公开(公告)号:DE50003285D1
公开(公告)日:2003-09-18
申请号:DE50003285
申请日:2000-05-03
Applicant: BASF AG
Inventor: DECKERS ANDREAS , WEBER WILHELM
Abstract: Copolymers of ethylene have from 1 to 30 mol % of alkyl(meth)acrylates and, if desired, other comonomers, and have a residual comonomer content of less than 0.5% by weight in the copolymer. A process for preparing copolymers of this type in a combination of stirred autoclave and tubular reactor is described, as is the use of the copolymers for preparing polyamide molding compositions.
-
公开(公告)号:DE10064800A1
公开(公告)日:2002-06-27
申请号:DE10064800
申请日:2000-12-22
Applicant: BASF AG
Inventor: WITTKOWSKI LARS , ZEITZ KATRIN , WEBER WILHELM , DECKERS ANDREAS
IPC: A61K8/86 , A61Q1/04 , A61Q11/00 , A61Q19/00 , C08F2/38 , C08F10/02 , A61K7/027 , A61K7/031 , A61K7/032 , C08J3/12
Abstract: A micronized (co)polyethylene wax obtained by high pressure copolymerization of ethylene with an aliphatic or alicyclic ketone as molecular weight regulator followed by micronization is new.
-
公开(公告)号:DE10064799A1
公开(公告)日:2002-06-27
申请号:DE10064799
申请日:2000-12-22
Applicant: BASF AG
Inventor: WITTKOWSKI LARS , ZEITZ KATRIN , WEBER WILHELM , DECKERS ANDREAS
IPC: A61K8/86 , A61Q1/04 , A61Q11/00 , A61Q19/00 , A61K7/00 , A61F13/15 , A61K7/02 , A61K7/04 , A61K7/48 , A61K7/50
Abstract: Polyethylene waxes (I), produced by high-pressure (co)polymerization of ethylene using an aliphatic or alicyclic ketone as a molecular weight regulator, are used in cosmetic compositions or applications.
-
公开(公告)号:DE10006900A1
公开(公告)日:2001-08-23
申请号:DE10006900
申请日:2000-02-16
Applicant: BASELL POLYOLEFINE GMBH , BASF AG
Inventor: MAEHLING FRANK-OLAF , DECKERS ANDREAS , LITTMANN DIETER , SUTORIS HEINZ FRIEDRICH , EVERTZ KASPAR
IPC: C08F2/01 , C08F2/38 , C08F2/40 , C08F10/00 , C08F110/02 , C08F297/08 , C08F10/02
Abstract: The invention relates to a method for polymerizing or copolymerizing ethylenically unsaturated monomers in the presence of radically decomposing polymerization initiators in a continuously operating polymerization device. Said polymerization device is composed of a fresh gas supply, a pre-compressor, a post-compressor, a reactor, a pressure maintaining valve, of a high-pressure circuit, which is provided with a high-pressure product separator and with a high-pressure circuit gas return, and of a product valve and a low-pressure circuit, which is provided with a low-pressure product separator and with a low-pressure circuit gas return. The inventive method is characterized in that nitrogen monoxide or oxygen is added in a dosed manner as an inhibitor into the high-pressure circuit, into the low-pressure circuit and/or into the pre-compressor.
-
公开(公告)号:DE19859391A1
公开(公告)日:2000-06-29
申请号:DE19859391
申请日:1998-12-22
Applicant: BASF AG
Inventor: SUTORIS HEINZ FRIEDRICH , DECKERS ANDREAS , WEBER WILHELM
IPC: C07B63/04 , C07C7/20 , C07C11/02 , C07C11/04 , C08F2/40 , C08F2/44 , C08F10/00 , C08F210/00 , C08F236/06
Abstract: A process for the compression of ethylenically unsaturated monomers at a pressure of 200-5,000 bar in the absence of a polymerization initiator is carried out in the presence of a nitroxyl compound (I). A process for the condensation of ethylenically unsaturated monomers at a pressure of 200-5,000 bar in the absence of a polymerization initiator is carried out in the presence of a nitroxyl compound of formula (I). Independent claims are included for: (i) a process for the production of copolymers by condensation of the comonomer, optionally as a mixture in the presence of (I) followed by polymerization at 50-350 degrees C by addition of a polymerization initiator; (ii) the resulting copolymer product. R , R = 1-4C alkyl or R and R together with the C atom they are bonded to form a 5 or 6 C saturated hydrocarbon ring; R = 1-4C alkyl; R = H or 1-12C alkyl.
