43.
    发明专利
    未知

    公开(公告)号:DE3733630A1

    公开(公告)日:1989-04-13

    申请号:DE3733630

    申请日:1987-10-05

    Applicant: BASF AG

    Abstract: Wood materials with reduced subsequent release of formaldehyde can advantageously be produced by mixing lignocellulose-containing particles, for example wood chippings, with a curable binder based on curable aminoplastic condensates and subsequently pressing the mixture with heating, a mixture A containing a water-compatible agent for binding formaldehyde to the particles being applied or mixed with the particles before the particles are mixed with the curable binder, to give good resin reactivity, high strength and good swelling values if the mixture A is an aqueous solution having a pH of from 3.0 to 6.5 which contains a) organic acids which do not attack wood, or only do so to an insignificant extent, in an amount of greater than 15 % by weight, based on the solids content of the solution, preferably mixtures of aliphatic carboxylic acids having 4 to 10 carbon atoms, and b) a formaldehyde-binding, nitrogen-containing compound, in particular urea.

    44.
    发明专利
    未知

    公开(公告)号:DK554088A

    公开(公告)日:1989-04-06

    申请号:DK554088

    申请日:1988-10-04

    Applicant: BASF AG

    Abstract: Wood materials with reduced subsequent release of formaldehyde can advantageously be produced by mixing lignocellulose-containing particles, for example wood chippings, with a curable binder based on curable aminoplastic condensates and subsequently pressing the mixture with heating, a mixture A containing a water-compatible agent for binding formaldehyde to the particles being applied or mixed with the particles before the particles are mixed with the curable binder, to give good resin reactivity, high strength and good swelling values if the mixture A is an aqueous solution having a pH of from 3.0 to 6.5 which contains a) organic acids which do not attack wood, or only do so to an insignificant extent, in an amount of greater than 15 % by weight, based on the solids content of the solution, preferably mixtures of aliphatic carboxylic acids having 4 to 10 carbon atoms, and b) a formaldehyde-binding, nitrogen-containing compound, in particular urea.

    45.
    发明专利
    未知

    公开(公告)号:NO884401D0

    公开(公告)日:1988-10-04

    申请号:NO884401

    申请日:1988-10-04

    Applicant: BASF AG

    Abstract: Wood materials with reduced subsequent release of formaldehyde can advantageously be produced by mixing lignocellulose-containing particles, for example wood chippings, with a curable binder based on curable aminoplastic condensates and subsequently pressing the mixture with heating, a mixture A containing a water-compatible agent for binding formaldehyde to the particles being applied or mixed with the particles before the particles are mixed with the curable binder, to give good resin reactivity, high strength and good swelling values if the mixture A is an aqueous solution having a pH of from 3.0 to 6.5 which contains a) organic acids which do not attack wood, or only do so to an insignificant extent, in an amount of greater than 15 % by weight, based on the solids content of the solution, preferably mixtures of aliphatic carboxylic acids having 4 to 10 carbon atoms, and b) a formaldehyde-binding, nitrogen-containing compound, in particular urea.

    WOOD ADHESIVE
    48.
    发明专利

    公开(公告)号:CA972491A

    公开(公告)日:1975-08-05

    申请号:CA111265

    申请日:1971-04-23

    Applicant: BASF AG

    Abstract: Procedure for obtaining wood glues, which per mole of melamine, or a mixture of at least 15 mole% melamine and up to 85 mole% urea, contain 1.7 to 3.0 moles of formaldehyde and 0.05 mol to 0.2 mol of a phenol, characterized in that in each case 1 mol of melamine and/or urea and from 1.5 to 2.5 mol of formaldehyde are condensed in a known manner in aqueous solution until a compatibility with water of 0.5 to 10 and the condensate is reacted at a ph of 7.5 to 10 and between 45 and 100º c, in each case with 0.05 to 0.2 mol of a phenol, if necessary, with up to 0.5 mol of formaldehyde and, if necessary, with up to 0.5 mol of melamine, until the aqueous solution reaches a viscosity of 300 to 2000 cp, measured with a solids content of 63% and 20ºc. (Machine-translation by Google Translate, not legally binding)

Patent Agency Ranking