching sequence prior to aging, the total percent reduction for the multiple step stretching sequence ranging between 1 and 20 percent reduction. In the multiple step stretching sequence, each of the stretching steps may have the same or different amounts of percent reduction to achieve the desired total percent reduction. An aluminum-lithium alloy wrought product subjected to the improved T8 temper practice has increased tensile yield stress and percent elongation in its transverse direction to facilitate commercial application of the product in high strength applications.

    Abstract translation: 通过使这些类型的合金改善T8回火实践,提高了铝 - 锂合金锻造产品在横向上的强度和延展性。 在固化热处理和淬火之后,锻造产品在老化之前经受多步拉伸程序,多步拉伸序列的总减少百分比范围在1%和20%之间。 在多步拉伸序列中,每个拉伸步骤可以具有相同或不同的百分比减少量以实现期望的总百分比降低。 经过改进的T8回火实践的铝锂合金锻造产品具有增加的拉伸屈服应力和其横向方向的百分比伸长率,以促进产品在高强度应用中的商业应用。

    SURFACE INSPECTION METHOD AND APPARATUS
    35.
    发明申请
    SURFACE INSPECTION METHOD AND APPARATUS 审中-公开
    表面检查方法和装置

    公开(公告)号:WO1993002350A1

    公开(公告)日:1993-02-04

    申请号:PCT/US1992005728

    申请日:1992-07-07

    Abstract: An apparatus (10) for inspecting the surface of an object S moving in the direction of travel (23) relative to the apparatus comprises a modular sensing head assembly (11) including a plurality of sensing head modules (12, 13), each of which includes a number of sensing stations (16 - 21). Each sensing station includes a light source (77, 81, 84) for generating a line of light extending across substantially the width of the surface of the object and a plurality of optical detector means for detecting light scattered from the line of light by the surface of the object. The optical detectors are positioned and oriented to receive scattered light scattered along paths lying in detection planes which are perpendicular to each other and perpendicular to the surface of the object. Signal processing electronics are provided to convert the light received by the detectors into analog signals which are multiplexed, converted to digital signals, filtered and then compared to preselected thresholds to determine the existence of any defects in the surface.

    METHOD AND APPARATUS FOR FORMING CAN ENDS
    36.
    发明申请
    METHOD AND APPARATUS FOR FORMING CAN ENDS 审中-公开
    用于形成罐头的方法和装置

    公开(公告)号:WO1992022194A1

    公开(公告)日:1992-12-23

    申请号:PCT/US1992004832

    申请日:1992-06-11

    CPC classification number: B21D51/38

    Abstract: Method and apparatus for forming can ends is disclosed wherein ends are blanked from sheet material and formed in a die in which the completed end is formed and removed from the die at a vertical position below the blanking position (226). Formation and removal of the end beneath the cut line enables better control of the ends after forming. Vacuum is applied (156) to the end (60) underside to positively seat the end against lower die forming elements (72, 58) as the lower elements raise the end to the level of an ejection slot where pressurized air blows the air from between the dies (54, 56). An automatic lubrication circuit for properly lubricating seal members forming pneumatic cushions for resiliently biasing the various die members is also disclosed.

    Abstract translation: 公开了用于形成罐头端部的方法和装置,其中端部从板材冲切并形成在模具中,在模具中,完成的端部在冲切位置(226)下方的垂直位置处形成并从模具移除。 切割线下方的端部的形成和移除能够在成形后更好地控制端部。 当下部元件将端部升高到喷射狭槽的高度时,其中加压空气从空气中吹出空气,将真空端部(156)施加到端部(60)的下侧,以将其端部靠着下模具形成元件(72,58) 模具(54,56)。 还公开了一种自动润滑电路,用于适当地润滑形成用于弹性偏压各种模具构件的气垫的密封构件。

    APPARATUS FOR AND PROCESS OF DIRECT CASTING OF METAL STRIP
    37.
    发明申请
    APPARATUS FOR AND PROCESS OF DIRECT CASTING OF METAL STRIP 审中-公开
    金属条直接铸造的设备和工艺

    公开(公告)号:WO1990010515A1

    公开(公告)日:1990-09-20

    申请号:PCT/US1990001211

    申请日:1990-03-14

    CPC classification number: B22D11/0622 B22D11/064 B22D11/0651

    Abstract: A melt drag metal strip casting system of the type wherein molten metal (20) is delivered from a supply (18) of the molten metal into contact with a grooved chill surface (14) and the chill surface (14) is driven at a predetermined linear rate to quench and withdraw a continuous strip of metal (16). The strip (16) having a bottom surface adhering to the chill surface (14) and an unsolidified top surface as it is withdrawn from the molten metal supply, including a top roll (80) adjustably mounted above the chill surface (14) and spaced therefrom by a distance substantially equal to the thickness of the strip (16) desired with the top roll (80) in contact only with the unsolidified top surface of the strip (16), with the temperature of the top roll (80) surface in contact with the unsolidified top surface of the strip being maintained at a level which will not solidify the top surface of the metal being cast.

    Abstract translation: 一种熔融金属带铸造系统,其中熔融金属(20)从熔融金属的供应源(18)被输送到与沟槽的冷却表面(14)和冷却表面(14)接触,并以预定的方式被驱动 线性速率淬火并取出连续的金属条(16)。 所述条带(16)具有粘附到所述冷却表面(14)的底表面,以及当从所述熔融金属供应源中取出时,所述未固化顶表面包括可调节地安装在所述冷却表面(14)上方的顶辊(80) 其距离基本上等于与顶辊(80)仅与带材(16)的未固化顶表面接触的条带(16)的厚度,顶辊(80)的表面在 与未固化的带材的顶表面接触保持在不凝固被铸造的金属的顶表面的水平。

    METHOD OF AND APPARATUS FOR DIRECT METAL STRIP CASTING
    38.
    发明申请
    METHOD OF AND APPARATUS FOR DIRECT METAL STRIP CASTING 审中-公开
    直接金属条带铸造的方法和装置

    公开(公告)号:WO1990005604A1

    公开(公告)日:1990-05-31

    申请号:PCT/US1989004869

    申请日:1989-11-03

    CPC classification number: B22D11/064

    Abstract: An improved method of and apparatus is disclosed for direct casting of molten metal to form a strip by solidification of the molten metal on a moving chill surface (12) using the vessel having a floor (30), space sidewalls (32, 34), an inlet (20) and an outlet (18) extending between the sidewalls (32, 34) for supplying the molten metal to the chill surface (12) in which the transverse dimension of the outlet may be adjusted during casting to change the width of the strip by central baffle (44) and preferably adjustable baffles (106, 108) to control the flow pattern to provide a substantially uniform flow of metal to the outlet.