公开(公告)号:KR1020140043521A
公开(公告)日:2014-04-10
申请号:KR1020120105090
申请日:2012-09-21
Applicant: 현대자동차주식회사
IPC: D06M15/507 , D06M101/04
CPC classification number: D06M15/507 , D06M2101/04 , D10B2201/01 , D10B2201/06 , D10B2505/12
Abstract: The present invention relates to a high density natural fiber containing polylactic acid and, more specifically, to a high density natural fiber containing polylactic acid which can improve processability through the increase of density by infiltrating, into the surface of the natural fiber, resin melt containing a polylactic acid resin and a coupling agent; and which can be utilized in various industrial material fields as well as vehicle components by using the high density natural fiber as a polylactic acid natural fiber composite material. [Reference numerals] (AA) Natural fabric; (BB) Molten resin; (CC) Cooling unit; (DD) Cutter
Abstract translation: 本发明涉及含有聚乳酸的高密度天然纤维,更具体地说,涉及一种含有聚乳酸的高密度天然纤维,其通过渗透密度增加而提高加工性,进入天然纤维表面,含有 聚乳酸树脂和偶联剂; 通过使用高密度天然纤维作为聚乳酸天然纤维复合材料,可以在各种工业材料领域以及车辆部件中使用。 (附图标记)(AA)天然织物; (BB)熔融树脂; (CC)冷却单元; (DD)切割机
-
公开(公告)号:KR101261917B1
公开(公告)日:2013-05-08
申请号:KR1020110036868
申请日:2011-04-20
Applicant: 현대자동차주식회사
Abstract: 본발명은 NaNO, KHPO, Mg Clㆍ6HO, NaCO, CaCl, 에틸렌다이아민테트라아세트산, 시트르산및 NaSiOㆍ9HO 또는구연산제2철을포함하는미세조류배양용배지에관한것이다. 본발명의배지에의해전분고함량의미세조류의제조가가능해져저가바이오소재원료를확보할수 있게됨으로써바이오소재저가화가가능하게되며, 결과적으로기존의석유계기반의폴리프로필렌계소재를바이오매스유래소재로대체하여자동차내외장재의소재로적용할수 있으므로, 고유가환경에서석유화합물의의존도를낮출수 있고, 내외장재제조단가도대폭절감할수 있다.
-
公开(公告)号:KR101241014B1
公开(公告)日:2013-03-11
申请号:KR1020110076017
申请日:2011-07-29
Applicant: 현대자동차주식회사 , 한국기술교육대학교 산학협력단
CPC classification number: C08J3/005 , C08J5/18 , C08J2367/04 , C08L67/04 , C08L2205/02
Abstract: 본 발명은 폴리유산 필름의 제조 방법에 관한 것으로, 더 구체적으로는 용매의 끓는점(boiling point)에 따라 용액캐스팅 법에 의한 스테레오 컴플렉스 결정 형성율을 극대화시킬 수 있는 폴리유산 필름을 제공할 수 있는 스테레오컴플렉스 결정을 포함하는 폴리유산의 제조방법에 관한 것이다.
-
公开(公告)号:KR1020130008104A
公开(公告)日:2013-01-22
申请号:KR1020110062513
申请日:2011-06-27
Applicant: 현대자동차주식회사
CPC classification number: Y02P20/544 , C08L67/04 , B29B7/00 , B60R13/00 , C08G63/08 , C08J5/00 , C08L2205/025
Abstract: PURPOSE: A manufacturing method of polylactic acid material with high degree of crystallinity is provided to reduce amount of D form polylactic acid. CONSTITUTION: A manufacturing method of polylactic acid material comprises the following steps: manufacturing stereo complex crystals by mixing D form and L form polylactic acids; mixing the added mixture after adding the stereo complex crystals to the D form and L form polylactic acids; and heating and holding the mixed stereo complex crystal-containing polylactic acid at 150-230 deg. Celsius. The D form and L form polylactic acids are respectively having the weight-average molecular weight of 30,000-150,000 g/mol. [Reference numerals] (AA) Manufacturing stereo complex crystal particles; (BB) Mixing the stereo complex particles and polylactic acid; (CC) Forming stereo complex particle dispersed polylactic acid; (DD) Nanoparticles: manufacturing supercritical water particles, microparticles: pulverization after blending, and fiber particles: melt spinning and others; (EE) Blending temperature condition: 180-210°C; (FF) Forming temperature condition: 180-210°C
