핫멜트 필름과 피착제를 접착시키는 방법 및 상기 방법으로 핫멜트 필름이 접착된 피착제

    公开(公告)号:KR1020110009617A

    公开(公告)日:2011-01-28

    申请号:KR1020100059382

    申请日:2010-06-23

    CPC classification number: C09J5/06 B32B7/12 B32B37/10 C09J175/04

    Abstract: PURPOSE: A method for adhering a hot melt film with fabric is provided to secure adhesion reliability, to minimize thickness deviation of laminating-fabric, and to maintain uniform thickness. CONSTITUTION: A method for adhering a hot melt film with fabric using a manufacturing device comprises the steps of: applying an adhesive(300) to the surface of an engraved roller(14); transferring an adhesive applied to the surface of the engraved roller by passing an adherend through the engraved roller and transfer roller(16); and adhering the adhesive to which the adhesive is applied with a hot melt film(200) through pressing rollers(20).

    Abstract translation: 目的:提供一种用织物粘附热熔膜的方法,以确保粘合可靠性,使层压织物的厚度偏差最小化并保持均匀的厚度。 构成:使用制造装置将热熔膜与织物粘合的方法包括以下步骤:将粘合剂(300)施加到雕刻辊(14)的表面; 通过将被粘物通过雕刻辊和转印辊(16)来转印施加到雕刻辊表面的粘合剂; 以及通过加压辊(20)将通过热熔胶膜(200)粘合到粘合剂上的粘合剂。

    흡음성과 단열성이 우수한 자동차용 내장재 및 그 제조방법
    2.
    发明授权
    흡음성과 단열성이 우수한 자동차용 내장재 및 그 제조방법 失效
    室内装饰材料,吸音性好,汽车绝热,是制造方法

    公开(公告)号:KR100705465B1

    公开(公告)日:2007-04-10

    申请号:KR1020060007110

    申请日:2006-01-24

    Inventor: 윤래원 황진영

    Abstract: 본 발명은 흡음성과 단열성이 우수한 자동차용 내장재 및 그 제조방법에 관한 것으로, 더욱 상세하게는 통상의 자동차용 내장재로 사용하는 플라스틱 성형물을 흡음 및 단열이 우수한 나노세라믹 섬유판과 층합시키되, 나노실버(Ag)와 이산화규소(SiO2)가 화학결합된 화합물과 플라스틱수지 분말 및 안정제을 혼합시킨 무기바인더로 층합시킴으로써, 흡음성 뿐만 아니라 단열성이 우수한 내장재를 제조할 수 있게 되어, 승차자들에게 쾌적하고 안락한 승차환경을 제공할 수 있고, 화재 사고시에 승차자들을 안전하게 보호할 수 있는 흡음성과 단열성이 우수한 자동차용 내장재 및 그 제조방법에 관한 것이다.
    본 발명에 따르면, 플라스틱 성형물과 나노세라믹 섬유판이 나노실버와 이산화규소가 화학 결합된 화합물을 플라스틱수지 분말과 안정제와 혼합시킨 무기바인더에 의해 층합됨을 특징으로 한 흡음성과 단열성이 우수한 자동차용 내장재 및 그 제조방법이 제공된다.
    자동차, 내장재, 무기바인더, 나노세라믹 섬유판, 흡음성, 단열성

    액상(液狀)접착제를 이용한 원단 합포방법
    3.
    发明公开
    액상(液狀)접착제를 이용한 원단 합포방법 失效
    使用液体粘合剂纺织布的方法

    公开(公告)号:KR1020020023919A

    公开(公告)日:2002-03-29

    申请号:KR1020010087992

    申请日:2001-12-29

    Inventor: 윤래원

    Abstract: PURPOSE: A method for doubling a fabric by coating a liquid adhesive on a roller and then doubling a flexible fabric for shoe and clothes with an inner liner in a non-heating method is provided, thereby reducing manufacturing processes, generating no dust during usage and reducing manufacturing cost. CONSTITUTION: A thermoplastic adhesive in a particle state is melted into a liquid state by a melting apparatus(1) and then coated on a roller(3) at room temperature by a spraying method through a discharging device(2) to spray-coat a liquid adhesive(5) on a fabric(100) passed between the roller and a coating roller(4). The adhesive-coated fabric and a fabric(200) for doubling supplied through another line are subjected to passing between a pressure roller(6)(6') to double and a cooling roller(7) to cool.

