Bonding and coating agents for metals - consisting of ethylene copolymers with free carboxyl groups and azo or azomethine cpds

    公开(公告)号:DE2245559A1

    公开(公告)日:1974-04-04

    申请号:DE2245559

    申请日:1972-09-16

    Applicant: BASF AG

    Abstract: Coatings and adhesives for brass, Cu, Zn, iron and steel consist of an ethylene copolymer contg. 0.5-30 wt.% bound ethylenically unsatd. carboxylic acid in bound form and 0.01-5 wt.% (on ethylene copolymer) of a hydroxyl gp.-contg. azo- or azomethine cpd. of formula HO-A-N=X-B-OH in which A and B = phenyl- or naphthyl residues and B may also be derived from pyrazole or quinolone-2, or of formula: (in which R1 and R2=H, Cl, Br, NO2, SO3H, COOH, NH2, NHR3 and R3 = alkyl, aryl or phenoxy residue). Pref. copolymer contains 60-90 wt.% ethylene, 0.5-20 wt.% acrylic acid and 0.5-20 wt.% tert. butyl acrylate. The compsns. which give good bond strength with no deterioration in water can be used for coating the metals e.g. by melt extrusion, powder sintering, etc., for bonding the metals to Al, plastics, textiles, rubber, glass, etc., and for the construction of sandwich panels useful in building, behicles, aircraft, containers, etc.

    68.
    发明专利
    未知

    公开(公告)号:FI117510B

    公开(公告)日:2006-11-15

    申请号:FI972059

    申请日:1997-05-14

    Applicant: BASF AG

    Abstract: The following are claimed: (A) biodegradable polyester P1, preparable by reaction of a mixt. comprising: (a1) a mixt. comprising: (a11) 35-95 mol.% of adipic acid and/or one or more ester-forming derivs. of this, (a12) 5-65 mol.% of terephthalic acid and/or one or more ester-forming derivs. of this, and (a13) 0-5 mol.% of a cpd. contg. sulphonate gps., the total of mol.% in (a11)-(a13) being 100 mol.%; and (a2) a dihydroxy cpd. selected from 2-6C alkane-diols and 5-10C cycloalkane-diols. The molar ratio of (a1) to (a2) is 0.4-1.5:1. In addn., 0.01-5 mol.% (based on the molar amt. of component (a1)) of a cpd. D, which comprises at least three gps. capable of forming ester gps., are also used for prodn. of polyester P1. Polyester P1 has (a) a mol.wt. (Mn) of 5000-50000 g/mol; (b) a viscosity no. of 30-350 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a P1 concn. of 0.5 wt.%); and (c) a m.pt. of 50-170 degrees C. (B) biodegradable polyester P2, preparable by reaction of a mixt. comprising: (b1) mixt. comprising: (b11) 20-95 mol.% of adipic acid and/or one or more ester-forming deriv. of this, (b12) 5-80 mol.% of terephthalic acid and/or one or more ester- forming deriv. of this, and (b13) 0-5 mol.% of a cpd. contg. sulphonate gps., the total of mol.% in (b11)-(b13) being 100 mol.%; (b2) a dihydroxy cpd. as (a2) above; (b3) 0.01-100 wt.% (based on the amt. of component (b1) of a hydroxycarboxylic acid B1 which is of formula (Ia) or (Ib); and (b4) 0-5 mol.% (based on the amt. of component (b1)) of a cpd. D. The molar ratio of (b1) to (b2) is 0.4-1.25:1. Polyester P2 has (a) a mol.wt. (Mn) of 5000-80000 g/mol; (b) a viscosity no. of 30 - 450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a P2 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. p = a whole no. from 1-1500; r = a whole no. from 1-4; G = phenylene, (CH2)k, C(R)H and C(R)HCH2; k = 1-5; R = Me or Et. (C) biodegradable polyester Q1 which have: (a) a mol.wt. (Mn) of 5000-100000 g/mol; (b) a viscosity no. of 30-450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a Q1 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. Q1 are obtained by reaction of a mixt. comprising; (c1) polyester P1 and/or a polyester PWD; (c2) 0.01-50 wt.% (based on (c1)) of a hydroxycarboxylic acid B1; and (c3) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of P1 and/or PWD) of a cpd. D. Polyester PWD is obtainable by reaction of components (a1) and (a2) in a molar ratio of (a1) to (a2) of 0.4-1.5:1. Polyester PWD have: (a) a mol.wt. (Mn) of 5000 - 50000 g/mol; (b) a viscosity no. of 30 - 350 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a PWD concn. of 0.5 wt.%); and (c) a m.pt. of 50-170 degrees C. (D) biodegradable polyesters Q2 which have: (a) a mol.wt. (Mn) of 6000 - 60000 g/mol; (b) a viscosity no. of 30-350 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a Q2 concn. of 0.5 wt.%); and (c) a m.pt. of 50-170 degrees C. Q2 are obtained by reaction of a mixt. comprising: (d1) 95-99.9 wt.% of polyester P1 and/or PWD; and (d2) 0.1-50 wt.% of a diisocyanate C1; and (d3) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of P1 and/or PWD) of a cpd. D. (E) biodegradable polymers T1 which have: (a) a mol.wt. (Mn) of 10000 - 100000 g/mol; (b) a viscosity no. of 30-450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a T1 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. T1 are obtd. by reaction of polyester Q1 with (e1) 0.1-5 wt.% (based on the amt. of Q1) of diisocyanate C1 and (e2) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of Q1 via the polyester P1 and/or PWD) of a cpd. D. (F) biodegradable polymers T2 which have: (a) a mol.wt. (Mn) of 10000 - 100000 g/mol/. (b) a viscosity no. of 30-450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a T2 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. T2 are obtained by reaction of polyester Q2 with (f1) 0.01-50 wt.% (based on the amt. of Q2) of hydroxycarboxylic acid B1 and (f2) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of Q2 via the polyester P1 and/or PWD) of a cpd

