Primer applying method
    43.
    发明申请
    Primer applying method 审中-公开
    引物施用方法

    公开(公告)号:US20030064155A1

    公开(公告)日:2003-04-03

    申请号:US10261360

    申请日:2002-09-30

    Inventor: Takeshi Yamane

    CPC classification number: B05D3/0245 B05D3/0227 B05D3/0254 B05D2202/10

    Abstract: To provide a method of applying a primer in which film thickness of the primer is maintained constant to prevent pinholes, and a furnace is shortened as well. In a method of applying a primer to a back plate for a friction member, prior to applying the primer, the back plate is heated in advance. The temperature at which the back plate is preheated is set to be higher or equal to a temperature at which primer resin starts hardening within a range that the primer layer after hardening does not lose smoothness. When the primer is applied to the back plate preheated, the primer is immediately dried, and is hardened successively. At the preheating, even if the temperature is rapidly increased, a solvent for the primer does not bump, so that uniform film can be formed.

    Abstract translation: 为了提供一种涂布底漆保持恒定的底漆的方法,以防止针孔,并且炉子也缩短。 在将底漆施加到摩擦构件的背板的方法中,在涂布底漆之前,预先加热背板。 将背板预热的温度设定为高于或等于底漆树脂开始硬化的温度在硬化后的底漆层不失去平滑度的范围内。 当将底漆施加到预热的背板上时,将底漆立即干燥并依次硬化。 在预热时,即使温度迅速升高,底漆的溶剂也不会发生碰撞,从而可以形成均匀的膜。

    AMBIENT CURE PAINTING METHOD WITH WATERBORNE BASECOAT
    50.
    发明申请
    AMBIENT CURE PAINTING METHOD WITH WATERBORNE BASECOAT 审中-公开
    具有水柱基础的环境固化涂漆方法

    公开(公告)号:US20110014388A1

    公开(公告)日:2011-01-20

    申请号:US12836055

    申请日:2010-07-14

    Abstract: Methods and associated compositions are described for applying onto a substrate a cured coating that includes at least one layer of a water-borne basecoat and one layer of clearcoat and that requires a maximum total curing time of less than about 45 minutes. Further described are methods and associated compositions for applying onto a substrate a cured coating that includes at least one layer of primer, at least one layer of a water-borne basecoat and at least one layer of clearcoat and that requires a maximum total curing time of less than about 65 minutes.

    Abstract translation: 描述的方法和相关组合物用于将包含至少一层水性底涂层和一层透明涂层的固化涂层施加到基底上,并且需要小于约45分钟的最大总固化时间。 还描述了用于将固化涂层施用到固化涂层上的方法和相关组合物,所述固化涂层包括至少一层底漆,至少一层水性底涂层和至少一层透明涂层,并且需要最大总固化时间 少于约65分钟。