    Abstract translation: 目的:提供一种通过在辊上涂布液体粘合剂并且然后用非加热方法用内衬将鞋和衣服的柔性织物加倍的方法,从而减少制造过程,在使用过程中不产生灰尘, 降低制造成本。 构成:通过熔融装置(1)将颗粒状态的热塑性粘合剂熔化成液态,然后通过喷射装置(2)在室温下通过喷射装置(2)涂布在辊(3)上以喷涂 液体粘合剂(5)在通过辊和涂布辊(4)之间的织物(100)上。 粘合剂涂覆的织物和用于通过另一条线供应的加倍的织物(200)在加压辊(6)(6')与双重和冷却辊(7)之间经过冷却。

    4.
    外观设计
    有权

    公开(公告)号:KR3007714100000S

    公开(公告)日:2014-11-17

    申请号:KR3020140021123

    申请日:2014-04-25

    Designer: 박의진

    자동차 시트의 라미네이팅 방법
    5.
    发明公开
    자동차 시트의 라미네이팅 방법 有权
    车辆座椅的层压方法

    公开(公告)号:KR1020140080108A

    公开(公告)日:2014-06-30

    申请号:KR1020120149552

    申请日:2012-12-20

    Abstract: The present invention relates to a laminating method for a vehicle seat capable of improving the adhesive strength between seat fabric and polyurethane foamed body by allowing adhesive filled in the groove of a mesh roller to be uniformly and completely transferred to a subject by being applied with a mesh type hot melt dot producing method, wherein the hot melt dot producing method is previously applied and registered (Korean patent publication No.10-1203629) by the applicant of the present invention. The laminating method of the present invention can improve the adhesive strength, although the density of a hot melt per unit area dot is not high, and also improve permeability by processing the seat fabric or polyurethane foamed body in advance through radiating the seat fabric or polyurethane foamed body with UV or plasma before hot melt dots are formed.

    Abstract translation: 本发明涉及一种车辆座椅的层压方法,其能够通过使网状辊的槽中填充的粘合剂均匀且完全地转移到被检体上而使座垫织物与聚氨酯发泡体的粘合强度提高, 网格型热熔点制造方法,其中热熔点生产方法预先被应用和登记(韩国专利公开No.10-1203629)由本发明的申请人。 本发明的层压方法虽然每单位面积点的热熔体的密度不高,但通过预先通过辐射座椅织物或聚氨酯来改善座椅织物或聚氨酯发泡体的渗透性,可以提高粘合强度 在形成热熔点之前用UV或等离子体发泡体。

    투습 방수포용 미세다공 형성 코팅제 및 그 제조방법
    6.
    发明授权
    투습 방수포용 미세다공 형성 코팅제 및 그 제조방법 失效
    투습방수포용미세다공형성코팅제및그제조방투습

    公开(公告)号:KR100726936B1

    公开(公告)日:2007-06-14

    申请号:KR1020060035680

    申请日:2006-04-20

    Inventor: 김한도

    Abstract: A water-permeable and waterproof coating agent is provided to produce microporous polyurethane water-permeable and waterproof cloth having high porosity and improved water permeability. The water-permeable and waterproof coating agent comprises: a water-dispersible polyurethane; a water-soluble polymer which is at least one selected from the group consisting of sodium alginate, polyvinyl alcohol, wheat flour, and starch and is contained in an amount of 40wt% or less of the water-dispersible polyurethane; a thickener in an amount of 0.5wt% of a mixture of water-dispersible polyurethane and water-soluble polymer; and a hardener in an amount of 3wt% of the mixture of water-dispersible polyurethane and water-soluble polymer.