-
公开(公告)号:NO20002778D0
公开(公告)日:2000-05-30
申请号:NO20002778
申请日:2000-05-30
Applicant: BASF AG
Inventor: DECKERS ANDREAS , WENDEROTH BERND , WEDEL PETER , WEBER WILHELM
IPC: C10L1/18 , C08F2/00 , C08F210/02 , C08F218/08 , C10L1/197 , C08F
Abstract: In a process for preparing ethylene-vinyl acetate copolymers in which a mixture of ethylene and vinyl acetate is polymerized continuously in the presence of free-radical polymerization initiators and, if desired, molecular weight regulators in a cooled tube reactor at a pressure in the range from 1000 to 3500 bar, and the poly-merization initiator is added at the beginning and at two or more points along the tube reactor, and temperature changes in the reaction mixture along the tube reactor, between the first temperature maximum and the last addition of the polymerization initiator, are within a range of not more than 20° C.
-
公开(公告)号:ES2139456T3
公开(公告)日:2000-02-01
申请号:ES97921743
申请日:1997-04-24
Applicant: BASF AG
Inventor: DECKERS ANDREAS , KINGMA AREND JOUKE , MOLL ULRICH , WEBER WILHELM
IPC: C09D123/30 , A23B7/16 , C08F4/659 , C08F4/6592 , C08F8/06 , C08F10/02 , C08F110/02 , C08L23/30 , C09G1/08
Abstract: Oxidized waxes are obtainable by oxidation of polyolefins obtainable by means of metallocene catalysis and having a molecular weight Mw in the range from 1000 to 40,000 g/mol.
-
公开(公告)号:BR9709269A
公开(公告)日:1999-08-10
申请号:BR9709269
申请日:1997-05-23
Applicant: BASF AG
Inventor: KINGMA AREND JOUKE , LAPPE ANDREA , DECKERS ANDREAS
IPC: C08J3/20 , B05D5/00 , B05D7/16 , C08L23/26 , C08L33/02 , C08L35/00 , C09D5/00 , C09D5/20 , C09D123/02 , C09D123/08
Abstract: Temporary protection of surfaces is achieved by application of an aqueous polymer dispersion containing a) at least one C2-C10 olefin, and b) at least one comonomer that may be copolymerized with the olefin under radical conditions. The dispersion layer applied is then dried to give a solid polymer film having a mean thickness exceeding 20 mu m. The invention also refers to coloured polymer dispersions and their use in temporarily protecting or in colouring surfaces.
-
公开(公告)号:AU7432098A
公开(公告)日:1998-12-08
申请号:AU7432098
申请日:1998-04-24
Applicant: BASF AG
Inventor: GONIOUKH ANDREI , SCHAUSS ECKARD , KLIMESCH ROGER , DECKERS ANDREAS , WEBER WILHELM
IPC: C08F4/623 , C08F2/06 , C08F4/629 , C08F4/642 , C08F4/6592 , C08F4/68 , C08F10/00 , C08F110/02
Abstract: A catalyst solution for polymerizing alpha-olefins is obtainable by reacting a metallocene compound with an activator compound which can react with the metallocene compound so as to displace a ligand from the central atom and stabilize the resulting cationic complex by a non-coordinating anion as an ion pair, adding one or more alpha-olefins in a molar ratio of metallocene compound: alpha-olefins of from 1:1 und 1:100 and mixing with at least 10 parts by volume of an aliphatic hydrocarbon.
-
公开(公告)号:AU2701297A
公开(公告)日:1997-11-19
申请号:AU2701297
申请日:1997-04-24
Applicant: BASF AG
Inventor: MOLL ULRICH , DECKERS ANDREAS , KINGMA AREND JOUKE , WEBER WILHELM
IPC: C08F2/00 , C08F4/44 , C08F4/46 , C08F4/50 , C08F4/622 , C08F4/639 , C08F4/6392 , C08F4/642 , C08F4/68 , C08F10/02 , C08F110/02
Abstract: A process is disclosed for preparing ethylene polymers with a molecular weight Mw (weight average) lower than 20,000 g/mole at temperatures in a range from 200 to 280 DEG C and pressures in a range from 1000 to 3500 bars in the presence of a catalyst system. The catalyst system used contains: (A) a non-bridged substituted or unsubstituted biscyclopentadienyl complex; (B) a metal compound of general formula (I) M (R )r (R )s (R )t, in which M is an alkaline, an alkaline earth metal or a metal of the third main group of the periodic table; R is hydrogen, C1-C10-alkyl, C6-C15-aryl, alkylaryl or arylalkyl with 1 to 10 C atoms in the alkyl radical and 6 to 20 C atoms in the aryl radical; R and R independently represent hydrogen, halogen, C1-C10-alkyl, C6-C15-aryl, alkylaryl, arylalkyl or alkoxy with 1 to 10 C atoms in the alkyl radical and 6 to 20 C atoms in the aryl radical; r is an integer from 1 to 3; and s and t are integers from 0 to 2, the sum r+s+t corresponding to the valency of M ; and (C) a metallocene ion-forming compound selected in a group which consists of strong, neutral Lewis acids, ionic compounds with lewis acid cations and ionic compounds with Brönsted acids as cations. Components (A), (B) and (C) are mixed together and after at the latest 5 minutes are dosed in the reactor.
-
-
-
-
-
-
-
-
-