Abstract:
A container comprising a propylene, ethylene, 1-hexene terpolymer wherein in the terpolymer: (i) the content of ethylene derived units ranges from 0.2 wt% to 1.0 wt%; (ii) the content of 1-hexene derived units ranges from 3.5 wt% to 5.5 wt%; (iii) the content of ethylene derived units fulfills the following equation (I): C2
Abstract:
Propylene polymer compositions comprising: A) from 70 wt% to 95 wt%, of a random copolymer of propylene with ethylene, containing from 1.5 wt% to 4.5 wt%, of ethylene derived units, having a content of fraction insoluble in xylene at 25°C of not less than 93%; B) from 5 wt% to 35 wt%, of a copolymer of propylene with ethylene, containing from 7.0 wt% to 17.0 wt % of ethylene derived units; the sum A+B being 100; wherein the melt flow rate, MFR.(Melt Flow Rate according to ASTM 1238, condition L, i.e. 230°C and 2.16 kg load) ranges from 40 g/10 min and 130 g /10 min; and wherein the relation (I) is fulfilled: 10
Abstract:
Automotive interior element comprising a polypropylene composition comprising (percent by weight): A) from 60% to 90% of a propylene homopolymer having: i) a polydispersity Index (P.I.) value of from 3.5 to 10.0; ii) a fraction insoluble in xylene at 25 °C, higher than 90 %; and iii) a MFR L (Melt Flow Rate according to ISO 1133, condition L, i.e. 230°C and 2.16 kg load) from 50 to 200 g/10 min; B) from 10% to 40%; of a copolymer of propylene with from 30% to 60% of ethylene derived units; the composition having an intrinsic viscosity of the fraction soluble in xylene at 25 °C comprised between 2.5 and 4.0 dl/g; a MFR L (Melt Flow Rate according to ISO 1133, condition L, i.e. 230°C and 2.16 kg load) from 15 to 100 g/10 min and all the three values of carbon emission measured according to VDA 227 (C-emission) are lower than 30.0 μgC/g; wherein the values of carbon emission are measured in the ex reactor propylene composition.
Abstract:
A process for the production of a corona-treated polyolefin film comprising the gas-phase polymerization of one or more α-olefins in the presence of a polymerization catalyst and an antistatic agent having a molecular weight higher than 500, said antistatic agent being fed at any stage of the polymerization process in an amount from 30 to 500 ppm weight based on the weight of the produced polyolefin.
Abstract:
A propylene composition comprising (percent by weight): A) 70%-95%, of a propylene homopolymer having a Polydispersity Index (P.I.) value of from 4.6 to 10, a fraction insoluble in xylene at 25°C, higher than 90 %, and MFR L (Melt Flow Rate according to ISO 1133, condition L, i.e. 230°C and 2.16 kg load) from 100 to 250 g/10 min; B) 5%-30%, of a copolymer of propylene containing from 36% to 44% of ethylene derived units; the composition having an intrinsic viscosity of the fraction soluble in xylene at 25°C comprised between 3 and 5 dl/g.
Abstract:
A masterbatch composition comprising: 70-90 %wt of a component (A) being a propylene homopolymer or copolymer of propylene with ethylene or C 4 -C 10 alpha olefins, having a MFR A according to ISO 1133 (230°C/2.16 Kg) ranging from 15 to 70 g/10 min; and 10-30 %wt of a component B) being a propylene-ethylene copolymer comprising 25-45 %wt of ethylene derived units and having a value of the intrinsic viscosity [η] of the fraction soluble in xylene at room temperature ranging from 5 to 9 dl/g, said masterbatch composition having a total MFR higher than 4 g/10 min, and a value of the fiexural modulus measured according to ISO method 178 ranging from 950 to 2000 MPa.
Abstract:
A polyolefϊn composition comprising, in percentage by weight based on the weight sum of the components (al), (a2) and (b): al) 16-78 % of a propylene homopolymer or copolymer containing at most 15% of ethylene and/or C4-C10 α-olefm(s), having an isotactic index over 80%; and a2) 6-44% of a copolymer of ethylene with one or more C 4 -C 10 α-olefm(s) containing from 10 to 40%, preferably from 15 to 35%,of said C 4 -C 10 α-olefm(s); b) 3-70% of a butene-1 (co)polymer having: - a content of butene-1 derived units of 80% wt or more, - flexural modulus (MEF) of 60 MPa or less. The polyolefϊn composition exhibits good impact resistance, excellent whitening resistance and relatively low stiffness combined with good optical properties suitable for injection and blow molding, thermoforming and film application.
Abstract:
A nucleated propylene polymer composition comprising: A) from 77 wt% to 91 wt%, of a propylene homopolymer having a fraction insoluble in xylene at 25 °C higher than 95 %; B) from 9 wt % to 23 wt%, of a copolymer of propylene with from 28.0 wt% to 42.0 wt% of ethylene derived units; the composition having an intrinsic viscosity of the fraction soluble in xylene at 25 °C comprised between 1.0 dl/g and 1.9 dl/g, a fraction soluble in xylene at 25 °C comprised between 9.0 wt% and 21.0 wt%, a total melt flow rate (Melt Flow Rate according to ISO 1133, condition L, i.e. 230°C and 2.16 kg load) comprised between 1.5 and 5 g/10 min and the value of the relation (I): 22.5+0.2*MFR-1.2*Xs+0.2*IV is higher than 5.9; wherein MFR is the melt flow rate of the nucleated composition (Melt Flow Rate according to ISO 1133, condition L, i.e. 230°C and 2.16 kg load); IV is the intrinsic viscosity of the fraction soluble in xylene at 25 °C; and Xs is the fraction soluble in xylene at 25°C; wherein the amount of A+B is equal to 100 wt% and wherein the nucleated agent is selected from the group consisting of aromatic or aliphatic carboxylic acids, aromatic metal phosphates, sorbitol derivatives and talc.
Abstract:
A polypropylene composition comprising: A) from 50 wt% to 90 wt%; of a propylene homopolymer; B) from 10 wt% to 50wt%; of a copolymer of propylene with from 30.0 wt% to 70.0wt%, of ethylene derived units; the sum of the amount of component A) and B) being 100; the composition having: i) an intrinsic viscosity of the fraction soluble in xylene at 25 °C comprised between 2.2 and 4.0 dl/g; ii) a MFR L (Melt Flow Rate according to ISO 1133, condition L, i.e. 230°C and 2.16 kg load) from 0.5 to 100 g/10 min; iii) a xylene soluble fraction ranging from 20 wt% to 50 wt%; the polypropylene composition being obtained by a two steps polymerization process wherein the catalyst system contains bismuth.
Abstract:
A polyolefin composition comprising: A) from 19 wt% to 50 wt% of a propylene ethylene copolymer having an ethylene derived units content ranging from 1.5 wt% to 6.0 wt% B) from 50 wt% to 81 wt% of a propylene ethylene 1-butene terpolymer having an ethylene derived units content ranging from 1.5 wt% and 6.0 wt% and 1-butene derived units content of between 4.8 wt% and 12.4 wt%; the sum of the amount of component A) and B) being 100.