    Abstract translation: 本发明提供了一种透水防水涂层剂,用于生产具有高孔隙率和改善透水性的微孔聚氨酯透水防水布。 所述透水防水涂布剂包含:水分散性聚氨酯; 水溶性聚合物,其是选自海藻酸钠,聚乙烯醇,小麦粉和淀粉中的至少一种,并且其含量占水分散性聚氨酯的40wt%或更少; 量为0.5重量%的水分散性聚氨酯和水溶性聚合物的混合物的增稠剂; 和水分散性聚氨酯和水溶性聚合物的混合物的量为3重量%的硬化剂。

    자동차 시트의 라미네이팅 방법
    7.
    发明授权
    자동차 시트의 라미네이팅 방법 有权
    车辆座椅的层压方法

    公开(公告)号:KR101455818B1

    公开(公告)日:2014-11-03

    申请号:KR1020120149552

    申请日:2012-12-20

    Abstract: 본 발명은 자동차 시트의 라미네이팅 방법에 관한 것으로, 더욱 상세하게는 본 발명의 출원인에 의해 선출원되어 등록(국내 등록특허공보 제10-1203629호)받은 메쉬 타입의 핫멜트 도트 제조방법을 자동차 시트의 라미네이팅 방법에 적용함으로써, 메쉬롤러의 홈에 충전되어 있던 접착제가 잔류 접착제 없이 피착제로 모두 균일하게 전이될 수 있도록 함으로써 시트 원단과 폴리우레탄 발포체 간의 접착력을 향상시킬 수 있도록 하며, 아울러, 상기와 같은 핫멜트 도트를 형성시키기 전에 UV 또는 플라즈마를 조사하여 시트 원단 또는 폴리우레탄 발포체를 선처리함으로써, 핫멜트 도트의 단위 면적당 밀도가 높지 않더라도 접착력을 더욱 향상시킬 수 있으며 이로 인해 통기성 역시 향상시킬 수 있도록 하는, 자동차 시트의 라미네이팅 방법에 관한 것이다.

    흡음성과 단열성이 우수한 자동차용 내장재 및 그 제조방법
    8.
    发明公开
    흡음성과 단열성이 우수한 자동차용 내장재 및 그 제조방법 失效
    内置装饰材料,具有良好的声音吸收和适用于汽车及其制造方法

    公开(公告)号:KR1020060013442A

    公开(公告)日:2006-02-09

    申请号:KR1020060007110

    申请日:2006-01-24

    Inventor: 윤래원 황진영

    Abstract: 본 발명은 흡음성과 단열성이 우수한 자동차용 내장재 및 그 제조방법에 관한 것으로, 더욱 상세하게는 통상의 자동차용 내장재로 사용하는 플라스틱 성형물을 흡음 및 단열이 우수한 나노세라믹 섬유판과 합포시키되, 나노실버(Ag)와 이산화규소(SiO2)가 화학결합된 화합물과 플라스틱수지 분말 및 안정제을 혼합시킨 무기바인더로 합포시킴으로써, 흡음성 뿐만 아니라 단열성이 우수한 내장재를 제조할 수 있게 되어, 승차자들에게 쾌적하고 안락한 승차환경을 제공할 수 있고, 화재 사고시에 승차자들을 안전하게 보호할 수 있는 흡음성과 단열성이 우수한 자동차용 내장재 및 그 제조방법에 관한 것이다.
    본 발명에 따르면, 플라스틱 성형물과 나노세라믹 섬유판이 나노실버와 이산화규소가 화학 결합된 화합물을 플라스틱수지 분말과 안정제와 혼합시킨 무기바인더에 의해 합포됨을 특징으로 한 흡음성과 단열성이 우수한 자동차용 내장재 및 그 제조방법이 제공된다.
    자동차, 내장재, 무기바인더, 나노세라믹 섬유판, 흡음성, 단열성

