公开(公告)号:DE50105945D1
公开(公告)日:2005-05-25
申请号:DE50105945
申请日:2001-10-08
Applicant: BASF AG
Inventor: LACH CHRISTIAN , BAUMSTARK ROLAND
IPC: C08F220/18 , C09D5/02 , C09D133/06 , C09D133/10
Abstract: Described is a water-based, pigmented coating composition essentially free from volatile organic compounds and comprising i) an aqueous binder formulation as component I, with a minimum film formation temperature MFFT
-
公开(公告)号:AU777848B2
公开(公告)日:2004-11-04
申请号:AU5349200
申请日:2000-08-18
Applicant: BASF AG
Inventor: BAUMSTARK ROLAND , KIRSCH STEFAN , DERSCH ROLF , DOBBELAAR JOHANNES , MELAN MICHAEL
IPC: C08L33/06 , C08F2/24 , C08F212/02 , C08F212/04 , C08F220/12 , C08K5/00 , C08L25/00 , C09D5/02 , C09D125/02 , C09D133/06 , E04C2/04 , C09D133/08 , C08L25/14 , C08L33/08 , C08L33/10 , C09D125/14 , C09D133/10
Abstract: Binder preparation with a minimum film-forming temperature below 10 degrees C, based on a dispersion containing anionic and non-ionic emulsifiers and a copolymer of 20-50 wt% vinyl-aromatic monomer, 45-70 wt% 1-18C alkyl acrylate or 5-18C alkyl methacrylate which forms a homopolymer with a Tg below 10 degrees C, 2-4 wt% methacrylic acid and optionally other comonomers. A binder preparation with a minimum film-forming temperature (MFT) below 10 degrees C, based on a binder polymer (P) in the form of an aqueous dispersion containing anionic emulsifier(s) and non-ionic emulsifier(s), in which (P) is a copolymer of (A1) 20-50 wt% vinyl-aromatic monomer(s), (A2) 0-15 wt% 1-4C alkyl (meth)acrylate(s), (A3) 0-30 wt% (meth)acrylonitrile, (B) 45-70 wt% monomer(s) which form a homopolymer with a glass transition point (Tg) below 10 degrees C, selected from 1-18C alkyl acrylates and 5-18C alkyl methacrylates, (C) 2-4 wt% methacrylic acid, (D) 0-3 wt% monomer(s) selected from amides, 1-4C hydroxyalkyl esters and 1-4C alkyl-polyalkyleneoxide-esters of 3-6C mono-unsaturated monocarboxylic acids and (E) 0-5 wt% other monomer(s), where the total amount of monomers (A1)-(A3) does not exceed 55 wt% of the total monomer content and the content of (A2) is at least 5 wt% if the content of (A3) is less than 0.5 wt%. An Independent claim is also included for emulsion paint containing binder preparation(s) as described.
-
公开(公告)号:ES2207937T3
公开(公告)日:2004-06-01
申请号:ES99911795
申请日:1999-03-15
Applicant: BASF AG
Inventor: ZHAO CHENG-LE , ROSER JOACHIM , DERSCH ROLF , BAUMSTARK ROLAND
IPC: C08L57/04 , C08F2/44 , C08F220/12 , C08F222/02 , C09D5/02 , C09D7/12 , C09D17/00 , C09D133/06 , C09D151/00
-
公开(公告)号:DE59908766D1
公开(公告)日:2004-04-08
申请号:DE59908766
申请日:1999-08-17
Applicant: BASF AG
Inventor: WOOD CLAUDIA , BAUMSTARK ROLAND , DOBBELAAR JOHANNES
-
公开(公告)号:DE59906872D1
公开(公告)日:2003-10-09
申请号:DE59906872
申请日:1999-03-15
Applicant: BASF AG
Inventor: ZHAO CHENG-LE , ROSER JOACHIM , DERSCH ROLF , BAUMSTARK ROLAND
IPC: C08L57/04 , C08F2/44 , C08F220/12 , C08F222/02 , C09D5/02 , C09D7/12 , C09D17/00 , C09D133/06 , C09D151/00
-
公开(公告)号:DE10049791A1
公开(公告)日:2002-04-18
申请号:DE10049791
申请日:2000-10-09
Applicant: BASF AG
Inventor: LACH CHRISTIAN , BAUMSTARK ROLAND
IPC: C08F220/18 , C09D5/02 , C09D133/06 , C09D133/10 , C09D17/00
Abstract: Pigmented, water-based, solvent-free coating material containing an aqueous binder comprising a dispersion of copolymer based on alkyl (meth)acrylate monomers plus 3-6C mono-unsaturated monocarboxylic acid in amounts of less than 1 wt%, with a total polar comonomer content (including these acids) of 0.1-10 wt%. Pigmented, water-based coating material, essentially free from volatile, water-insoluble organic compounds, containing (I) an aqueous binder with a minimum film-forming temperature (MFT) of not more than 5 deg C, based on an aqueous dispersion of polymer(s) (P) derived from (A) 90-99.9 wt.% of at least two different types of monomer comprising (A1) 2-12C alkyl acrylates and (A2) 1-12C alkyl methacrylates, (B) from 0 to less than 1 wt.% 3-6C mono-unsaturated monocarboxylic acid, (C) 0-0.5 wt.% 4-6C mono-unsaturated dicarboxylic acid and/or unsaturated sulfonic acid, (D) 0-2 wt.% amides of mono-acids of type (B), (E) 0-5 wt.% 2-4C hydroxyalkyl esters of (B) (E1) and/or esters of (B) with poly-(2-3C alkylene oxides) (E2), (F) 0-5 wt% mono-unsaturated monomers with urea groups and/or mono-unsaturated monomers with an acetylacetoxy group (CH3COCH2COO-), where the total amount of (B) and (C) is less than 1 wt% (based on A-F) and the total amount of (B-F) is 0.1-10 wt.%, (II) inorganic pigment particles, (III) optionally inorganic filler particles and (IV) typical auxiliary substances for coating materials. The coating material contains less than 0.05 wt% Photoinitiators (based on P) and has a pigment volume concentration (PVC) of more than 20.