    69.
    发明专利
    未知

    公开(公告)号:NO319412B1

    公开(公告)日:2005-08-08

    申请号:NO991354

    申请日:1999-03-19

    Applicant: BASF AG

    Abstract: PCT No. PCT/EP97/04908 Sec. 371 Date Mar. 17, 1999 Sec. 102(e) Date Mar. 17, 1999 PCT Filed Sep. 19, 1997 PCT Pub. No. WO98/12242 PCT Pub. Date Mar. 20, 1998Biodegradable polyesters based on A) 95-99.99 mol % of at least one polyester A containing as monomeric building blocks of an acid component comprising a11) 20-95 mol % of at least one aliphatic or cycloaliphatic dicarboxylic acid or its ester-forming derivative and a12) 5-80 mol % of at least one aromatic dicarboxylic acid or its ester-forming derivative and at least one dihydroxy compound or at least one amino alcohol or their mixtures, and B) 0.01-5 mol % of a mixture comprising mono-, bi-, tri-, tetra- and higher-nuclear isocyanurates or corresponding compounds containing two, three or four functional groups capable of reacting with the end groups of polyester A, or mixtures of the isocyanurates and the corresponding compounds, as well as molding compositions comprising said polyesters, their manufacture and their use in the manufacture of moldings, filsm, fibers and coatings.

    BIODEGRADABLE POLYMERS, THE PREPARATION THEREOF, AND THE USETHEREOF FOR PRODUCING BIODEGRADABLE MOLDINGS

    公开(公告)号:CA2205072C

    公开(公告)日:2005-01-11

    申请号:CA2205072

    申请日:1995-06-27

    Applicant: BASF AG

    Abstract: Biodegradable polyether esters P1 obtainable by the reaction of a mixture consisting essentially of: (a1) a mixture essentially of 20 to 95 mol% adipic acid or ester-forming derivatives thereof or mixtures thereof, 5 to 80 mol% terephthalic acid or ester-forming derivatives thereof or mixtures thereof, and 0 to 5 mol% of a sulphonate group-containin g compounds in which the sum of the individual mol percentages is 100; and (a2) a mixture of dihydroxy compounds consisting essentially of (a21) 15 to 99 mol% of a dihydroxy compound selected from the group consisting of C2-C6 alkane diols and C5-C10 cycloalkane diols; (a2 2) 85 to 0.2 mol% of an ether function-containing dihydroxy compound as in formula I HO-[(CH2)n-O]m-H in which n is 2, 3 or 4 and m is a whole number from 2 to 250, or mixtures thereof, in which the molar ratio of (a1) to (a2) is in the range from 0.4:1 to 1.5:1 wi th the proviso that the polyether esters P1 have a molar weight (M n) in the range from 5,000 to 80,000 g/mol, a viscosity index in the rang e from 30 to 450 g/ml (measured in o-dichlorobenzole/phenol (weight ratio 50/50) at a concentration of 0.5 wt.% polyether esters P1 at a temperature of 25 .degree.C) and a melting point in the range from 50 to 200 .degree.C, and with the further proviso that from 0.01 to 5 mol%, in relation to the molar quantity of the components (a1) used, of a compound D with at least three groups capable of ester formation are used to produce the polyether esters P1, and other biodegradable polymers and thermoplastic moulding compounds, process for their production and biodegradable mouldings, adhesives, foams and blends with starch obtainable from the polymers or moulding compounds of the invention.

Patent Agency Ranking