公开(公告)号:JPH04357186A
公开(公告)日:1992-12-10
申请号:JP15752191
申请日:1991-05-31
Applicant: NISSHA PRINTING
Inventor: SHIMAMOTO KOICHIRO
Abstract: PURPOSE:To obtain a colored metal oxide dyed to various deep and brilliant colors. CONSTITUTION:A glass substrate is spray-coated with a hydrolyzate produced by hydrolyzing aluminum isopropylate with acetic acid and the coating layer is dried and baked to obtain a glass substrate having an alumina film. The substrate is immersed in a warm aqueous solution of p-sulfophenylazo-5- carboxyl-1-(p-sulfophenyl)-3-pyrazolone sodium salt, washed with water and dried. The dried substrate is immersed in a warm aqueous solution of diamond green, washed with water and dried to obtain a glass substrate having a beautiful transparent green alumina film of a high color purity.
-
公开(公告)号:JPH04179586A
公开(公告)日:1992-06-26
申请号:JP30777590
申请日:1990-11-13
Applicant: NISSHA PRINTING
Inventor: SHIMAMOTO KOICHIRO , KITANO HISAO , NISHIMURA KENICHI
Abstract: PURPOSE:To make possible the manufacture of large amounts of various synthetic resin molded products with warmth-giving appearance, massive looks, a feeling of high quality and an impression of pliability as outstanding features by first providing a soluble layer consisting mainly of soluble resin and fibrous organic filler on a base sheet with mold lubrication properties, and further providing a patterned layer. CONSTITUTION:First, a soluble layer consisting mainly of soluble resin and organic filler is provided on a base sheet with mold lubrication properties, and then a patterned layer is provided for the manufacture of a transfer material. A coating paper on which mold lubricants such as polyethylene terephthalate and silicone are applied, is used as the base sheet. Soluble resins are used for a soluble layer based on soluble resin and fibrous organic filler are organic solvent-soluble resins such as ester (metha)acrylate resin and alcohol or water soluble resins such as polyvinyl pyrrolidone resin. If these resins are used, their molded products are hardly damaged by alcohol or water their mixture which is used when the soluble layer is removed. Therefore, such resins can be used advantageously for most applications.
-
公开(公告)号:JPH04139270A
公开(公告)日:1992-05-13
申请号:JP26202990
申请日:1990-09-29
Applicant: NISSHA PRINTING
Inventor: SHIMAMOTO KOICHIRO , INOUE HIROKO , KITANO HISAO , YAMAMOTO KUNITOSHI , FUKUSHIMA YUTAKA
IPC: C09D11/02 , C09D11/033 , C09D11/037 , C09D11/10 , C09D11/101 , C09D11/103 , C09D11/104 , C09D11/106
Abstract: PURPOSE:To obtain the subject ink useful for signboards, display, etc., and capable of keeping the advertisement effect over a long period by compounding a specific azo pigment and a specific binder resin at a specific ratio. CONSTITUTION:The objective ink can be produced by compounding (a) one or more kinds of azo pigment selected from azo pigment having N-substituted sulfamoyl group and expressed by formula I (A and B are OH, OCH3, SH, etc.; X is F, Cl or Br; D is H, CH3, etc.) and azo compound nickel complex pigment of formula II, formula III (E and F are H, OH, etc.; G is H, F, Cl, etc.; J is H, CH3, etc.), etc., and (b) a binder resin having ester bond group and selected from modified phenolic resin, modified alkyd resin, etc., at a weight ratio (a/b) of 0.01-2.00.