Abstract translation: 目的:提供具有高结晶度的聚乳酸材料的制造方法以减少D型聚乳酸的量。 构成:聚乳酸材料的制造方法包括以下步骤:通过混合D型和L型聚乳酸制造立体复合晶体; 在将立体络合物晶体加入到D型中后,混合加入的混合物,L形成聚乳酸; 并加热并保持在150-230度的混合立体络合物含晶聚乳酸。 摄氏度。 D型和L型聚乳酸的重均分子量分别为30,000-150,000g / mol。 (附图标记)(AA)制造立体复合晶体颗粒; (BB)混合立体复合颗粒和聚乳酸; (CC)形成立体复合颗粒分散聚乳酸; (DD)纳米颗粒:制造超临界水颗粒,微粒:混合后粉碎,纤维颗粒:熔融纺丝等; (EE)混合温度条件:180-210℃; (FF)成型温度条件:180-210℃
-
公开(公告)号:KR1020110116889A
公开(公告)日:2011-10-26
申请号:KR1020100036559
申请日:2010-04-20
Applicant: 현대자동차주식회사
Abstract: 본 발명은 D 타입 유산의 제조방법에 관한 것으로서, 더욱 상세하게는 쌀 도정 과정에서 발생하는 쌀겨 및 쌀 분쇄물을 알파아밀라제(α-amylase)와 아밀로글루코시다아제를 이용하여 당화시킨 후, 이를 스포로락토바실러스 이누리너스 (
Sporolactobacillus
Inulinus )미생물에 의해 발효시킴으로서 D 타입 유산을 제조하는 방법에 관한 것이다. 본 발명에 의하면 국내외에서 생산되고 있는 쌀 도정 부산물 자원의 부가가치를 높일 수 있으며, 제조된 D 타입 유산은 자동차 내외장용 식물계 소재로서 유망한 스테레오 컴플렉스 폴리유산를 제조하기 위한 D타입 폴리유산의 원료 등으로 유용하게 적용할 수 있다.-
公开(公告)号:KR1020110116888A
公开(公告)日:2011-10-26
申请号:KR1020100036558
申请日:2010-04-20
Applicant: 현대자동차주식회사
CPC classification number: C08L23/10 , C08L33/02 , C08L51/06 , C08L51/08 , C08L67/04 , C08L2205/03 , C08K3/00 , C08L33/10
Abstract: 본 발명은 폴리프로필렌-폴리유산 복합재료 조성물에 관한 것으로서, 더욱 상세하게는 폴리프로필렌 수지와 폴리유산 수지의 혼합물에 그들의 상용성을 위해 무수 말레인산 그라프트 에틸렌-옥텐 공중합체 및 무수 말레인산 그라프트 폴리유산, 폴리에틸렌-글리시딜 메타아크릴레이트 수지 및 탈크 입자를 첨가한 복합재료 조성물에 관한 것이다. 본 발명의 폴리프로필렌-폴리유산 복합재료 조성물은 이탄화탄소 저감 효과가 큰 바이오 소재인 폴리유산 수지를 사용함으로 해서 저탄소, 녹색성장에 대응 가능하며, 폴리유산 수지의 문제점인 기계적 강도 및 내열성을 향상시킨 소재이므로 자동차 내외장재 및 건축용 내장재 등으로 유용하게 적용할 수 있다.
-
公开(公告)号:KR1020110039901A
公开(公告)日:2011-04-20
申请号:KR1020090096941
申请日:2009-10-12
Applicant: 현대자동차주식회사
CPC classification number: C08L1/12 , C08G69/24 , C08K7/02 , C08L1/00 , C08L1/02 , C08L51/06 , C08L77/02 , C08L97/02 , C08L2666/20 , C08L2666/02
Abstract: PURPOSE: A nylon-4 composite composition is provided to ensure excellent heat resistance and mechanical properties and to reduce fabrication costs compared with nylon composite materials in which existing glass fiber reinforcement is added. CONSTITUTION: A nylon-4 composite composition comprises 60~80 weight% of nylon-4 resin, 15~35 weight% of nano cellulose, 5~25 weight% of maleic anhydride graft poly (ethylene-octene) copolymer resin. The nano cellulose is dispersed inside a maleic anhydride graft poly(ethylene-octene) copolymer resin. The maleic anhydride graft poly(ethylene-octene) copolymer resin is dispersed inside the nylon-4, wherein the nylon-4 resin has a number average molecular weight of 20,000~150,000.