    액상(液狀)접착제를 이용한 원단 합포방법
    9.
    发明授权
    액상(液狀)접착제를 이용한 원단 합포방법 失效
    액상(液状)접착제를이용한원단합포방법

    公开(公告)号:KR100419240B1

    公开(公告)日:2004-02-21

    申请号:KR1020010087992

    申请日:2001-12-29

    Inventor: 윤래원

    Abstract: PURPOSE: A method for doubling a fabric by coating a liquid adhesive on a roller and then doubling a flexible fabric for shoe and clothes with an inner liner in a non-heating method is provided, thereby reducing manufacturing processes, generating no dust during usage and reducing manufacturing cost. CONSTITUTION: A thermoplastic adhesive in a particle state is melted into a liquid state by a melting apparatus(1) and then coated on a roller(3) at room temperature by a spraying method through a discharging device(2) to spray-coat a liquid adhesive(5) on a fabric(100) passed between the roller and a coating roller(4). The adhesive-coated fabric and a fabric(200) for doubling supplied through another line are subjected to passing between a pressure roller(6)(6') to double and a cooling roller(7) to cool.

    Abstract translation: 目的:提供一种通过在辊上涂布液体粘合剂并且随后以非加热方法使具有内衬的鞋和衣服的柔性织物加倍的方法来加倍织物的方法,由此减少制造工艺,在使用期间不产生灰尘并且 降低制造成本。 组成:通过熔融设备(1)将处于颗粒状态的热塑性粘合剂熔化成液态,然后通过喷射装置(2)在室温下在室温下涂覆在辊子(3)上,以喷涂 在织物(100)上的液体粘合剂(5)通过辊和涂布辊(4)之间。 粘合剂涂覆的织物和用于通过另一条线提供的加倍的织物(200)在加压辊(6)(6')和加热辊(7)之间通过以进行冷却。

    항균성과 방취성을 가지는 합포용 내피 직물 및 그 제조방법
    10.
    发明公开
    항균성과 방취성을 가지는 합포용 내피 직물 및 그 제조방법 无效
    用于具有抗菌性能的组合织物的内衬织物和其生产的物质和生产

    公开(公告)号:KR1020010071653A

    公开(公告)日:2001-07-31

    申请号:KR1020010036921

    申请日:2001-06-27

    Inventor: 윤래원

    Abstract: PURPOSE: A process for preparing an inner lining fabric for combined fabric by mixing natural inorganic material excellent in sterilizing or antibacterial property and deodorizing property with a thermoplastic adhesive agent for adhering to the surface of an inner surface and coating is provided. Whereby, the obtained fabric has excellent deodorizing effect, air permeability and moisture permeation property. CONSTITUTION: The titled inner lining fabric is prepared by the characteristic process comprising the steps of: mixing a thermoplastic adhesive agent exhibiting an adhesion function on the surface of a substrate(1) used as an inner coat(100) and an antibacterial agent in a specified rate and coating to produce a stripe pattern(2); and heating. The fabric contains 90 to 97% by weight of a thermoplastic adhesive agent and 3 to 10% by weight of an antibacterial.

    Abstract translation: 目的:提供一种制备用于组合织物的内衬织物的方法,其通过将具有优异的消毒或抗菌性能和除臭性能的天然无机材料与用于粘附到内表面和涂层的表面的热塑性粘合剂混合来制备。 由此得到的织物具有优异的除臭效果,透气性和水分渗透性。 构成:通过特征性方法制备标题的内衬织物,其特征在于包括以下步骤:将表现出粘附功能的热塑性粘合剂混合在用作内涂层(100)的基材(1)的表面和抗菌剂 指定速率和涂层以产生条纹图案(2); 并加热。 该织物含有90至97重量%的热塑性粘合剂和3至10重量%的抗菌剂。

Patent Agency Ranking