Abstract: A method for producing a glass preform for an optical fiber comprises (a) dehydrating a porous preform composed of GeO2-SiO2 fine glass particles, (b) heating the preform under oxygen gas atmosphere contg. at least F-system gas so as to be dehydrated at a temp. at which violent shrinkage does not occur, and then (c) heating the preform under He gas atmosphere at such temp. that the preform is throughly vitrified. The fine glass particles are composed of P2O5, GeO2 and SiO2.
Abstract translation: 制造光纤用玻璃预制体的方法包括:(a)使由GeO 2 -SiO 2微细玻璃粒子构成的多孔预成型体脱水,(b)在氧气气氛下加热预成型体。 至少F系统气体,以便在温度下脱水。 不会发生剧烈收缩,然后(c)在这样的温度下在He气体气氛下加热预制件。 预成型件通透玻璃化。 细玻璃颗粒由P2O5,GeO2和SiO2组成。
-
公开(公告)号:KR100028565B1
公开(公告)日:1989-07-24
申请号:KR1019850003265
申请日:1985-05-14
Applicant: 스미토모덴키고교가부시키가이샤
IPC: C03B37/018
-
公开(公告)号:KR100040845B1
公开(公告)日:1991-04-01
申请号:KR1019850003146
申请日:1985-05-09
Applicant: 스미토모덴키고교가부시키가이샤
IPC: C03B37/012 , C03C13/04
-
公开(公告)号:KR1019900008503B1
公开(公告)日:1990-11-24
申请号:KR1019850003146
申请日:1985-05-09
Applicant: 스미토모덴키고교가부시키가이샤
IPC: C03B37/012 , C03C13/04
CPC classification number: C03B37/0146 , C03B37/01446 , C03B37/01453 , C03B2201/12 , C03B2203/22 , Y10S65/16 , Y10S65/90
Abstract: 내용 없음.
-
-
-