Abstract:
본 발명에 따른 금속 정련 방법은 바이너리 상태도상 금속 산화물의 금속인 제1금속과 공정 점(eutectic point)을 갖는 금속 음극을 이용한 전해환원을 통해, 상기 제1금속과 상기 액체 금속 음극의 금속인 제 2금속간의 합금(alloy)을 제조하는 전해환원 단계; 및 고화된 상기 합금을 전해정련하여, 상기 합금으로부터 제1금속을 회수하는 전해정련 단계;를 포함한다.
Abstract:
A method for manufacturing a pasteboard is provided to increase bulk and bending stiffness of the pasteboard, by using adding woody fiber particles, which are physically reformed, in a middle layer of the pasteboard. A timber chip is beat by defibrators, thereby forming woody fiber particles each having a length weighted mean fiber length of 1.0-3.0 mm and a fiber wall thickness of less than 0.9 mg/m. The formed woody fiber particles are chemically processed by using oxidizers, acid, or alkali. The chemically processed woody fiber particles and chemically unprocessed woody fiber particles are physically processed by using beaters, refiners, or defibrators, thereby forming woody fiber particles each having a length weighted mean fiber length of less than 1.0 mm and a fiber wall thickness of less than 0.9 mg/m.
Abstract translation:提供一种用于制造纸板的方法,其通过使用在纸板的中间层中添加物理重整的木质纤维颗粒来增加纸板的松厚度和弯曲刚度。 用解纤器打碎木材碎片,由此形成木质纤维颗粒,每个木质纤维颗粒的长度加权平均纤维长度为1.0-3.0mm,纤维壁厚小于0.9mg / m 2。 所形成的木质纤维颗粒通过使用氧化剂,酸或碱进行化学处理。 化学处理的木质纤维颗粒和化学未加工的木质纤维颗粒通过使用搅拌器,磨浆机或解纤器进行物理处理,由此形成木质纤维颗粒,每个木质纤维颗粒的长度加权平均纤维长度小于1.0mm且纤维壁厚小于 0.9毫克/米。
Abstract:
본 발명은 자전거에서, 앞바퀴축(130)의 양단에 일단이 연결되어 회전가능한 2개의 수직바(110); 상기 2개의 수직바(110) 타단에 각각 연결되어 핸들기능을 수행하는 2개의 핸들(120); 및, 상기 2개의 핸들(120) 상호간을 연결하는 연결바(140);를 포함하여 구성되되, 지면에 설치된 거치대를 앞바퀴 앞에 두고 상기 연결바(140)가 해제된 상태에서 상기 수직바(110)가 상기 앞바퀴축(130)을 중심으로 회전하여 상기 핸들(120)이 지면에 닿은 후 상기 연결바(140)를 결속하면 자전거거치대의 기능을 수행함과 동시에 자전거잠금장치 기능을 수행하는 것을 특징으로 하는 핸들을 이용한 잠금장치를 가진 자전거(100)를 제공한다. 더불어, 상기 연결바(140)는 다이얼식자물쇠 또는 열쇠식자물쇠가 추가로 구성되는 것을 특징으로 하는 핸들을 이용한 잠금장치를 가진 자전거(100)를 제공한다.