公开(公告)号:DE10149870A1
公开(公告)日:2003-04-24
申请号:DE10149870
申请日:2001-10-10
Applicant: BASF AG
Inventor: WEBER MARTIN , CHAROENSIRISOMBOON PIYADA
Abstract: Molding composition contains: (A) polyarylene ether sulfone; (B) thermoplastic polyamide; (C) polyarylene ether sulfone with 0.01-10 wt.% units derived from compound with \- 3 hydroxyl or halogen substituents linked directly to aromatic ring and substitutable under polyarylene ether sulfone synthesis conditions and also anhydride groups; (D) filler; (E) impact-modifying rubber; and (F) additives. Molding composition contains: (A) 1-98.5 wt.% polyarylene ether sulfone; (B) 1-98.5 wt.% thermoplastic polyamide; (C) 0.5-30 wt.% polyarylene ether sulfone with 0.01-10 wt.% units derived from compound with \- 3 hydroxyl or halogen substituents linked directly to aromatic ring and substitutable under polyarylene ether sulfone synthesis conditions and also anhydride groups; (D) 0-60 wt.% filler; (E) 0-40 wt.% impact-modifying rubber; and (F) 0-40 wt.% additives. Independent claims are also included for the following: (1) Production of the molding compositions by mixing components A to F; (2) Moldings, films or fibers made from the molding compositions.
-
公开(公告)号:DE59803148D1
公开(公告)日:2002-03-28
申请号:DE59803148
申请日:1998-11-04
Applicant: BASF AG
Inventor: WEBER MARTIN , WOLF PETER , GRUTKE STEFAN
Abstract: Thermoplastic molding compositions compriseA) from 10 to 97.9% by weight of a partly crystalline polyamide,B) from 0.1 to 50% by weight of a copolyamide composed ofB1) from 60 to 90 mol % of units derived from s-caprolactam andB2) from 10 to 40 mol % of units derived from aliphatic dicarboxylic acids and from aliphatic diamines,C) from 1 to 40% by weight of a copolymer based on styrene or on substituted styrenes and on unsaturated nitriles,D) from 1 to 50% by weight of a fibrous filler andE) from 0 to 30% by weight of other additives,where the percentages by weight of components A) to E) are 100% in total.
-
公开(公告)号:ES2161467T3
公开(公告)日:2001-12-01
申请号:ES97927075
申请日:1997-05-28
Applicant: BASF AG
Inventor: WEBER MARTIN , HORN PETER , WEISS ROBERT , HECKMANN WALTER , HINGMANN ROLAND
IPC: C08K3/04 , C08K5/49 , C08K7/00 , C08K7/22 , C08K7/24 , C08L25/00 , C08J5/18 , C08L25/06 , C08L71/12 , D01F1/07 , D01F6/56 , D01F6/88
Abstract: Flame-retardant, thermoplastic molding materials containingA) at least one polyphenylene ether,B) at least one vinylaromatic polymer andC) at least one flameproofing agent,compriseD) an amount of expandable graphite which increases the resistance of the molding material to drippingand are used for the production of flame-retardant moldings, fibers and films.
-
公开(公告)号:AT203254T
公开(公告)日:2001-08-15
申请号:AT97920704
申请日:1997-04-17
Applicant: BASF AG
Inventor: GAREISS BRIGITTE , SCHNEIDER HANS-MICHAEL , WEBER MARTIN
Abstract: PCT No. PCT/EP97/01912 Sec. 371 Date Oct. 15, 1998 Sec. 102(e) Date Oct. 15, 1998 PCT Filed Apr. 17, 1997 PCT Pub. No. WO97/40092 PCT Pub. Date Oct. 30, 1997Flame-retardant thermoplastic molding compositions comprise A) from 5 to 99% by weight of a thermoplastic polymer, B) from 0.1 to 50% by weight of a phosphazene of the general formula I(PN2-xH1-y)zI where the numerical values of x, y and z, independently of one another, are as follows: 1>x>0.05 1>y>0.05 z>1, and C) from 0 to 70% by weight of other additives and processing aids, where the total of the percentages by weight of components A) to C) is 100%.
