Abstract:
A film comprising a polyolefin composition comprising: A) 5-35% by weight of a propylene homopolymer or a propylene ethylene copolymer; B) 25-50% by weight; of a copolymer of ethylene and a C 3 -C 8 alpha-olefin containing from 0.1% to 20% by weight of alpha-olefin units; and C) 30-60% by weight of a copolymer of ethylene and propylene containing from 25% to 75% by weight of ethylene units.
Abstract:
A polypropylene composition comprising: A) from 50 wt% to 90 wt%; of a propylene homopolymer; B) from 10 wt% to 50wt%; of a copolymer of propylene with from 30.0 wt% to 70.0wt%, of ethylene derived units; the sum of the amount of component A) and B) being 100; the composition having: i) an intrinsic viscosity of the fraction soluble in xylene at 25 °C comprised between 2.2 and 4.0 dl/g; ii) a MFR L (Melt Flow Rate according to ISO 1133, condition L, i.e. 230°C and 2.16 kg load) from 0.5 to 100 g/10 min; iii) a xylene soluble fraction ranging from 20 wt% to 50 wt%; the polypropylene composition being obtained by a two steps polymerization process wherein the catalyst system contains bismuth.
Abstract:
A polyolefin composition comprising: A) from 19 wt% to 50 wt% of a propylene ethylene copolymer having an ethylene derived units content ranging from 1.5 wt% to 6.0 wt% B) from 50 wt% to 81 wt% of a propylene ethylene 1-butene terpolymer having an ethylene derived units content ranging from 1.5 wt% and 6.0 wt% and 1-butene derived units content of between 4.8 wt% and 12.4 wt%; the sum of the amount of component A) and B) being 100.
Abstract:
A polyolefin composition comprising: A) from 19 wt% to 50 wt% of a propylene ethylene copolymer having an ethylene derived units content ranging from 1.5 wt% to 6.0 wt% B) from 50 wt% to 81 wt% of a propylene ethylene 1-butene terpolymer having an ethylene derived units content ranging from 1.5 wt% and 6.0 wt% and 1-butene derived units content of between 4.8 wt% and 12.4 wt%; the sum of the amount of component A) and B) being 100; the composition being characterized by the following features: molecular weight distribution (MWD), expressed in terms of Mw/Mn, greater than 4.0; the creep and recovery curve measured on the polymer fuse at 200°C measured according to the procedure reported in the characterizing section shows a maximum value between 600 and 1200 seconds lower than 53x10 -5 1/Pa.
Abstract:
Polyolefin compositions comprising: (A) 5-35% by weight of a propylene-based polymer containing 90% by weight or more of propylene units and containing 10% by weight or less of a fraction soluble in xylene at 25 °C (XS A ), both the amount of propylene units and of the fraction XS A being referred to the weight of (A); (B) 25-50% by weight, of a copolymer of ethylene and a C 3 -C 8 alpha-olefin containing from 0.1% to 15% by weight of alpha-olefin units and containing 75% by weight or less of a fraction soluble in xylene at 25 °C (XS B ), both the amount of ethylene units and of the fraction XS B being referred to the weight of (B); and (C) 30-60% by weight, of a copolymer of ethylene and propylene containing from 45% to 75% by weight of ethylene units and containing from 55% to 95% by weight, of a fraction soluble in xylene at 25 °C (XS c ), both the amount of ethylene units and of the fraction XS c being referred to the weight of (C).
Abstract:
A terpolymer containing propylene, ethylene and 1-hexene wherein: (i) the content of 1-hexene derived units ranges from 1 wt% to 2.6 wt%; (ii) the content of ethylene derived units is higher than 0.7 wt% and fulfils the following relation (1): C2
Abstract:
A container comprising a polyolefin composition comprising: A) from 59 wt% to 84 wt%, of a propylene homopolymer having isotactic pentads (mmmm) measured with by 13 C-NMR higher than 96%, B) from 16 wt% to 41 wt%, of a copolymer of propylene and ethylene with from 30wt% to 44wt%, of ethylene derived units; the sum A) + B) being 100; the composition having an MFR L (Melt Flow Rate according to ISO 1133, condition L, i.e. 230°C and 2.16 kg load) comprised from 72 to 100 g/10 min.
Abstract:
A propylene composition comprising (percent by weight): A) 60%-95%, of a crystalline propylene copolymer containing from 2.0% to 10.0% of ethylene derived units having a melting point ranging from 148°C to 160°C; wherein the melting temperature Tm is measured by DSC on the as-reactor polymer; B) 40%-5%, of a copolymer of ethylene containing from 70% to 85%, of ethylene derived units intrinsic viscosity ranging from 0.8 to 3 dl/g.
Abstract:
Plastic tanks comprising a propylene-hexene-1 copolymer having a xylene soluble fraction lower than 5%wt with respect to the total weight of the copolymer and satisfying the relation (1), wherein A is the MFR measured according to the method ISO 1133 (230° C, 5 kg) expressed in g/10min, T m is the melting temperature measured by GPC expressed in °C and B is the hexene-1 content expressed in percentage by weight with respect to total weight of the copolymer.
Abstract:
The present invention relates to a process for producing a propylene terpolymer comprising comonomer units derived from ethylene and from one alpha-olefin selected from the group of C 4 -C 8 alpha-olefins and being characterized by a total content of comonomer units not less than 8 % wt and a value of the ratio of ethylene to the C 4 -C 8 alpha-olefins ranging from 0.1 to 0.8, said process being carried out in a gas-phase reactor comprising two interconnected polymerization zones. The present invention further relates to the propylene terpolymer obtained by said process particularly suitable to be used as films such as cast films, bi- or mono-oriented films and heat-sealable films having good optical properties and excellent sealing properties combined with good shrinkage properties and softness.