公开(公告)号:DE3733630A1
公开(公告)日:1989-04-13
申请号:DE3733630
申请日:1987-10-05
Applicant: BASF AG
Inventor: SCHMIDT-HELLERAU CHRISTOF , MAYER JOHANN DR
Abstract: Wood materials with reduced subsequent release of formaldehyde can advantageously be produced by mixing lignocellulose-containing particles, for example wood chippings, with a curable binder based on curable aminoplastic condensates and subsequently pressing the mixture with heating, a mixture A containing a water-compatible agent for binding formaldehyde to the particles being applied or mixed with the particles before the particles are mixed with the curable binder, to give good resin reactivity, high strength and good swelling values if the mixture A is an aqueous solution having a pH of from 3.0 to 6.5 which contains a) organic acids which do not attack wood, or only do so to an insignificant extent, in an amount of greater than 15 % by weight, based on the solids content of the solution, preferably mixtures of aliphatic carboxylic acids having 4 to 10 carbon atoms, and b) a formaldehyde-binding, nitrogen-containing compound, in particular urea.
-
公开(公告)号:DE2243857A1
公开(公告)日:1974-04-04
申请号:DE2243857
申请日:1972-09-07
Applicant: BASF AG
Inventor: ERHARDT KLAUS DR , PETERSEN HARRO DR , TEUTHER WOLFGANG DR , WITTMANN OTTO , BRUNNMUELLER FRITZ DR , GRABOWSKY OTTO DR , MAYER JOHANN DR , LENZ JOHANN
Abstract: A urea-formaldehyde resin is formed by (a) reacting formaldehyde and urea of an initial molar ratio of >=3, in an aqs. soln., pH 3, until 1% of the urea has reacted to form urone gps., or by reacting as above during a time t = 10pH-2 (between 90-100 degrees C), (b) adding urea to the obtd. prod., at pH=3, such that the polar ratio HCHO:urea is 2-2.75 and condensing until the aqs. soln. of the condensate is no longer indefinitely dilutable in water at room temp., and (c) concentrating or evaporating the soln. formed to give a prod. contg. HCHO and urea in a molar ratio 1-2.75. The resin is used partic. in the mfr. of plywood and has a reduced tendency to evolve free HCHO.
-
公开(公告)号:GR71009B
公开(公告)日:1983-03-31
申请号:GR800163375
申请日:1980-11-15
Applicant: BASF AG
Inventor: SCHATZ HERMANN , DUDECK CHRISTIAN DR , DIEM HANS , MAYER JOHANN DR , SCHMIDT-HELLERAV CHRISTOF
IPC: C08G14/10 , C08L61/34 , C09J161/34
-
公开(公告)号:DE2860778D1
公开(公告)日:1981-09-24
申请号:DE2860778
申请日:1978-09-04
Applicant: BASF AG
Inventor: GRASER MARTIN , HANN ERNST WILHELM , HENKEL HELMUT , MAYER JOHANN DR , SCHMIDT-HELLERAU CHRISTOF
-
公开(公告)号:DE2745809A1
公开(公告)日:1979-04-26
申请号:DE2745809
申请日:1977-10-12
Applicant: BASF AG
Inventor: LEHMANN GERHARD DR , MAYER JOHANN DR , SCHMIDT-HELLERRAU CHRISTOF
IPC: C08G12/12 , C08G12/40 , C09J161/24 , C08L61/24 , C09J3/16
Abstract: A urea-HCHO resin soln. with a molar ratio of HCHO urea of is not 1.2:1 and a viscosity of 500-1500 mPas at 65% solids and 20 degrees C, is brought to a pH of is not 7.5, and a temp. of is not 40 degrees C, and mixed with stirring, with sulphite waste liquor, the amt. of the liquor is 1-6 wt % solids w.r.t. the resin soln. The soln. is a wood glue. It has improved pre-bonding strength, and the pre-glued wood parts can be transported without sepg.
-
公开(公告)号:CH598294A5
公开(公告)日:1978-04-28
申请号:CH916174
申请日:1974-07-04
Applicant: BASF AG
Inventor: EISELE WOLFGANG DR , PETERSEN HARRO DR , MAYER JOHANN DR , WITTMANN OTTO
IPC: C08G12/00 , B27N3/02 , C08G12/12 , C09J161/20 , C09J161/24 , C09J3/16
Abstract: Condensates containing urea and formaldehyde in a molar ratio of from 1:2.5 to 1:4.5 are converted into wood glue by allowing the viscosity to increase at a pH of from 1 to 3 and at only slightly elevated temperature and then adding urea at a pH of 7 to 9.
-
公开(公告)号:DE2241995A1
公开(公告)日:1974-04-04
申请号:DE2241995
申请日:1972-08-26
Applicant: BASF AG
Inventor: BRUNNMUELLER FRITZ DR , SCHATZ HERMANN , MAYER JOHANN DR , GRABOWSKY OTTO DR
Abstract: In parent patent, aminoplast solns. for use as adhesives were prepd. continuously by condensing cpds. capable of forming aminoplants and HCHO in the presence of a catalytic mixt. consisting of ammonia or an amine, and an acid or acid salt, in homogeneous aq. soln. at boiling temp. in >=3 successive reactors. Here, the molar ratio of HCHO to aminoplast precursor in the second reactor and the following reactors is maintained at 1.6-2.6:1, the pH being 4.0-6.0, pref. 5.0-6.0. Lower residence time is needed for a given degree of condensation. Less corrosion of the metallic surfaces of the appts. is caused and the aminoplast solns. have better storage stability.
-
公开(公告)号:AT81050T
公开(公告)日:1992-10-15
申请号:AT88105373
申请日:1988-04-02
Applicant: BASF AG
Inventor: NEUMANN CLAUS DR , MAYER JOHANN DR , KARAU DIETER , NEUNER SEPP
-
公开(公告)号:DE3712347A1
公开(公告)日:1988-10-20
申请号:DE3712347
申请日:1987-04-11
Applicant: BASF AG
Inventor: NEUMANN CLAUS DR , MAYER JOHANN DR , KARAU DIETER , NEUNER SEPP
-
公开(公告)号:DE3466553D1
公开(公告)日:1987-11-05
申请号:DE3466553
申请日:1984-12-17
Applicant: BASF AG
Inventor: MAYER JOHANN DR , SCHMIDT-HELLERAU CHRISTOF
-
-
-
-
-
-
-
-
-