公开(公告)号:KR1019900001409B1
公开(公告)日:1990-03-09
申请号:KR1019870012578
申请日:1987-11-07
Applicant: 한국과학기술연구원
IPC: H01L41/18
Abstract: The piezo-electric material is prepared by mixing 0-0.05 wt.% Pb (Cd1/2 W1/2) O3 and 0.4-0.6 wt.% PbTiO3 with 0.4 - 0.6 wt.% PbZrO3, calcining the mixture at 750-950 deg.c, pulverizing and moulding under 1000 kg/cm2, and sintering at 1000 -1100 deg.C.