-
公开(公告)号:DE19939327A1
公开(公告)日:2001-02-22
申请号:DE19939327
申请日:1999-08-19
Applicant: BASF AG
Inventor: BAUMSTARK ROLAND , KIRSCH STEFAN , DERSCH ROLF , DOBBELAAR JOHANNES , MELAN MICHAEL
IPC: C08L33/06 , C08F2/24 , C08F212/02 , C08F212/04 , C08F220/12 , C08K5/00 , C08L25/00 , C09D5/02 , C09D125/02 , C09D133/06 , E04C2/04 , C08L33/04 , C08L25/08
Abstract: Binder preparation with a minimum film-forming temperature below 10 degrees C, based on a dispersion containing anionic and non-ionic emulsifiers and a copolymer of 20-50 wt% vinyl-aromatic monomer, 45-70 wt% 1-18C alkyl acrylate or 5-18C alkyl methacrylate which forms a homopolymer with a Tg below 10 degrees C, 2-4 wt% methacrylic acid and optionally other comonomers. A binder preparation with a minimum film-forming temperature (MFT) below 10 degrees C, based on a binder polymer (P) in the form of an aqueous dispersion containing anionic emulsifier(s) and non-ionic emulsifier(s), in which (P) is a copolymer of (A1) 20-50 wt% vinyl-aromatic monomer(s), (A2) 0-15 wt% 1-4C alkyl (meth)acrylate(s), (A3) 0-30 wt% (meth)acrylonitrile, (B) 45-70 wt% monomer(s) which form a homopolymer with a glass transition point (Tg) below 10 degrees C, selected from 1-18C alkyl acrylates and 5-18C alkyl methacrylates, (C) 2-4 wt% methacrylic acid, (D) 0-3 wt% monomer(s) selected from amides, 1-4C hydroxyalkyl esters and 1-4C alkyl-polyalkyleneoxide-esters of 3-6C mono-unsaturated monocarboxylic acids and (E) 0-5 wt% other monomer(s), where the total amount of monomers (A1)-(A3) does not exceed 55 wt% of the total monomer content and the content of (A2) is at least 5 wt% if the content of (A3) is less than 0.5 wt%. An Independent claim is also included for emulsion paint containing binder preparation(s) as described.
-
公开(公告)号:AU3035199A
公开(公告)日:1999-10-11
申请号:AU3035199
申请日:1999-03-15
Applicant: BASF AG
Inventor: ZHAO CHENG-LE , ROSER JOACHIM , DERSCH ROLF , BAUMSTARK ROLAND
IPC: C08L57/04 , C08F2/44 , C08F220/12 , C08F222/02 , C09D5/02 , C09D7/12 , C09D17/00 , C09D133/06 , C09D151/00
-
公开(公告)号:DE59404792D1
公开(公告)日:1998-01-22
申请号:DE59404792
申请日:1994-09-27
Applicant: BASF AG
Inventor: BAUMSTARK ROLAND , PORTUGALL MICHAEL
IPC: C08L57/00 , C08F2/22 , C08K5/07 , C08L33/06 , C09D129/00 , C09D129/10 , C09D133/02 , C09D133/04 , C09D133/06 , C09D133/14 , C09D133/24 , C09D137/00 , C09D139/00 , C09D141/00 , C09D157/00 , C09D157/12 , C09D201/02 , C09J157/00 , C09J201/00 , C09K3/10
Abstract: PCT No. PCT/EP94/03224 Sec. 371 Date Mar. 11, 1996 Sec. 102(e) Date Mar. 11, 1996 PCT Filed Sep. 27, 1994 PCT Pub. No. WO95/09896 PCT Pub. Date Apr. 13, 1995Aqueous polymer compositions which contain a polymer having ureido groups and a polyaldehyde compound are suitable for the production of coatings having high adhesion to substrate and having high cohesion.
-
公开(公告)号:AU683090B2
公开(公告)日:1997-10-30
申请号:AU7810294
申请日:1994-09-27
Applicant: BASF AG
Inventor: BAUMSTARK ROLAND , PORTUGALL MICHAEL
IPC: C08L57/00 , C08F2/22 , C08K5/07 , C08L33/06 , C09D129/00 , C09D129/10 , C09D133/02 , C09D133/04 , C09D133/06 , C09D133/14 , C09D133/24 , C09D137/00 , C09D139/00 , C09D141/00 , C09D157/00 , C09D157/12 , C09D201/02 , C09J157/00 , C09J201/00 , C09K3/10
Abstract: PCT No. PCT/EP94/03224 Sec. 371 Date Mar. 11, 1996 Sec. 102(e) Date Mar. 11, 1996 PCT Filed Sep. 27, 1994 PCT Pub. No. WO95/09896 PCT Pub. Date Apr. 13, 1995Aqueous polymer compositions which contain a polymer having ureido groups and a polyaldehyde compound are suitable for the production of coatings having high adhesion to substrate and having high cohesion.
-
-
-
-
-
-
-
-
-