    Abstract: PURPOSE: A ceramic chip antenna is provided to reduce the size of structure by connecting a plurality of helical conductors to a single feeding unit. CONSTITUTION: A chip main frame(100) is produced by layering a plurality of green sheets, each of which is made of a ceramic insulating material. A first helical conductor(120) and a second helical conductor(130) are formed within the chip main frame(100). A single power supplying unit is connected to the first helical conductor(120) and the second helical conductor(130) to apply a predetermined voltage to the first helical conductor(120) and the second helical conductor(130). The first helical conductor(120) and the second helical conductor(130) have an identical spiral rotational axis centering on the single power supplying unit.

    Abstract translation: 目的:提供陶瓷芯片天线,以通过将多个螺旋导体连接到单个馈送单元来减小结构的尺寸。 构成:通过层叠多个生坯片来制造芯片主框架(100),每个生坯片由陶瓷绝缘材料制成。 第一螺旋导体(120)和第二螺旋导体(130)形成在芯片主框架(100)内。 单个供电单元连接到第一螺旋导体(120)和第二螺旋导体(130),以向第一螺旋导体(120)和第二螺旋导体(130)施加预定电压。 第一螺旋导体(120)和第二螺旋导体(130)具有以单个供电单元为中心的相同螺旋旋转轴。

    고주파용 유전체 세라믹 조성물

    公开(公告)号:KR100356641B1

    公开(公告)日:2002-10-18

    申请号:KR1020000016760

    申请日:2000-03-31

    Abstract: 본 발명은 조성식 (1-x)(Al
    1/2 Ta
    1/2 )O
    2 - x(Mg
    1/3 Ta
    2/3 )O
    2 로 표시되고, x의 범위가 0≤x≤1인 고주파용 유전체 조성물을 제공한다. 이 조성물은 유전율이 8.7 내지 27.1이고, Qxf
    O (GHz)가 6500 내지 111230이며, 공진 주파수의 온도 계수(τ
    f )의 범위가 -55.2 내지 +51.2 ppm/℃로서 조성의 변화에 따라 τ
    f 를 0 ppm/℃로 조절이 가능하여 고주파용 유전체 세라믹스 부품의 재료로서 사용될 수 있는 우수한 특성을 갖는 고주파용 유전체 조성물이다.

    마이크로파용 유전체 세라믹 조성물
    73.
    发明公开
    마이크로파용 유전체 세라믹 조성물 失效
    用于微波的电介质陶瓷组合物

    公开(公告)号:KR1020020074714A

    公开(公告)日:2002-10-04

    申请号:KR1020010014667

    申请日:2001-03-21

    Abstract: PURPOSE: Provided is a microwave dielectric ceramic composition of the (1-x)(Al1/2Ta1/2)O2-xTiO2 system having high dielectric constant, large Q value, and temperature coefficient of resonant frequency which can be turned to zero. CONSTITUTION: The dielectric ceramic composition is expressed by the formula of (1-x)(Al1/2Ta1/2)O2-xTiO2, wherein x is in the range of 0.1

    Abstract translation: 目的:提供具有高介电常数,大Q值和谐振频率温度系数可以变为零的(1-x)(Al1 / 2Ta1 / 2)O2-xTiO2系的微波介电陶瓷组合物。 构成:电介质陶瓷组合物由式(1-x)(Al1 / 2Ta1 / 2)O2-xTiO2表示,其中x在0.1≤x≤0.5的范围内。 该组成范围的材料的介电常数为14.1〜45.5,Qxfo为6700-78690GHz,共振频率(TCF)的温度系数为-31.7〜+ 99.9ppm /℃。 该组合物用于诸如谐振器,双工器,滤波器等移动电信设备。

    고주파용 유전체 조성물
    74.
    发明授权
    고주파용 유전체 조성물 失效
    高频电介质的组成

    公开(公告)号:KR100327153B1

    公开(公告)日:2002-03-13

    申请号:KR1019990037026

    申请日:1999-09-02

    Abstract: 본발명은하기조성식으로표시되는, 높은유전율과품질계수(Q값)를갖고공진주파수의온도계수가우수한고주파용유전체조성물을제공한다. x(BaCaMg)O-0.125NdO-zTiO+vBiO+wAlO 상기식에서, x, y, z, v, w는각각 0.13≤x≤0.16, 0.01≤y≤0.10, 0.59≤z≤0.62, 10≤v(wt%)≤11.5, 0≤w(wt%)≤1.5이다. 또한, 상기고주파용유전체조성물은 x, y, z, v, w가각각 x=0.15, 0.07≤y≤0.10, z=0.60, 10≤v(wt%)≤11, 0≤w(wt%)≤1.5일때, 공진주파수의온도계수가 ±10 이내로실제이용이가능한조성물을포함한다. 이조성물은고순도(>99.9%)의원료를사용할경우유전율이 82 내지 97이고, Qxf(GHz)가 3400 내지 5480이며, 공진주파수의온도계수(TCF)의범위가 0 내지 +37 ppm/℃로서조성의변화에따라공진주파수의온도계수(TCF)를 0 ppm/℃로조절할수 있다. 양산용저순도(