-
公开(公告)号:JPH04139269A
公开(公告)日:1992-05-13
申请号:JP26202890
申请日:1990-09-29
Applicant: NISSHA PRINTING
Inventor: SHIMAMOTO KOICHIRO , INOUE HIROKO , KITANO HISAO , YAMAMOTO KUNITOSHI , FUKUSHIMA YUTAKA
IPC: B41M3/18 , C09D11/02 , C09D11/033 , C09D11/037 , C09D11/10 , C09D11/101 , C09D11/103 , C09D11/104 , C09D11/106
Abstract: PURPOSE:To obtain the subject sheet having excellent light-resistance and weather resistance by printing a sheet substrate with an ink composed of a specific pigment and a binder resin having ester bond group and forming a coating film having a specific thickness on the substrate. CONSTITUTION:The objective sheet having excellent long-term storage stability can be produced by printing a sheet substrate (preferably polyacrylate sheet, polyester sheet, etc.) with an ink containing (A) pigments consisting of (i) an azo pigment and/or an azo compound nickel complex pigment having N- substituted sulfamoyl group as a yellow ink pigment, (ii) a quinacridone pigment as a magenta ink pigment and (iii) a phthalocyanine pigment as a cyan ink pigment and (B) a binder resin having an ester bond group at a weight ratio (A:B) of 0.01-2.00. The thickness of the coating layer on the sheet is 0.01-30mum.
-
公开(公告)号:JPH0263827A
公开(公告)日:1990-03-05
申请号:JP21755788
申请日:1988-08-31
Applicant: NISSHA PRINTING
Inventor: SHIMAMOTO KOICHIRO , KITANO HISAO
Abstract: PURPOSE:To regulate divergence of aroma in accordance with temperature by utilizing hydrophilic resin for at least one of an aroma-retaining layer and a resin binder forming a coating layer. CONSTITUTION:In an aroma-retaining base material wherein both an aroma- retaining layer having an aroma-retaining material and a coating layer for covering the aroma-retaining layer are formed on a base material, at least one of the aroma-retaining layer and a resin binder forming the coating layer is made of hydrophilic resin. Hydrophilic resin is selected from a cellulose derivative soluble in an organic solvent or a synthetic high polymer. Therein moisture is allowed to act on both the aroma-retaining layer contg. the aroma- retaining material and the coating layer; thereby the physical properties of the high polymer such as crystallinity in the aroma-retaining layer and the coating layer, density, thickness and the state of the surfaces or the relative physical properties between the respective resin layers are fluctuated in accordance with humidity thereof. Thereby diffusibility and permeability of aroma are fluctuated and divergence of aroma from the aroma-retaining material can be regulated in accordance with it.
-
公开(公告)号:JPH01249171A
公开(公告)日:1989-10-04
申请号:JP7979488
申请日:1988-03-30
Applicant: NISSHA PRINTING
Inventor: SHIMAMOTO KOICHIRO , MEN RIYOUMEI
Abstract: PURPOSE:To obtain the pattern of an inorg. oxide film on a base body having low heat resistance by coating the hydrate of an inorg. oxide on the base body, then subjecting the same to laser irradiation to effect a dehydration reaction. CONSTITUTION:The sol of the alumina hydrate is coated by a roll coater on a glass plate and is dried for 15 minutes at about 60 deg.C. While this coating is heated to about 150 deg.C, the coating is irradiated by the laser beam from a YAG laser device along, the prescribed circumferential pattern to effect the dehydration reaction. The sol of the non-irradiated part is cleaned and removed by a dilute acid and the glass plate is heated at about 450 deg.C to further progress the dehydration reaction. The patterned inorg. oxide film is thereby easily obtd. Formation of the inorg. oxide film on a film having low heat resistance is possible as well by coating the hydrate sol of the inorg. oxide having 90:5:5 atomic ratio of Al, Ti and Si on a polyether ketone film and causing the coating to be irradiated by the laser beam from a CO2 laser.