-
公开(公告)号:DE10080359D2
公开(公告)日:2001-08-09
申请号:DE10080359
申请日:2000-02-05
Applicant: BASF AG
Inventor: QUEISSER JOACHIM , WEBER MARTIN , MUEHLBACH KLAUS
IPC: C08G67/02 , C08F283/00 , C08L51/08 , C08L73/00
-
公开(公告)号:AU1279001A
公开(公告)日:2001-06-04
申请号:AU1279001
申请日:2000-11-10
Applicant: BASF AG
Inventor: WEBER MARTIN , HECKMANN WALTER
Abstract: The invention relates to thermoplastic molding materials containing the following main components: A) 2 to 97.9 wt. % of at least one polyester; B) 0 to 95.9 wt. % of at least one polycarbonate; C) 1 to 80 wt. % of at least one graft polymer which is made up of c 1 ) 40 to 80 wt. % of a graft base consisting of a rubber elastic polymer based on alkyl acrylates with 1 to 8 C-atoms in the alkyl radical and with a glass transition temperature of less than 10° C., c 2 ) 20 to 60 wt. % of a graft support consisting of c 21 ) 60 to 95 wt. % styrene or substituted styrenes of general formula (I), wherein R represents an alkyl radical with 1 to 8 C-atoms or a hydrogen atoms and R 1 represents an alcohol radical with 1 to 8 C-atoms and the value of n is 1, 2 or 3 and c 22 ) 5 to 40 wt. % of at least one unsaturated nitrile; D) 1 to 80 wt. % of a copolymer consisting of d 1 ) 60 to 95 % styrene or substituted styrenes of general formula (I) or mixtures thereof and d 2 ) 5 to 40 wt. % of at least one unsaturated nitrile; E) 0.1 to 10 wt. % of an epoxyde resin; and F) 0 to 80 wt. % other additives, the sum of the weight percentages of components A) to F) being 100%.
-
公开(公告)号:DE19956539A1
公开(公告)日:2001-05-31
申请号:DE19956539
申请日:1999-11-24
Applicant: BASF AG
Inventor: WEBER MARTIN , HECKMANN WALTER
Abstract: A thermoplastic molding material containing as essential components (wt.%): (A) at least one polyester (2-97.9), (B) at least one polycarbonate (0-95.9), (C) at least one graft polymerisate, (D) a copolymerisate, (E) an epoxy resin (0.1-10), and (F) further additives, where the sum of components A to F = 1-% is new. the thermoplastic molding materials contains as essential components (wt.%): (A) at least one polyester (2-97.9), (B) at least one polycarbonate (0-95.9), (C) at least one graft polymerisate, (D) a copolymerisate, (E) an epoxy resin (0.1-10), and (F) further additives, where the sum of components A to F = 100%. The graft polymerisate of C comprises (wt.%): (c1) a graft base of elastic rubber polymers (40-80) based on alkyl acrylates with a 1-8 C alkyl residue, glass transition temperature below 10 deg C, (c2) a graft support (20-60) comprising (c21) styrene or a substituted styrene (60-95) of formula (I): where R = 1-8C alkyl or H, R = 1-8C alkyl, n = 1,2, or 3, and (c22) at least one unsaturated nitrile (5-40). Component D comprises (wt.%): (d1) optionally substituted styrene of formula (I) or their mixtures (60-95), and (d2) at least one unsaturated nitrile (5-40).
-
公开(公告)号:ES2155705T3
公开(公告)日:2001-05-16
申请号:ES97951224
申请日:1997-11-18
Applicant: BASF AG
Inventor: GOTTSCHALK AXEL , WEBER MARTIN , KOCH ANDREAS , AUMULLER ALEXANDER
-
公开(公告)号:DE59703314D1
公开(公告)日:2001-05-10
申请号:DE59703314
申请日:1997-11-18
Applicant: BASF AG
Inventor: GOTTSCHALK AXEL , WEBER MARTIN , KOCH ANDREAS , AUMUELLER ALEXANDER
-
80.
公开(公告)号:BG104695A
公开(公告)日:2001-04-30
申请号:BG10469500
申请日:2000-08-17
Applicant: BASF AG
Inventor: MOHRSCHLAND RALF , WEBER MARTIN , HILDEBARNDT VOLKER
IPC: C08G69/00 , C08G69/04 , C08L25/04 , C08L51/04 , C08L71/00 , C08L71/12 , C08L77/00 , C08L79/08 , C08L81/06 , C08L101/00
Abstract: The invention relates to a method for producing polymer mixtures by reacting at least one amino nitrile with water in the presence of thermoplastic polymers and optional additional monomers which form polyamide. The inventive method comprises the following steps: (1) reacting at least one amino nitrile with water at a temperature ranging from 90 to 400 degrees C and under a pressure ranging from 0.1 to 35 x 106 Pa, whereby a reaction is obtained; (2) additional reaction of the reaction mixture ranging from 150 to 400 degrees C and under a pressure which is lower than the pressure in step (1), whereby the temperature and pressure are selected in such a way that a first gas phase and a first liquid or a first solid phase of a mixture comprised of the first solid and first liquid phases are obtained, and the first gas phase is separated off from the first liquid or the first solid phase or from the mixture comprised of the first liquid and the first solid phases; and (3) mixing the first liquid or the first solid phase or the mixture comprised of the first liquid and first solid phases with a gaseous or liquid phase which contains water and which can contain thermoplastic polymers and optional additional monomers which form polyamide. Said mixing occurs at a temperature ranging from 150 to 370 degrees C and under a pressure ranging from 0.1 to 30 x 106 Pa, whereby the polymer mixture is obtained and whereby the thermoplastic polymers and optional additional monomers which form polyamide are added in one or more of the steps. 6 claims
-
-
-
-
-
-
-
-
-