    일체형 유전체 필터
    75.
    发明授权
    일체형 유전체 필터 失效
    电介质滤波器

    公开(公告)号:KR100265675B1

    公开(公告)日:2000-09-15

    申请号:KR1019980007447

    申请日:1998-03-06

    Abstract: PURPOSE: An integral dielectric filter is provided to easily control a band width by controlling a capacitance connection between two resonators which are present in one block. CONSTITUTION: One dielectric block(1) has a hexahedral shape. Two resonating holes(2,2') are longitudinally formed in the dielectric block(1). The two resonating holes(2,2') include an open surface(3) which is electrically opened and a short surface which is electrically shorted. The short surface of the two resonating holes(2,2') acts as an external electrode for a ground of a dielectric filter. Input and output electrode terminals(4,4') are symmetrically formed to each other. The input and output electrode terminals(4,4') and the external electrode(8) are divided into each other and electrically intercepted.

    Abstract translation: 目的:提供一个整体介质滤波器,通过控制一个块中存在的两个谐振器之间的电容连接来容易地控制带宽。 构成:一个介质块(1)具有六面体形状。 两个谐振孔(2,2')在介质块(1)中纵向形成。 两个谐振孔(2,2')包括电气打开的开放表面(3)和电短路的短表面。 两个谐振孔(2,2')的短表面用作介质滤波器的接地的外部电极。 输入和输出电极端子(4,4')彼此对称地形成。 输入和输出电极端子(4,4')和外部电极(8)彼此分开并电截取。

    고주파용 유전체 자기 조성물
    76.
    发明授权
    고주파용 유전체 자기 조성물 失效
    用于微波应用的电介质陶瓷组合物

    公开(公告)号:KR100227763B1

    公开(公告)日:1999-11-01

    申请号:KR1019970035786

    申请日:1997-07-29

    Abstract: 본 발명은 x(Ba
    0.85 Ca
    (1-W) Mg
    w )O-yNd
    2 O
    3 -zTiO
    2 +vBi
    2 O
    3 를 기본 조성으로 하는 x의 범위는 0.13 내지 0.16몰, y는 0.25몰, z의 범위는 0.59 내지 0.62몰, w의 범위는 0.01 내지 0.1몰, 첨가물 Bi
    2 O
    3 인 v의 함량은 10 내지 11중량 %인 고주파용 유전체 조성물에 관한 것이다. 이 조성물은 Ba, Ti와 Ca, Mg의 함량과 첨가몰 Bi
    2 O
    3 의 함량을 조절함으로써 유전율이 78 내지 92이고, Q·f
    0 (GHz)가 2730 내지 5780이며 공진 주파수의 온도계수는 0 내지 +33ppm/℃로서, 공진 주파수의 온도계수 조정이 용이하여 유전체 공진기 소재로 응용이 적합하다.

    고주파용 유전체 자기 조성물

    公开(公告)号:KR1019990012412A

    公开(公告)日:1999-02-25

    申请号:KR1019970035786

    申请日:1997-07-29

    Abstract: 본 발명은 x(Ba
    0.85 Ca
    (1-W) Mg
    w )O-yNd
    2 O
    3 -zTiO
    2 +vBi
    2 O
    3 를 기본 조성으로 하는 x의 범위는 0.13 내지 0.16몰, y는 0.25몰, z의 범위는 0.59 내지 0.62몰, w의 범위는 0.01 내지 0.1몰, 첨가물 Bi
    2 O
    3 인 v의 함량은 10 내지 11중량 %인 고주파용 유전체 조성물에 관한 것이다. 이 조성물은 Ba, Ti와 Ca, Mg의 함량과 첨가몰 Bi
    2 O
    3 의 함량을 조절함으로써 유전율이 78 내지 92이고, Q·f
    0 (GHz)가 2730 내지 5780이며 공진 주파수의 온도계수는 0 내지 +33ppm/℃로서, 공진 주파수의 온도계수 조정이 용이하여 유전체 공진기 소재로 응용이 적합하다.

    고주파용 유전체 조성물
    78.
    发明公开

    公开(公告)号:KR1019980068362A

    公开(公告)日:1998-10-15

    申请号:KR1019970004899

    申请日:1997-02-18

    Abstract: 본 발명은 마이크로파 대역에서 높은 품질 계수와 유전율을 가지며 공진 주파수의 온도 계수가 안정한 고주파용 유전체 자기 조성물로서, (1-x)(La
    1/2 Na
    1/2 )TiO
    3 - xCa(Fe
    1/2 Nb
    1/2 )O
    3 (식중, 0.4 ≤ x ≤ 0.7)로 나타내지는 고주파용 유전체 자기 조성물에 관한 것이다. 이 조성물은 Ca(Fe
    1/2 Nb
    1/2 )O
    3 의 함량을 조절함으로써 공진 주파수의 온도 계수의 조정이 용이해서, 유전체 공진기 소재로서의 응용에 적합하다.