Abstract translation: 目的:与添加现有玻璃纤维增强材料的尼龙复合材料相比,提供了尼龙-4复合材料组合物,以确保优异的耐热性和机械性能,并降低制造成本。 构成:尼龙-4复合组合物包含60〜80重量%的尼龙-4树脂,15〜35重量%的纳米纤维素,5〜25重量%的马来酸酐接枝聚(乙烯 - 辛烯)共聚物树脂。 纳米纤维素分散在马来酸酐接枝聚(乙烯 - 辛烯)共聚物树脂内。 马来酸酐接枝聚(乙烯 - 辛烯)共聚物树脂分散在尼龙-4内,其中尼龙-4树脂的数均分子量为20,000〜150,000。
-
公开(公告)号:KR100936326B1
公开(公告)日:2010-01-12
申请号:KR1020080019361
申请日:2008-02-29
Inventor: 홍채환
Abstract: 본 발명은 폴리염화비닐계 인조피혁에 관한 것으로서, 더욱 상세하게는 콩 단백질 분쇄물을 함유한 표면층 및 코팅층을 포함하는 폴리염화비닐계 인조피혁에 관한 것이다.
본 발명의 폴리염화비닐계 인조피혁은 기존의 인조피혁과 비교하여 수분 흡수력이 매우 우수한 바, 촉감 등의 물성이 뛰어나고 끈적임이 없는 인조피혁 제조에 매우 적합하게 사용할 수 있을 뿐만 아니라, 낮은 단가로 제조가 가능하다.
인조피혁, 폴리염화비닐, 콩 단백질 분쇄물, 콩 단백질 분리체-
公开(公告)号:KR1020090120985A
公开(公告)日:2009-11-25
申请号:KR1020080047057
申请日:2008-05-21
Inventor: 홍채환
CPC classification number: C08K7/02 , C08J5/045 , C08J2401/02 , C08K5/09 , C08L23/12 , C08L51/06 , C08L97/02
Abstract: PURPOSE: A polypropylene-bamboo short fiber bio composite material is provided to improve adhesion between polypropylene resin and bamboo fiber by introducing a polypropylene resin grafted with maleic anhydride and to ensure excellent tensile strength and impact strength. CONSTITUTION: A polypropylene-bamboo short fiber bio composite material suitable for inner and outer materials of automobile comprises 65 ~ 80 weight%of a polypropylene resin with a melt index 0.5 ~ 30 g/10 minute; 15 ~ 30 weight% of bamboo short fiber; and 3 ~ 10 weight% of a polypropylene resin grafted with maleic anhydride.
Abstract translation: 目的:提供聚丙烯竹短纤维生物复合材料,通过引入接枝马来酸酐的聚丙烯树脂,确保优异的拉伸强度和抗冲击强度,提高聚丙烯树脂与竹纤维之间的粘合力。 构成:适用于汽车内外材料的聚丙烯竹纤维短纤维生物复合材料,其熔融指数为0.5〜30g / 10分钟的聚丙烯树脂的65〜80重量%。 15〜30%的竹短纤维; 和3〜10重量%的用马来酸酐接枝的聚丙烯树脂。
-
公开(公告)号:KR1020090093685A
公开(公告)日:2009-09-02
申请号:KR1020080019361
申请日:2008-02-29
Inventor: 홍채환
Abstract: A manufacturing method of polyvinyl chloride artificial leather of which water absorbing power is improved is provided to offer inexpensive raw material cost compared to manufacturing cost of the existing polyvinyl chloride artificial leather containing silk crushed materials. A manufacturing method of polyvinyl chloride artificial leather of which water absorbing power is improved includes a surface layer(3) containing polyvinyl chloride resin 85 ~ 95 weight%, soybean protein crushed materials 5 ~ 15 weight% of which average diameter is 5 ~ 75 mum, and a coating layer(4) containing the soybean protein crushed materials of which diameter is 5 ~ 75 mum and an adhesive with a weight ratio of 70 : 30 ~ 60 : 40. The polyvinyl chloride artificial leather further includes one or more layer selected from a base layer(1) and a foam layer(2). The degree of polymerization the polyvinyl chloride resin is 900 ~ 1400. The base material layer is one or more selected from cloth, non-woven, and raw cotton etc.
Abstract translation: 与现有的含有丝绸粉碎材料的聚氯乙烯人造革的制造成本相比,提供了改善吸水能力的聚氯乙烯人造革的制造方法,从而提供廉价的原材料成本。 改善吸水力的聚氯乙烯人造革的制造方法包括含有85〜95重量%的聚氯乙烯树脂的表层(3),大豆蛋白粉碎物料,其平均直径为5〜75μm的5〜15重量% ,以及含有直径为5〜75μm的大豆蛋白粉碎材料和重量比为70:30〜60:40的粘合剂的涂层(4)。聚氯乙烯人造革还包括一个或多个选择的层 从基层(1)和泡沫层(2)。 聚氯乙烯树脂的聚合度为900〜1400。基材层是从布,无纺布和原棉等中选择的一种或多种。
-
-
-
-
-
-
-
-
-