-
公开(公告)号:JPH01192746A
公开(公告)日:1989-08-02
申请号:JP1821588
申请日:1988-01-28
Applicant: NISSHA PRINTING
Inventor: SHIMAMOTO KOICHIRO , YOSHIKAWA HIROKO , NAKAHATA TOKIKO , INOUE HIROKO , FUJITA JUNKO
Abstract: PURPOSE:To obtain colored glass having excellent transparency and physical properties, capable of showing various colors, by adsorbing and/or sticking a metal (ion) to a porous film consisting essentially of alumina formed on plate glass. CONSTITUTION:Alumina aqueous sol is obtained or aqueous sol (a) consisting essentially of alumina is prepared by blending the alumina aqueous sol with at least one selected from silica aqueous sol, titania aqueous sol, zirconia aqueous sol and magnesia aqueous sol in the atomic ratio of 199-9:1. A saturated solution of at least one metallic compound selected from V, Cr, Mn, Fe, Co, Ni, Cu, W, Mo, rare earth metal and platinum element is mixed with 1-40wt.% binder (e.g., PVA) solution having 5-50wt.% concentration to give a coating solution (b). Then a glass plate is coated with the component (a), dried at 30-120 deg.C for 1-30 minutes, calcined at 350-550 deg.C for 0.5-10 hours to form a porous film having 0.1-10mu thickness on the glass plate. The porous film is then coated with the component (b), dried at room temperature, then at 40-100 deg.C for 1-20 minutes and heated at 100-550 deg.C for 1-2 hours to adsorb or to stick a metal (ion) to the porous film.
-
公开(公告)号:JPH01171633A
公开(公告)日:1989-07-06
申请号:JP33060387
申请日:1987-12-25
Applicant: NISSHA PRINTING
Inventor: SHIMAMOTO KOICHIRO , NAKAHATA TOKIKO
IPC: B01F17/22 , B01J13/00 , C01B33/145 , C01F7/02 , C01G23/047 , C01G25/02 , C09K3/00
Abstract: PURPOSE:To stabilize the viscosity of sol, by compounding acid amide of specified formula with one or more kinds of aq. sol selected among alumina, silica, titania and zirconia. CONSTITUTION:One or more kinds of the aq. sol selected among alumina, silica, titania and zirconia are incorporated with the acid amide of formula I (where, R1, R2 and R3 are hydrogen atom., amino group, substd. amino group, lower alkyl group, substd. lower alkyl group and any two groups of R1, R2 and R3 can form cyclic structure through any of oxygen atom., alkylene group, carbonyl group, acylamino group and carboxyl group in the terminal of group) to prepare an aq. sol having stabilized viscosity. The aq. sol preferably contains one or more of alcohol, polyol and Broensted acid.
-
公开(公告)号:JPS62234245A
公开(公告)日:1987-10-14
申请号:JP7746886
申请日:1986-04-02
Applicant: NISSHA PRINTING
Inventor: NAKAMURA YUZO , SHIMAMOTO KOICHIRO , OKAZAKI AKIRA , KITANO HISAO
Abstract: PURPOSE:To obtain substantial surface hardness, to eliminate the deterioration in light transmittance and to improve productivity by providing a curable resin layer on the surface of an optical disk substrate. CONSTITUTION:An aluminum film is formed as a reflective layer 2 by vapor deposition on the substrate 1 formed of an acrylic or polycarbonate resin. A rear surface protective layer 3 is formed on the reflective layer 2. The curable resin layer 4 is formed by a transfer printing method, etc., on the surface to be irradiated with laser light of the substrate 1. The surface of the substrate is thereby hardened to substantial hardness and the deterioration in the light transmittance is eliminated; in addition, the productivity is improved.
-
公开(公告)号:JPH08241160A
公开(公告)日:1996-09-17
申请号:JP7093595
申请日:1995-03-03
Applicant: NISSHA PRINTING
Inventor: SHIMAMOTO KOICHIRO , NAKAMURA KAZUO , OKUMURA TADASHI
Abstract: PURPOSE: To provide the transparent touch panel which does not spoil linearity. CONSTITUTION: A lower electrode which has a conductive film and a couple of parallel bus bars 3 formed on the top surface of a transparent insulating base material and an upper electrode which has a transparent conductive film and a couple of parallel bus bars 7 formed on a transparent flexible insulating base material are put on over the other by interposing spacers between the transparent films so that the direction between the bus bars 3 of the lower electrode and the direction between the bus bars 7 of the upper electrode cross each other at right angles, and the peripheral parts are adhered together with an adhesion layer 10 to constitute the analog resistance type transparent touch panel, which is provided with an insulating layer 16 which is discontinuous at least at the inside end part in a frame area which is present between the upper and lower electrodes adjacently to the adhesion layer 10.
-
-
-
-
-
-
-
-
-